1.
公开(公告)号:WO2016162348A1
公开(公告)日:2016-10-13
申请号:PCT/EP2016/057465
申请日:2016-04-06
Inventor: GU, Yongming , CHENG, Yuan , GU, Yichen , SUN, Guobin , XIAO, Shuangyin
CPC classification number: B29C70/443 , B29C70/546 , B29K2063/00 , B29K2075/00
Abstract: The present invention relates to a method for manufacturing fiber-reinforced plastic products. This method comprises the following steps of: preparing a fiber preform (2) on a mold (1); disposing first (4a) and second (4b) flow meshes and first (3a) and second (3b) demolding cloths; sealing the fiber preform to form a vacuum system by pumping; penetrating the resin through the first peel ply via the first flow mesh and impregnates the fiber preform from bottom to top; penetrating the resin through the second peel ply via the second flow mesh and impregnates the fiber preform from top to bottom; and attaining a resin-impregnated fiber perform and finally attaining fiber-reinforced plastic products. The invention is characterized in that : a first film (5a) is disposed on a resin-injection side of the fiber perform to cover the first injection port (8a), the first demolding cloth, the first flow mesh and at least a part of the fiber perform, after the resin is supplied to the first flow mesh, the resin is supplied to the second flow mesh when the resin over said fiber perform flows beyond the area covered by the first film.
Abstract translation: 本发明涉及一种纤维增强塑料制品的制造方法。 该方法包括以下步骤:在模具(1)上制备纤维预制件(2); 设置第一(4a)和第二(4b)流动网和第一(3a)和第二(3b)脱模布; 密封纤维预制件以通过泵送形成真空系统; 通过第一流动网穿透树脂穿过第一剥离层,并从下到上浸渍纤维预制件; 通过第二流动网穿透树脂通过第二剥离层,并从上到下浸渍纤维预制件; 并获得树脂浸渍纤维,并最终达到纤维增强塑料制品。 本发明的特征在于:第一膜(5a)设置在纤维的树脂注射侧,以覆盖第一注射口(8a),第一脱模布,第一流 所述纤维的至少一部分在所述树脂供应到所述第一流动网之后,当所述纤维上的树脂流过超过由所述第一膜覆盖的区域时,将所述树脂供给到所述第二流动网。
-
2.
公开(公告)号:WO2017009348A1
公开(公告)日:2017-01-19
申请号:PCT/EP2016/066562
申请日:2016-07-12
Inventor: ZHANG, Chenxi , CHENG, Yuan
CPC classification number: B29C37/0092 , B29B13/06 , B29B13/08 , B29C2035/0855 , B29L2031/085 , C08L63/10 , C08L75/04
Abstract: The present invention relates to an apparatus for drying a material in a mold cavity, comprising: a microwave device (20) for supplying microwave to the material; and a walking device (10) disposed outside the microwave device (20) and allows the microwave device to be movable along a guide rail (11) disposed inside the mold cavity. The present invention also relates to a method for manufacturing a molded article, comprising: a moisture removing step, in which microwave is applied to the material in the mold cavity to phase the moisture contained in the material into vapor by means of the preceding apparatus, and then the vapor in the mold cavity is removed; and an infusing step, in which a macromolecule material resin is infused into the mold cavity under a negative pressure to manufacture the molded article.
Abstract translation: 本发明涉及一种用于干燥模腔中的材料的装置,包括:用于向材料提供微波的微波装置(20); 以及设置在所述微波装置(20)外部并且允许所述微波装置能够沿着设置在所述模腔内部的导轨(11)移动的行走装置(10)。 本发明还涉及一种用于制造模制品的方法,包括:除湿步骤,其中对模腔中的材料施加微波,以通过前述装置使包含在该材料中的水分成蒸汽, 然后去除模腔中的蒸气; 以及在负压下将高分子材料树脂注入模腔中以制造模塑制品的注入步骤。
-
3.
公开(公告)号:WO2016162348A8
公开(公告)日:2016-10-13
申请号:PCT/EP2016/057465
申请日:2016-04-06
Inventor: GU, Yongming , CHENG, Yuan , ZHENG, Yichen , SUN, Guobin , XIAO, Shuangyin
Abstract: The present invention relates to a method for manufacturing fiber-reinforced plastic products. This method comprises the following steps of: preparing a fiber preform (2) on a mold (1); disposing first (4a) and second (4b) flow meshes and first (3a) and second (3b) demolding cloths; sealing the fiber preform to form a vacuum system by pumping; penetrating the resin through the first peel ply via the first flow mesh and impregnates the fiber preform from bottom to top; penetrating the resin through the second peel ply via the second flow mesh and impregnates the fiber preform from top to bottom; and attaining a resin-impregnated fiber perform and finally attaining fiber-reinforced plastic products. The invention is characterized in that: a first film (5a) is disposed on a resin-injection side of the fiber perform to cover the first injection port (8a), the first demolding cloth, the first flow mesh and at least a part of the fiber perform, after the resin is supplied to the first flow mesh, the resin is supplied to the second flow mesh when the resin over said fiber perform flows beyond the area covered by the first film.
Abstract translation: 本发明涉及一种用于制造纤维增强塑料产品的方法。 该方法包括以下步骤:在模具(1)上制备纤维预制件(2); 设置第一(4a)和第二(4b)流动网以及第一(3a)和第二(3b)脱模布; 通过泵送密封光纤预制件以形成真空系统; 通过第一流动网将树脂穿过第一剥离层并从下至上浸渍纤维预制件; 通过所述第二流动网穿过所述第二剥离层,并从上至下浸渍所述纤维预制件; 并获得树脂浸渍纤维制品并最终获得纤维增强塑料制品。 本发明的特征在于:在纤维的树脂注入侧设置第一膜(5a)以覆盖第一注入口(8a),第一脱模布,第一流动网和至少一部分 在将树脂供应到第一流动网格之后,当所述纤维上的树脂流过第一薄膜覆盖的区域时,将树脂供应到第二流动网格。 p>
-
公开(公告)号:WO2016087366A1
公开(公告)日:2016-06-09
申请号:PCT/EP2015/078054
申请日:2015-11-30
Inventor: SUN, Guobin , CHENG, Yuan , GU, Yongming , ZHENG, Ian , XIAO, Shuangyin
CPC classification number: C08G18/7671 , C08G18/10 , C08G18/284
Abstract: The present invention relates to a free radical polymerizable polyurethane composition comprising a polyurethane having active olefinic bond, and a reactive diluent C), wherein the polyurethane having active olefinic bond is prepared by components including (meth) acrylate, and the polyurethane composition has favorable pot-life, improved heat distortion temperature and lower exothermic peak.
Abstract translation: 本发明涉及包含具有活性烯键的聚氨酯的自由基聚合性聚氨酯组合物和反应性稀释剂C),其中具有活性烯键的聚氨酯由包含(甲基)丙烯酸酯的组分制备,并且聚氨酯组合物具有有利的罐 寿命,改善的热变形温度和较低的放热峰。
-
-
-