QUENCH HARDENED STEEL
    4.
    发明申请

    公开(公告)号:WO2018138270A1

    公开(公告)日:2018-08-02

    申请号:PCT/EP2018/051971

    申请日:2018-01-26

    Abstract: The present invention relates to a hardenable steel, hardened steel components made from the same, and methods for forming the same. The steel contains relatively high levels of molybdenum in comparison to chromium, silicon and manganese, with the molybdenum providing an excellent combination of hardness and impact strength in the hardened steel. The steel can be cold formed then reheat-quenchhardened with water as the quenching agent with no cracking and optionally no tempering. The steels formed have Vickers hardness levels of over 630 Hv10 (e.g. over 700 Hv10), and impact strengths of over 3 J/cm 2 (e.g. over 20 J/cm 2 ).

    HIGH-STRENGTH STEEL PRODUCT AND METHOD OF MANUFACTURING THE SAME

    公开(公告)号:WO2020120563A1

    公开(公告)日:2020-06-18

    申请号:PCT/EP2019/084620

    申请日:2019-12-11

    Abstract: A high-strength steel product comprising a composition consisting of, in terms of weight percentages, 0.02 % to 0.05 % C, 0.1% to 0.6 % Si, 1.1 % to 2.0 % Mn, 0.01 % to 0.15 % Al, 0.01 % to 0.08 % Nb, 0.5 % or less Cu, 0.5 % or less Cr, 0.7% or less Ni, 0.03 % or less Ti, 0.1 % or less Mo, 0.1 % or less V, 0.0005 % or less B, 0.015 % or less P, 0.005 % or less S, and the remainder being Fe and inevitable impurities, wherein the steel product has a microstructure comprising a matrix consisting of, in terms of volume percentages, 40 % to 80 % quasi-polygonal ferrite,20 % to 40 % polygonal ferrite, 20 % or less bainite, and the remainder being pearlite and martensite of 20%or less.The steel product has a yield strength of at least 400 MPa, an ultimate tensile strength of at least 500 MPa, and a Charpy-V impact toughness of at least 34J/cm 2 at a temperature in the range of -50 °C to -100 °C.

    HOT-ROLLED STEEL STRIP & MANUFACTURING METHOD

    公开(公告)号:WO2020099473A1

    公开(公告)日:2020-05-22

    申请号:PCT/EP2019/081149

    申请日:2019-11-13

    Abstract: Hot-rolled steel strip having a tensile strength greater than 875 MPa and containing in mass-%: C 0.06-0.12, Si 0-0.5, Mn 0.70-2.20, Nb 0.005-0.100, Ti 0.01-0.10, V 0.11-0.40, whereby the total amount of V + Nb + Ti is 0.20-0.40 Al 0.005-0.150, B 0-0.0008, Cr 0-1.0, whereby the total amount of Mn + Cr is 0.9−2.5, Mo 0-0.5, Cu 0-0.5, Ni 0-1.0, P 0-0.05, S 0-0.01, Zr 0-0.1 Co 0-0.1 W 0-0.1 Ca 0-0.005, N 0-0.01, balance Fe and unavoidable impurities, and having a microstructure at ¼ thickness that is: • at least 90% martensite and bainite with island-shaped martensite-austenite (MA) constituents, preferably at least 95% and more preferably over 98%, the remainder being: • less than 5% polygonal ferrite and quasi-polygonal ferrite, preferably less than 2%, 30 more preferably less than 1%, • less than 5% pearlite, preferably less than 2%, more preferably less than 1%, • less than 5% austenite, preferably less than 2%, more preferably less than 1% so that the total area percentage is 100%.