公开(公告)号:WO1997025160A1
公开(公告)日:1997-07-17
申请号:PCT/US1997000001
申请日:1997-01-03
Applicant: CHEMICAL LIME COMPANY
Inventor: CHEMICAL LIME COMPANY , HUEGE, Fred, R. , SALTER, Timothy, L.
IPC: B05D07/22
CPC classification number: C04B28/10 , B05D7/222 , C04B2111/00146 , C04B2111/00482 , C04B2111/23 , C04B2111/56 , E03F3/06 , E03F2003/065 , F16L58/04 , C04B22/062 , C04B2103/0084 , C04B2103/402
Abstract: A method of treating concrete pipe (10) is carried out by providing an aqueous lime slurry supply having a lime solids content above 35 % by weight of the slurry. This is mixed within an amount of dispersing agent and may contain an alkali metal hydroxide so that the slurry has a pumpable viscosity. A spray assembly (28) is located within the interior of the pipe. The lime slurry is pumped from this lime slurry supply through the spray assembly (28) so that the lime slurry is applied to the interior surface of the pipe to neutralize acids thereon. Applying the lime spray also provides a protective coating of the lime slurry on the interior surfaces of the pipe.
Abstract translation: 一种处理混凝土管道(10)的方法是通过提供石灰固体含量高于浆料重量的35%的水性石灰浆料供应来进行的。 这在一定量的分散剂中混合,并且可以含有碱金属氢氧化物,使得浆料具有可泵送的粘度。 喷雾组件(28)位于管道内部。 将石灰浆料从该石灰浆料供应源泵送通过喷雾组件(28),使得石灰浆料施加到管的内表面以中和其上的酸。 施加石灰喷雾还在管的内表面上提供石灰浆的保护涂层。
-
公开(公告)号:WO1997007882A1
公开(公告)日:1997-03-06
申请号:PCT/US1996013476
申请日:1996-08-23
Applicant: CHEMICAL LIME COMPANY
Inventor: CHEMICAL LIME COMPANY , HUEGE, Fred, R. , SALTER, Timothy, L.
IPC: B01J13/00
CPC classification number: C02F1/54 , C02F1/5236
Abstract: A composition for a pumpable lime slurry which is adapted for use as a replacement for caustic solutions is formed by combining a dispersing agent in lime and water to form an aqueous slurry. The amount of lime used is between 35 to 55 % by weight of the slurry. The dispersing agent, which is an anionic polyelectrolyte, such as polyacrylic, polycarboxylic acids and alkali metal salts thereof, is added in an amount between 0.1 to 3 % by weight of the lime. To this is added an alkali metal hydroxide of 0.1 to 1.5 % by weight of lime. The order of addition of the alkali metal hydroxide is important. The later addition of the alkali metal hydroxide results in a decreased viscosity so that a lower amount of dispersing agent is required.
Abstract translation: 通过将石灰和水中的分散剂组合以形成水性浆料,形成适用于替代苛性碱溶液的可泵送石灰浆料的组合物。 所使用的石灰的量为浆料的35至55重量%。 作为阴离子聚电解质的分散剂,例如聚丙烯酸,多元羧酸及其碱金属盐,其添加量为石灰重量的0.1〜3%。 向其中加入0.1至1.5重量%的石灰的碱金属氢氧化物。 加入碱金属氢氧化物的顺序是重要的。 碱金属氢氧化物的后续添加导致粘度降低,从而需要较低量的分散剂。
-
公开(公告)号:WO1996013550A1
公开(公告)日:1996-05-09
申请号:PCT/US1995012697
申请日:1995-10-12
Applicant: CHEMICAL LIME COMPANY
Inventor: CHEMICAL LIME COMPANY , HUEGE, Fred, R. , GRAVES, Robin, E. , SALTER, Timothy, L. , SHIELDS, Patrick , HAINS, Norman, L.
IPC: C08L95/00
CPC classification number: E01C7/187 , E01C7/26 , E01C19/1004 , E01C23/065
Abstract: A method of treating aggregate for use in hot mix asphalt compositions to promote adhesion between the aggregate material and bituminous binder by mixing together in a mixing tank (12) unslaked quicklime and an aqueous slaking medium to form a quicklime slurry and pumping the slurry through a conduit (70) to be mixed with aggregate from a feed bin (75) at a pugmill (74) of a hot asphalt plant.
Abstract translation: 一种处理用于热混沥青组合物中的骨料的方法,以通过在未沉淀的生石灰的混合罐(12)和水性消化介质中混合在一起以促进骨料和沥青粘合剂之间的粘附,以形成生石灰浆料并将浆料泵送通过 导管(70)与来自热沥青设备的搅拌机(74)的进料仓(75)与骨料混合。
-
-