CPC分类号: B32B37/1018 , B32B17/10036 , B32B17/10137 , B32B17/10743 , B32B17/10761 , B32B17/1077 , B32B17/10788 , B32B17/10853 , B32B17/1088 , B32B17/10889 , B32B17/10972 , B32B37/06 , B32B37/182 , B32B2250/03 , B32B2250/40 , B32B2307/10 , B32B2309/02 , B32B2309/12 , B32B2309/68 , B32B2315/08 , B32B2329/06 , B32B2331/04 , B32B2375/00 , C03B23/0357 , C03C27/10 , Y10T156/1044
摘要: A process using a vacuum ring or vacuum bag to produce glass laminates with improved optical distortion and shape consistency using thin glass having a thickness not exceeding 1.0 by using a soak temperatures not exceeding 120° C or not exceeding 100° C and a vacuum not exceed about -0.6 bar. One or more assembled stacks of two glass sheets and a polymer interlayer being laminated may be stacked on a single reference mold and processed simultaneously in a single vacuum bag or vacuum ring. One more thin glass sheets may be placed on top the assembled stack(s) on the reference mold to protect the assembled stack from irregular forces applied by the vacuum bag or the vacuum ring.
摘要翻译: 使用真空环或真空袋来制造具有改善的光学变形和形状一致性的玻璃层压板的方法,使用厚度不超过1.0的薄玻璃通过使用不超过120℃或不超过100℃的浸泡温度和真空不超过 约-0.6巴。 将两个玻璃板和层压聚合物夹层的一个或多个组装堆叠堆叠在单个参考模具上,同时在单个真空袋或真空环中进行处理。 可以在参考模具上的组装的堆叠的顶部放置一个更薄的玻璃板,以保护组装的堆叠免受真空袋或真空环施加的不规则的力。
-
公开(公告)号:WO2008082499A3
公开(公告)日:2009-01-22
申请号:PCT/US2007025796
申请日:2007-12-18
CPC分类号: D01D5/0038 , D01D5/0069 , D01F6/60 , D04H1/4374 , D04H1/559 , D04H1/56 , D04H1/728
摘要: A process for electroblowing a multiple layered sheet using multiple spinning beams to produce different component webs wherein the sheet doesn't stick to the forming screen and has improved web stability.
摘要翻译: 一种使用多个纺丝电极吹制多层片材以产生不同组分纤维网的方法,其中片材不粘附到成型筛网并且具有改进的幅材稳定性。
-
公开(公告)号:WO2012177426A1
公开(公告)日:2012-12-27
申请号:PCT/US2012/041811
申请日:2012-06-11
CPC分类号: B32B17/10091 , B32B17/10036 , B32B17/10119 , B32B17/10137 , B32B17/10761 , Y10T428/24628 , Y10T428/2495
摘要: A glass laminate comprises an external glass sheet, an internal glass sheet, and a polymer interlayer formed between the external glass sheet and the internal glass sheet. The external glass sheet is a chemically-strengthened glass sheet having a thickness of less than 1 mm, the polymer interlayer has a thickness of less than 1.6 mm, and the internal glass sheet is a non-chemically-strengthened glass sheet having a thickness of less than 2.5 mm.
摘要翻译: 玻璃层压体包括外部玻璃板,内部玻璃板和形成在外部玻璃板和内部玻璃板之间的聚合物中间层。 外部玻璃板是厚度小于1mm的化学强化玻璃板,聚合物中间层的厚度小于1.6mm,内部玻璃板是非化学强化玻璃板,其厚度为 小于2.5毫米。
-
公开(公告)号:WO2013181505A1
公开(公告)日:2013-12-05
申请号:PCT/US2013/043561
申请日:2013-05-31
CPC分类号: B32B17/10036 , B32B17/10137 , B32B2250/03 , B32B2250/40 , B32B2419/00 , B32B2605/00 , Y10T428/24355 , Y10T428/24967
摘要: A glass laminate includes at least one chemically-strengthened glass sheets with a thickness not exceeding 2.0 mm and a polymer interlayer between the glass sheets. Flaws are created in the surface of one of the glass sheets in order to weaken the glass laminate upon an impact event on a first side of the laminate, while retaining the strength of the laminate upon impact on the opposing second side of the laminate. The opposing side of the glass sheet with the flaws or a surface of the other glass sheet may be strengthened with an acid etch treatment in order to further strengthen the laminate upon impact on the opposing second side of the laminate.
摘要翻译: 玻璃层压体包括至少一层厚度不超过2.0mm的化学强化玻璃板和玻璃板之间的聚合物中间层。 在玻璃板之一的表面上产生裂纹,以便在层叠体的第一面上的冲击事件时削弱玻璃层压体,同时保持层压体在层压体的相对的第二侧上的冲击强度。 具有瑕疵的玻璃板或另一玻璃板的表面的相对侧可以通过酸蚀刻处理来加强,以便在层压体的相对的第二侧上冲击时进一步加强层压板。
-
公开(公告)号:WO2008082499A2
公开(公告)日:2008-07-10
申请号:PCT/US2007/025796
申请日:2007-12-18
CPC分类号: D01D5/0038 , D01D5/0069 , D01F6/60 , D04H1/4374 , D04H1/559 , D04H1/56 , D04H1/728
摘要: A process for electroblowing a multiple layered sheet using multiple spinning beams to produce different component webs wherein the sheet doesn't stick to the forming screen and has improved web stability.
摘要翻译: 一种使用多个纺丝电极吹制多层片材以产生不同组分纤维网的方法,其中片材不粘附到成型筛网并且具有改进的幅材稳定性。
-
6.
公开(公告)号:WO2014052229A1
公开(公告)日:2014-04-03
申请号:PCT/US2013/061164
申请日:2013-09-23
申请人: CORNING INCORPORATED , CITES, Jeffrey Scott , CLEARY, Thomas Michael , COUILLARD, James Gregory , MOORE, Michael John
CPC分类号: C03C21/002 , B32B3/263 , B32B17/10036 , B32B17/10119 , B32B17/10137 , B32B17/10761 , B32B2250/03 , B32B2250/40 , B32B2419/00 , B32B2605/006 , C03C3/085 , C03C3/095 , C03C15/00 , C03C27/10 , Y10T428/2495 , Y10T428/24967 , Y10T428/24983 , Y10T428/269 , Y10T428/315
摘要: A laminate structure having a first glass layer, a second glass layer, and at least one polymer interlayer intermediate the first and second glass layers. The first glass layer is comprised of a thin, chemically strengthened glass having a surface compressive stress of between about 250 MPa and about 350 MPa and a depth of layer (DOL) of compressive stress greater than about 60 µm. The second glass layer can also be comprised of a thin, chemically strengthened glass having a surface compressive stress of between about 250 MPa and about 350 MPa and a depth of layer (DOL) of compressive stress greater than about 60 µm.
摘要翻译: 一种具有第一玻璃层,第二玻璃层和在第一和第二玻璃层之间的至少一个聚合物夹层的层压结构。 第一玻璃层由薄的化学强化的玻璃构成,表面压应力在约250MPa至约350MPa之间,压缩应力的层厚度(DOL)大于约60μm。 第二玻璃层还可以由表面压应力在约250MPa至约350MPa之间的薄化学强化玻璃和压应力大于约60μm的层深度(DOL)组成。
-
公开(公告)号:WO2012051038A1
公开(公告)日:2012-04-19
申请号:PCT/US2011/055065
申请日:2011-10-06
申请人: CORNING INCORPORATED , FISHER, William Keith , MOORE, Michael John , ROSENBLUM, Steven S. , SHI, Zhiqiang , THOMAS, John Christopher
发明人: FISHER, William Keith , MOORE, Michael John , ROSENBLUM, Steven S. , SHI, Zhiqiang , THOMAS, John Christopher
CPC分类号: B32B17/10137 , B32B17/10036 , B32B17/10045 , B32B17/10119 , B32B17/1055 , B32B17/10761 , Y10T428/24628 , Y10T428/24967 , Y10T428/266
摘要: A glass laminate includes at least one chemically-strengthened glass sheet and a polymer interlayer formed over a surface of the sheet. The chemically-strengthened glass sheet has a thickness of less than 2.0 mm, and a near-surface region under a compressive stress. The near surface region extends from a surface of the glass sheet to a depth of layer (in micrometers) of at least 65-0.06(CS), where CS is the compressive stress at the surface of the chemically-strengthened glass sheet and CS > 300 MPa.
摘要翻译: 玻璃层压体包括至少一个化学强化玻璃片和在该片的表面上形成的聚合物中间层。 化学强化玻璃板的厚度小于2.0mm,压缩应力下的近表面区域。 近表面区域从玻璃板的表面延伸至至少65-0.06(CS)的层(微米)深度,其中CS是化学强化玻璃板表面处的压应力,CS> 300 MPa。
-
-
-
-
-
-