公开(公告)号:WO2022174283A1
公开(公告)日:2022-08-25
申请号:PCT/AU2022/050076
申请日:2022-02-09
Applicant: LK MANAGEMENT PTY LTD
Inventor: DUNBAR, Karl , WALLACE, Robert
IPC: A01G24/12 , C09K17/08 , C09K17/04 , C09K101/00
Abstract: Described herein are synergetic preparations for enhancing the water holding capacities of solid plant growth medium, consisting of a) ground zeolite, and b) powdered hypocalcic Montmorillonite expanse clay, and optionally c) granular expansive clay. Wherein the ratio of zeolite to Montmorillonite is between 1 to 0.25 and 1 to 30, and the ratio of powdered hypocalcic Montmorillonite expanse clay in the total amount of expansive clay is between 2 and 100%. Further optionally including components which aid product attractiveness, extend soil water retention, and assist plant and soil microbe growth.
-
公开(公告)号:WO2022070761A1
公开(公告)日:2022-04-07
申请号:PCT/JP2021/032418
申请日:2021-09-03
Applicant: デンカ株式会社
Abstract: ガラス化率が70%以上、CaO/Al2O3モル比が1.0~2.7、不純物含有量が15質量%以下であるカルシウムアルミネート、石膏、および、セメントを水又は水溶液中に含有する地盤改良材料スラリーであって、前記カルシウムアルミネートと前記石膏と前記セメントに含まれる塩素の総量が、20ppm~2000ppmであり、前記地盤改良材料スラリーの酸化還元電位が、-0.4~0.1Vである、地盤改良材料スラリーである。
-
公开(公告)号:WO2021161868A1
公开(公告)日:2021-08-19
申请号:PCT/JP2021/003903
申请日:2021-02-03
Applicant: 花王株式会社
Inventor: 島田 聡之
Abstract: フミン酸、フルボ酸、ヒューミン、ビチューメンなどの有機物を含む酸性土の土壌を用いた場合でもソイルセメントの圧縮強度を高めることができる、地盤の改良工法を提供する。強熱減量法によって求められる有機質分量が30%以上である土壌に、水硬性粉体と、水と、下記の(A)成分とを混合する、地盤の改良工法であって、(A)成分を水硬性粉体に対して0.5質量%以上10質量%以下となるように混合する、地盤の改良工法。 (A)成分:水中で、アルミニウムイオン及び/又はカルシウムイオンと、塩化物イオンとを放出する供給源となる1種以上の化合物(但し、水硬性粉体を除く)
-
公开(公告)号:WO2017069807A1
公开(公告)日:2017-04-27
申请号:PCT/US2016/035996
申请日:2016-06-06
Applicant: WORCESTER POLYTECHNIC INSTITUTE
Inventor: TAO, Mingjiang , ZHANG, Mo
CPC classification number: C09K17/08 , C04B28/006 , C04B2111/00732 , E02D3/123 , Y02P40/165 , Y02W30/91 , Y02W30/92 , Y02W30/94 , C04B14/106 , C04B18/0409 , C04B18/08 , C04B18/141
Abstract: Geopolymers are one type of aluminosilicate materials formed through the polymerization of silicate and aluminate tetrahedrons. Geopolymer is used as a non-calcium-based stabilizer to mix with sulfate-rich soils. The stabilized soils were exposed to deionized water for 7 days until the volume of soil samples reached constant. Volumetric expansion of the sulfate-rich soil samples stabilized with metakaolin based geopolymer was 7 times lower than those stabilized with lime while the mechanical strength of stabilized soil samples were significantly improved.
Abstract translation: 地聚合物是通过硅酸盐和铝酸盐四面体的聚合形成的一种类型的硅铝酸盐材料。 地质聚合物被用作非钙基稳定剂与富含硫酸盐的土壤混合。 将稳定的土壤暴露于去离子水中7天,直到土壤样品的体积达到恒定。 用偏高岭土基地聚合物稳定的富含硫酸盐的土壤样品的体积膨胀比用石灰稳定的那些低7倍,而稳定土壤样品的机械强度显着提高。 p>
-
公开(公告)号:WO2008126691A1
公开(公告)日:2008-10-23
申请号:PCT/JP2008/055910
申请日:2008-03-27
CPC classification number: C02F1/281 , B01J20/06 , B09C1/08 , C02F2101/103
Abstract: 【課題】As(III)及びAs(V)の両イオンに対して高い吸着能を示し、かつ吸着剤単独でAs(III)及びAs(V)の両イオンに対して広いpH領域で大きな吸着能を示し、かつ単独で用いることのできる砒素吸着剤及びこれを用いた砒素汚染土壌の不溶化方法、汚染土壌の原位置不溶化方法、重金属汚染水の処理方法並びに砒素吸着剤の使用方法を提供すること。 【解決手段】本発明の砒素吸着剤は、鉄・アルミニウム複水酸化物を少なくとも含み、pH3~11の範囲の砒素汚染水又は砒素汚染土壌に対して、単位重量当たりのAs(V)とAs(III)の吸着量が高く、且つ単位重量当たりのAs(V)吸着量の変動率が10%以内であることを特徴とし、粉末状又はスラリー状として用いる。砒素汚染土壌の不溶化方法は、粉末状の砒素吸着剤を、砒素汚染土壌に対して、0.7wt%~2.0wt%の範囲で添加し、混練して砒素を不溶化することを特徴とする。
Abstract translation: [问题]为了提供对As(III)和As(V)离子具有高吸附能力的砷吸附剂,单独确保在宽范围的pH和pH范围内显示As(III)和As(V)离子的高吸附能力 可以单独使用; 并利用砷吸附剂,不溶解砷污染土壤的方法,原位不溶污染土壤的方法及处理重金属污染水的方法; 以及使用砷吸附剂的方法。 [解决问题的手段]砷吸附剂的特征在于至少含有铁/铝双氢氧化物,每重量的砷污染土壤或砷污染水中吸附的As(V)和As(III)的量大 3〜11个pH范围,以每重量As(V)吸附量的变化率在10%以内。 砷吸附剂以粉末状或浆状形式使用。 不污染砷污染土壤的方法的特点是将0.7〜2.0%的粉末状砷吸附剂添加到砷污染土壤中,混合混合物,从而达到不溶解砷的目的。
-
公开(公告)号:WO2006129884A1
公开(公告)日:2006-12-07
申请号:PCT/JP2006/311475
申请日:2006-06-01
Applicant: 強化土エンジニヤリング株式会社 , 島田 俊介 , 大場 美紀
Abstract: A grout for ground that simultaneously satisfies the mutually conflicting property requirements of when injected in a ground under pressure, not infiltrating in soil grain interstices, and while maintaining fluidity in the ground as well, not departing outside a given range through fractures and forming lumps at a given position, and not only effecting growth to lumps by grout liquid per se as large as possible but also during the period up to attainment of solidification, pushing away surrounding soil grains to thereby increase the density of peripheral soil and sand; and a relevant method of ground reinforcement. There is provided a plastic gel grout injected under pressure through an injection hole disposed in a ground and tending to with time or by dehydration, lose fluidity and form lumps, which plastic gel grout comprises, as active components, components (1) and (3) or components (1), (2) and (3) as follows: (1) silica based non-hardening powdery material (material F), (2) calcium based powdery hardening material (material C), and (3) water (material W). Further, there is provided a method of ground reinforcement using the plastic gel grout.
Abstract translation: 同时满足在压力下注入地面时不会渗入土壤颗粒间隙的同时满足相互矛盾的性能要求的灌浆,同时在地面保持流动性的同时,不会通过断裂和成形团块离开给定范围 给定的位置,不仅通过灌浆液本身尽可能大的增长,而且在固化期间,推挤周围的土壤颗粒,从而增加周边土壤和沙子的密度; 和相关的地面加固方法。 提供了一种在压力下通过设置在地面中的注入孔注入的塑料凝胶灌浆,并随时间或通过脱水倾向于失去流动性并形成团块,塑料凝胶灌浆作为活性组分包含组分(1)和(3) )或组分(1),(2)和(3)如下:(1)二氧化硅基非硬化粉末材料(材料F),(2)钙基粉末硬化材料(材料C)和(3)水 (材料W)。 此外,提供了使用塑料凝胶灌浆的地面强化方法。
-
公开(公告)号:WO2022073252A1
公开(公告)日:2022-04-14
申请号:PCT/CN2020/121126
申请日:2020-10-15
Applicant: 江苏隆昌化工有限公司
IPC: C09K17/40 , C09K17/08 , C09K101/00 , C09K109/00
Abstract: 一种砷污染土壤修复材料,其包括pH值调节剂和修复剂,修复剂的原料包括生物质碳、凹凸棒土、铁基化合物和钙铝水滑石,修复剂的原料重量份配比为:凹凸棒土10-15%、麦饭石20-25%、铁基化合物20-30%、钙铝水滑石25-35%;pH值调节剂为SiO 2含量不少于60%、Al 2O 3含量不少于15%的麦饭石粉末。砷污染土壤修复材料撒施到受污染土壤中,无论酸性还是碱性土壤都能自动调节pH值,降低土壤环境中的砷活性,提高耐砷菌的活性,并通过钙铝水滑石稳定土壤环境,对于修复和改良土壤、减轻环境污染、提高食品安全、提高农作物产量有显著的功效。
-
公开(公告)号:WO2017173737A1
公开(公告)日:2017-10-12
申请号:PCT/CN2016/087207
申请日:2016-06-27
Applicant: 北京高能时代环境技术股份有限公司
Abstract: 一种用于处理铬污染土壤的稳定化药剂及其应用,所述稳定化药剂包括晶容扩增剂、沉淀剂、絮凝剂和pH调节剂,其中,所述晶容扩增剂是水泥或粘土材料的其中之一或其组合;所述沉淀剂为硫化物、多硫化物、亚硫酸盐或焦亚硫酸盐的其中之一或其组合,所述药剂可以显著降低土壤中铬的浸出浓度,并且不会对土壤的性质产生破坏。
-
公开(公告)号:WO2017110999A1
公开(公告)日:2017-06-29
申请号:PCT/JP2016/088341
申请日:2016-12-22
Applicant: 太平洋セメント株式会社
Abstract: 重金属等に汚染された土壌に添加し、混合することで、土壌中の重金属等を不溶化して、重金属等の溶出を抑制することができる不溶化材を提供する。軽焼マグネシアを主成分とする不溶化材であって、不溶化材の全量100質量%中、フォルステライトの含有率が6.0質量%以下であり、かつ、ふっ素(F)の含有率が0.045質量%以下である不溶化材。不溶化材100質量部、および、添加材3~100質量部を含む不溶化混合物であって、上記添加材が、炭酸カルシウム、高炉スラグ、水酸化マグネシウム、第二リン酸カルシウム、硫酸カルシウム、硫酸第一鉄、硫酸アルミニウム、およびゼオライトからなる群より選ばれる一種以上からなる粉末である、不溶化混合物。
Abstract translation: 它被添加到
土壤污染重金属如通过混合,在土壤等不溶化重金属,提供了一种能够抑制重金属的溶出的不溶性物质。 为主的光A不溶化材料烧氧化镁,不溶性物质的总量100质量%,镁橄榄石或更少6.0%(重量)的含量,和氟(F)0的内容。 具有045质量%以下的不溶化材料。 100质量份的不溶解的材料,和含添加剂3至100重量份的不溶于混合物,所述添加剂是碳酸钙,高炉矿渣,氢氧化镁,磷酸二钙,硫酸钙,硫酸亚铁, 硫酸铝和沸石,其中粉末是不溶混合物。 p>
-
公开(公告)号:WO2012144099A1
公开(公告)日:2012-10-26
申请号:PCT/JP2011/074606
申请日:2011-10-26
Applicant: 国立大学法人群馬大学 , 株式会社デイ・シイ , 半井 健一郎 , 鯉渕 清 , 二戸 信和
CPC classification number: B01J20/12 , B09B3/0041 , G21F9/162 , G21F9/34 , G21F9/36
Abstract: カルシウムイオンを含む水に接触しても膨潤性が低下し難い止水性充填材と該止水性充填材を人工多重バリアの充填材とした人工多重バリア用充填材を提供する。Na型ベントナイトを主体とした止水性充填材であって、前記ベントナイトにフライアッシュやシリカフューム等のポゾラン物質を内割りで30重量%以下混和してなる止水性充填材、及び、該止水性充填材を用いた充填材であって、放射性廃棄物処分施設の人工多重バリアに用いられる人工多重バリア用充填材。
Abstract translation: 提供一种阻水填料,其溶胀性能即使在与含有钙离子的水接触时也不容易降低,并且具有所述防水填料作为人造多阻隔填料的人造多屏障填料。 一种主要包含钠膨润土的阻水填料,其通过以内部百分比混合30重量%或更少的火山灰物质如飞灰或硅灰与所述膨润土和使用所述阻水填料的填料获得, 用于放射性废物处理设施的人造多重障碍。
-
-
-
-
-
-
-
-
-