1.
公开(公告)号:WO2013151412A1
公开(公告)日:2013-10-10
申请号:PCT/MY2013/000045
申请日:2013-03-01
Applicant: ECO GREENBUILD INDUSTRIES SDN BHD
Inventor: LOO, MENG HAW , LOO, SHU TING , LOO, SHU LI
CPC classification number: C04B2/00 , C04B14/00 , C04B20/023 , C04B28/02 , C04B28/04 , C04B28/18 , Y02W30/92 , C04B18/06 , C04B18/08 , C04B14/06 , C04B18/101 , C04B22/064 , C04B22/143 , C04B40/0071 , C04B40/024 , C04B2103/32
Abstract: A method of producing a construction material comprising the steps of treating an aqueous slurry of bottom ash and fly ash chemically to prevent heavy metals thereof from deposition, settling the treated slurry to allow the bottom ash and fly ash to sediment and discarding the top aqueous layer of the settled slurry and incorporating the sediment to a mixture of hydrated lime, oil palm ash, mineral particles, a binder and a plasticizer thereby forming the construction material.
Abstract translation: 一种制造建筑材料的方法,包括以下步骤:化学地处理底灰和飞灰的含水浆料,以防止其重金属沉积,使经处理的浆料沉淀,使底灰和飞灰沉淀并弃去顶部水层 的沉淀物并将沉淀物掺入熟石灰,油棕灰,矿物颗粒,粘合剂和增塑剂的混合物中,从而形成施工材料。