MOLYBDENUM DISULFIDE COATED NON-FERROUS AND FERROUS MATERIALS AND METHODS FOR COATING THE NON-FERROUS AND FERROUS MATERIALS WITH MOLYBDENUM DISULFIDE
    1.
    发明申请
    MOLYBDENUM DISULFIDE COATED NON-FERROUS AND FERROUS MATERIALS AND METHODS FOR COATING THE NON-FERROUS AND FERROUS MATERIALS WITH MOLYBDENUM DISULFIDE 审中-公开
    多晶硅非晶硅和非金属材料和非金属和非金属材料与莫来石分解剂的方法

    公开(公告)号:WO2016004332A1

    公开(公告)日:2016-01-07

    申请号:PCT/US2015/039035

    申请日:2015-07-02

    IPC分类号: C23C2/04

    摘要: The present invention provides methods and systems for applying a coating to a non-ferrous or ferrous material that includes providing a material, a heat source, an immersion tank, and a drying environment. The material is placed within the heat source and heated to a temperature between the range of between about 204.44°C to about 537.78°C (400°F to about 1000°F). The material is immersed within an immersion containing a ratio of molybdenum disulfide solution to water of between about 2:1 to about 4:1 at a temperature between about 26.67°C to about 48.89°C (about 80°F to 120°F), and the material is dried at a temperature between about 51.67°C to about 98.89°C (125°F and 210°F).

    摘要翻译: 本发明提供了将涂层施加到有色金属或含铁金属材料上的方法和系统,该方法和系统包括提供材料,热源,浸渍槽和干燥环境。 将材料放置在热源内并加热至约204.44℃至约537.78℃(400°F至约1000°F)之间的温度。 在约26.67℃至约48.89℃(约80°F至120°F)的温度下,将该材料浸入含有二硫化钼溶液与水的比例在约2:1至约4:1之间的浸渍中, ,并将材料在约51.67℃至约98.89℃(125°F和210°F)之间的温度下干燥。