BIOMASS DIRECT REDUCED IRON
    1.
    发明申请

    公开(公告)号:WO2022061398A1

    公开(公告)日:2022-03-31

    申请号:PCT/AU2021/051094

    申请日:2021-09-20

    Abstract: A method for producing direct reduced iron ("DRI") from iron ore and biomass is disclosed. The method includes heating a batch of iron ore and biomass in each oven chamber of a non-recovery batch oven by a combination (i) the thermal mass of a lining of the oven chamber and (ii) combustion of a fuel gas from at least one other oven chamber and at least partially reducing the iron ore and forming DRI. The method also includes discharging gases from the oven chamber through passageways in a wall and a floor of the oven chamber and further combusting combustible gases and transferring heat to the wall and the floor of the oven chamber as the gases move through the passageways. The method also includes discharging at least a portion of gases from the oven chamber, without passing the gases through passageways in the floor of the oven chamber, and using these gases as a fuel gas in subsequent combustion heating in other batch oven chambers when a first predetermined trigger point is reached. A non-recovery batch oven is also disclosed.

    COLD START-UP METHOD FOR A DIRECT SMELTING PROCESS
    2.
    发明申请
    COLD START-UP METHOD FOR A DIRECT SMELTING PROCESS 审中-公开
    直接燃烧过程的冷启动方法

    公开(公告)号:WO2006119575A1

    公开(公告)日:2006-11-16

    申请号:PCT/AU2006/000624

    申请日:2006-05-12

    CPC classification number: C21C5/04 C21B11/08 C21C5/567 Y02P10/136

    Abstract: A method of cold starting a molten bath-based direct smelting process for producing molten iron in a vessel (3) is disclosed. The method includes a step of preheating the vessel before supplying solid feed materials into the vessel. The method also includes a subsequent step of supplying an oxygen-containing gas and solid feed materials including material for forming slag, iron-containing feed material, and carbonaceous material into the vessel and generating heat and forming a bath of molten material that includes molten iron and molten slag in the vessel. This step includes supplying feed materials to promote formation of molten slag over molten iron in an early stage of developing the molten bath

    Abstract translation: 公开了一种在容器(3)中冷起始用于生产铁水的基于熔池的直接熔炼方法。 该方法包括在向容器提供固体进料之前预热容器的步骤。 该方法还包括以下步骤:向容器中供应含氧气体和固体进料,包括用于形成炉渣,含铁原料和碳质材料的材料,并产生热量并形成熔融材料浴,其包括铁水 和容器中的熔渣。 该步骤包括在显影熔浴的早期阶段提供饲料材料以促进在铁水上形成熔渣