METHOD FOR PRODUCING TINPLATE AND PRODUCT PRODUCED THEREWITH
    1.
    发明申请
    METHOD FOR PRODUCING TINPLATE AND PRODUCT PRODUCED THEREWITH 审中-公开
    生产锡板及其生产产品的方法

    公开(公告)号:WO2014006031A1

    公开(公告)日:2014-01-09

    申请号:PCT/EP2013/063912

    申请日:2013-07-02

    IPC分类号: C25D5/48 C25D11/34 C25D3/30

    摘要: The invention relates to a method for forming a passivation layer on a strip of packaging steel for producing a packaging container or a can, said strip having at least one tinplated surface having excellent sulphide staining resistance. The method comprises the steps of: (i) subjecting said tin-plated surface to an anodic treatment at a pH of from 8 to 12 in a suitable aqueous electrolyte, wherein the suitable electrolyte is a phosphate solution, borate solution, sulphate solution or a carbonate solution, wherein the electrolyte for the anodic treatment does not contain mono-atomic halogen anions (Group 17) such as CI-, F-, wherein the thickness of the tin oxide layer (D), expressed in Coulomb/m2 and representing the total charge needed to reduce the layer to metallic tin is related to anodic treatment time (t), current density (A) by D = E x A x t, where E is the efficiency of the electrochemical reaction, and wherein D is at least 30 C/m2; wherein the electrolyte comprises monoatomic cations from Group 1 or 2 from the periodic table or polyatomic cations, and polyatomic anions; (ii) optionally rinsing and drying the anodically treated tin-plated surface - subjecting the anodically treated tin-plated surface to a chemical passivation treatment free from using hexavalent chromium compounds; (iii) drying of the passivated anodically treated tin-plated surface; (iv) final processing such as oiling, winding, cutting etc.

    摘要翻译: 本发明涉及一种用于在包装用钢带上形成钝化层的方法,用于生产包装容器或罐,所述带具有至少一个具有优异的耐硫化物耐污染性的镀锡表面。 该方法包括以下步骤:(i)在合适的含水电解质中使所述镀锡表面经受8-12的pH值的阳极处理,其中合适的电解质是磷酸盐溶液,硼酸盐溶液,硫酸盐溶液或 碳酸盐溶液,其中用于阳极处理的电解质不含有单原子卤素阴离子(第17族),例如Cl-,F-,其中氧化锡层(D)的厚度以C / L表示,代表 将层减少到金属锡所需的总电荷与阳极处理时间(t),电流密度(A)D = E x A xt有关,其中E是电化学反应的效率,其中D为至少30 C /平方米; 其中电解质包括来自元素周期表第1或2族的单原子阳离子或多原子阳离子和多原子阴离子; (ii)任选地冲洗和干燥阳极处理的镀锡表面 - 对阳极处理的镀锡表面进行化学钝化处理,不使用六价铬化合物; (iii)钝化阳极处理镀锡表面的干燥; (iv)上油,卷绕,切割等最终加工