Abstract:
A method for shaping a coating on a razor blade, and a razor blade produced using the aforesaid method, are provided. The method includes the steps of; a) providing a razor blade having a tip end defined by at least one tip surface and a cutting edge; b) applying a surface coating having a first thickness on at least one tip surface; and c) shaping the surface coating on the at least one tip surface to have a second thickness using a fluid stream, which second thickness is less than the first thickness.
Abstract:
A method for shaping a coating on a razor blade, comprising the steps of: a) providing a razor blade having a tip end defined by at least one tip surface; b) applying a surface coating having a first thickness on at least one tip surface; and c) shaping the applied surface coating on the at least one tip surface to have a second thickness using a centrifuge, which second thickness is less than the first thickness.