Abstract:
A process to form a composition comprising a crosslinked olefin-based polymer derived from an anhydride-functionalized olefin-based polymer, said process comprising at least the following steps A) and B) : A) mixing together at least the following components a and b to form a first composition: a) the anhydride-functionalized olefin-based polymer, and b) at least one epoxy-silane compound; B) exposing the first composition to moisture to form the crosslinked olefin-based polymer. The first compositions and crosslinked compositions are also disclosed.
Abstract:
A composition comprising an acid and/or anhydride grafted ethylene/alpha-olefin interpolymer that comprises the following properties: A) number of grafts per polymer chain ≥ 1.80, and B) melt viscosity (at 177℃) ≤ 50,000 mPa.s.
Abstract:
A process to form a composition, said process comprising at least the following steps A) and B) : A) mixing together at least the following components a and b to form a first composition: a) the "anhydride-functionalized olefin-based polymer", and b) at least one multifunctional epoxy compound comprising at least two epoxy groups, or at least one oxetane compound comprising at least one oxetane group; B) exposing the first composition to moisture to form the crosslinked olefin-based polymer. Also, related is first compositions and crosslinked compositions.
Abstract:
A hot melt adhesive (HMA) composition includes (A) from 1-60 wt% of a block composite compatibilizer comprising (i) a hard polymer that includes propylene, (ii) a soft polymer that includes ethylene, and (iii) a block copolymer having a soft block and a hard block, the hard block of the block copolymer having the same composition as the hard polymer of the block composite compatibilizer and the soft block of the block copolymer having the same composition as the soft polymer of the block composite compatibilizer; (B) from 1-70 wt% of a tackifier; (C) from 1-40 wt% of at least one selected from the group of a wax and an oil; and (D) Optionally, from greater than zero to 97 wt% of a polymer component that includes an ethylene-based polymer and/or a propylene-based polymer.
Abstract:
A hot melt adhesive (HMA) composition comprises: a) an ethylene/alpha-olefin multi-block interpolymer that has a melt viscosity (177℃) ≤ 50,000 mPa·s; b) an anhydride and/or carboxylic acid functionalized propylene-based polymer that has a melt viscosity (190℃) ≤ 50,000 mPa·s; c) a tackifier; and d) a wax. Such composition delivers both a high temperature heat resistance and a fast set time.
Abstract:
A composition comprising the following components: A) propylene/ethylene copolymer that has a density ≤ 0.880 g/cc, and a MWD(conv) from 2.00 to 3.00 and a melt viscosity (177C) ≤ 80,000 mPa*s; B) olefin multi-block copolymer that has a density ≤ 0.890 g/cc and a melt index (I2) ≥ 0.5 g/10 min.
Abstract:
The present disclosure provides a composition comprising: A) a propylene/C4-C10 alpha-olefin interpolymer; (i)) a total unsaturation per mole of propylene from 0.010% to 0.030%, (ii) a density from 0.855 g/cc to 0.890 g/cc, and (iii) a melt viscosity, at 177C, from 500 cP to 200,000 cP.