公开(公告)号:WO2004065325A1
公开(公告)日:2004-08-05
申请号:PCT/JP2004/000423
申请日:2004-01-20
IPC分类号: C04B35/44
CPC分类号: C04B35/20 , B32B18/00 , B32B2311/08 , C04B35/16 , C04B35/44 , C04B35/6264 , C04B35/63 , C04B2235/3201 , C04B2235/3203 , C04B2235/3206 , C04B2235/3208 , C04B2235/3213 , C04B2235/3217 , C04B2235/3222 , C04B2235/3232 , C04B2235/3234 , C04B2235/3236 , C04B2235/3284 , C04B2235/3418 , C04B2235/3427 , C04B2235/3445 , C04B2235/3463 , C04B2235/3481 , C04B2235/36 , C04B2235/365 , C04B2235/6025 , C04B2235/656 , C04B2235/80 , C04B2237/341 , C04B2237/343 , C04B2237/408 , C04B2237/704 , H01B3/004 , H01B3/12 , H05K1/0306 , Y10T428/24926
摘要: A dielectric ceramic composition which can be formed into a built-in or multilayer structure through simultaneously firing with a low resistance conductor such as Ag or Cu and can be fired at 800 to 1000°C into a dielectric ceramic exhibiting a dielectric constant (ϵr) of 10 or below, a large Qxf0 value and an absolute value of temperature coefficient (tauf) of resonance frequency (f0) of 20 ppm/°C or less whose regulation is easy. The dielectric ceramic composition comprises 5 to 150 pts.wt. of glass component per 100 pts.wt. of main components of the general formula: aZnAl2O4-bZn2SiO4-cTiO2-dZn2TiO4 wherein the molar fractions a, b, c and d of individual components satisfy the relationships: 5.0
摘要翻译: 一种电介质陶瓷组合物,其可以通过同时用诸如Ag或Cu的低电阻导体同时烧制而形成内置或多层结构,并且可以在800至1000℃下烧制成介电常数(εr)的介电陶瓷, 10或以下,调节容易的大的Qxf0值和谐振频率(f0)的温度系数(τf)绝对值为20ppm /℃以下。 电介质陶瓷组合物包含5至150重量份 的玻璃成分每100重量份 的主要成分为:aZnAl2O4-bZn2SiO4-cTiO2-dZn2TiO4,其中各组分的摩尔分数a,b,c和d满足以下关系:5.0 <= a <= 80.0摩尔%,5.0 <= b <= 70.0 mol%,5.0 <= c <= 27.5摩尔%,0 <= d <= 30.0摩尔%(条件是a + b + c + d = 100摩尔%)。