Abstract: Process for making a particulate (oxy)hydroxide of TM wherein TM represents metals and TM comprises at least 75 mol-% nickel and wherein said process comprises the steps of: (a) providing an aqueous solution (α) containing a water-soluble salt of nickel and of one metal selected from cobalt and manganese, and further in the range of from 0.05 to 3.0 mol-% of a compound of at least one metal selected from Ti, Zr, Mg and Nb, and in the range of from 0.05 to 2.0 mol-%, referring to TM, of an α- or β-hydroxy carboxylic acid or ascorbic acid or of an amino acid selected from glycine, alanine and serine, or their alkali metal salts, and an aqueous solution (β) containing an alkali metal hydroxide and, optionally, an aqueous solution (γ) containing ammonia, (b) combining a solution (α) and a solution (β) and, if applicable, a solution (γ) at a pH value in the range of from 11.0 to 13.0 in a stirred tank reactor, thereby creating solid particles of a hydroxide containing nickel, said solid particles being slurried.
-
公开(公告)号:WO2022128805A2
公开(公告)日:2022-06-23
申请号:PCT/EP2021/085261
申请日:2021-12-10
Applicant: BASF SE
Inventor: SOMMER, Heino , ERK, Christoph , HAAG, Jacob , SIOSS, James A , KOEHLER, Daniela , MICHEL, Kathrin , GARVE, Lennart Karl Bernhard , BERGNER, Benjamin Johannes Herbert
IPC: C01G53/00 , H01M4/00 , C01G53/04 , C01G53/006 , C01G53/42 , C01G53/50 , C01P2002/52 , C01P2002/54 , C01P2004/32 , C01P2004/50 , C01P2004/51 , C01P2004/61 , C01P2006/12 , C01P2006/40 , C01P2006/82 , H01M4/525
Abstract: Process for making an electrode active material wherein said process comprises the follow-ing steps: (a) Providing a hydroxide TM(OH)2 or an oxyhydroxide of TM wherein TM is one or more metals and contains Mn and, optionally, Co, and from 85 to 95 mol% Ni, referring to the sum of Ni, Co and Mn, (b) Drying said hydroxide TM(OH)2 or oxyhydroxide of TM at a temperature in the range of from 400 to 600°C, thereby obtaining an oxide or oxyhydroxide of TM with a residual moisture content of from 200 to 500 ppm, (c) mixing said oxide or oxyhydroxide from step (b) with a source of lithium and with at least one compound of Mg or Al and with at least one compound of Ti or Zr, (d) treating the mixture obtained from step (c) thermally at a temperature in the range of from 550 to 875°C.
-
公开(公告)号:WO2021244963A1
公开(公告)日:2021-12-09
申请号:PCT/EP2021/064322
申请日:2021-05-28
Applicant: BASF SE
Abstract: Process for making a particulate (oxy)hydroxide of TM wherein TM comprises nickel and where-in said process comprises the steps of:(a) Providing an aqueous solution (α) containing water-soluble salts of Ni and of at least one transition metal selected from Co and Mn, and, optionally, at least one further metal se-lected from Ti, Zr, Mo, W, Al, Mg, Nb, and Ta, and an aqueous solution (β) containing an alkali metal hydroxide and, optionally, an aqueous solution (γ) containing ammonia,(b) combining a solution (α) and a solution (β) and, if applicable, a solution (γ) at a pH valuein the range of from 12.0 to 13.0 in a stirred tank reactor, thereby creating solid particles ofa hydroxide containing nickel, said solid particles being slurried, (c) transferring said slurry into another stirred tank reactor and combining it with a solution (α)and a solution (β) and, if applicable, a solution (γ) at a pH value in the range of from 11.0to 12.7 and at conditions wherein the solubility of nickel is higher than in step (b),wherein the stirring speed is reduced in the course of step (c).
-
4.
公开(公告)号:WO2021228614A1
公开(公告)日:2021-11-18
申请号:PCT/EP2021/061636
申请日:2021-05-04
Applicant: BASF SE
Abstract: Process for making a particulate (oxy)hydroxide of TM wherein TM comprises nickel wherein said process comprises the steps of: (a) Providing an aqueous solution (α) containing water-soluble salts of Ni and of at least one transition metal selected from Co and Mn, and, optionally, at least one further metal selected from Ti, Zr, Mo, W, Al, Mg, Nb, and Ta, and an aqueous solution (β) containing an alkali metal hydroxide and, optionally, an aqueous solution (γ) containing ammonia, (b) combining a solution (α) and a solution (β) and, if applicable, a solution (γ) at a pH value in the range of from 12.0 to 13.0, thereby creating solid particles of hydroxide containing nickel, (c) continuing combining solutions (α) and (β) and, if applicable, (γ) at a pH value in the range of from 9.0 to 12.0 and in any way below the pH value in step (b), (d) adding a solution (α) and a solution (β) and, if applicable, a solution (γ) at a pH value in the range of from 12.0 to 12.7 and in any way above the pH value in step (c), (e) continuing combining such solutions (α) and (β) and, if applicable, (γ) at a pH value in the range of from 9.0 to 12.0 and in any way below the pH value in step (d), wherein step (d) has a duration in the range of from rt-0.01 to rt-0.15 and wherein rt is the average residence time of the reactor in which steps (b) to (e) are carried out.
-
公开(公告)号:WO2020260102A1
公开(公告)日:2020-12-30
申请号:PCT/EP2020/066814
申请日:2020-06-17
Applicant: BASF SE
Inventor: BERGNER, Benjamin Johannes Herbert , SOMMER, Heino , HARTMANN, Pascal , TEUFL, Tobias Maximilian
IPC: C01G53/00
Abstract: Particulate material of the composition Li 1+x TM 1-x O 2 wherein x is in the range of from –0.02 to + 0.05, TM comprises at least 93 mol-% nickel and (A) at least one element M 1 wherein M 1 is selected from Nb, Ta, Ti, Zr, W and Mo, (B) at least one element M 2 wherein M 2 is selected from B, Al, Mg and Ga, wherein said particulate material has an average particle diameter (D50) in the range of from 2 to 20 µm.
-
公开(公告)号:WO2022207383A1
公开(公告)日:2022-10-06
申请号:PCT/EP2022/057294
申请日:2022-03-21
Applicant: BASF SE
Inventor: BEIERLING, Thorsten , KOEHLER, Daniela , BERGNER, Benjamin Johannes Herbert , ERK, Christoph
IPC: C01G53/00 , H01M4/525 , H01M4/04 , H01M10/052 , H01M4/02
Abstract: The present invention is directed towards a process for making a particulate oxyhydroxide or oxide of TM with a bimodal particles diameter distribution wherein TM represents metals, and wherein TM comprises nickel and at least one metal selected from cobalt and manganese.
-
公开(公告)号:WO2022122448A2
公开(公告)日:2022-06-16
申请号:PCT/EP2021/083359
申请日:2021-11-29
Applicant: BASF SE
Inventor: BERGNER, Benjamin Johannes Herbert , HARTMANN, Pascal
IPC: C01G53/00 , H01M4/505 , H01M4/525 , C01G53/42 , C01G53/50 , C01P2002/54 , C01P2004/04 , C01P2004/50 , C01P2004/51 , C01P2004/61 , C01P2006/40 , C01P2006/80
Abstract: Process for making an electrode active material wherein said process comprises the following steps: (a) Providing an (oxy)hydroxide or oxide of TM wherein TM is a combination of metals and wherein TM contains Ni and at least one of Mn and Co; (b) treating said oxide or (oxy)hydroxide from step (a) with a non-aqueous or aqueous solution of a compound of M2 wherein M2 is selected from Ti, Zr, Nb or Ta; (c) removing the solvent(s), thereby obtaining a solid residue; (d) mixing the solid residue from step (c) with a source of lithium and, optionally, at least one compound of Ti or Al or Zr; (e) treating the mixture obtained from step (d) thermally at a temperature in the range of from 550 to 900°C.
-
公开(公告)号:WO2022122448A1
公开(公告)日:2022-06-16
申请号:PCT/EP2021/083359
申请日:2021-11-29
Applicant: BASF SE [DE]/[DE]
Inventor: BERGNER, Benjamin Johannes Herbert , HARTMANN, Pascal
Abstract: Process for making an electrode active material wherein said process comprises the following steps: (a) Providing an (oxy)hydroxide or oxide of TM wherein TM is a combination of metals and wherein TM contains Ni and at least one of Mn and Co; (b) treating said oxide or (oxy)hydroxide from step (a) with a non-aqueous or aqueous solution of a compound of M2 wherein M2 is selected from Ti, Zr, Nb or Ta; (c) removing the solvent(s), thereby obtaining a solid residue; (d) mixing the solid residue from step (c) with a source of lithium and, optionally, at least one compound of Ti or Al or Zr; (e) treating the mixture obtained from step (d) thermally at a temperature in the range of from 550 to 900°C.
-
-
-
-
-
-
-