Two-step sealing of anodized aluminum coatings
Abstract:
A method includes providing a workpiece with at least one surface having an anodized aluminum coating and a trivalent chromium sealant. The at least one surface of the workpiece is submerged in a post-treatment sealant solution for 0.5 to 20 minutes. The sealant composition consists essentially of a corrosion inhibitor formulation, a water soluble polymer, an organic complexing agent, and an oxidant. The corrosion inhibitor formulation is formulated from at least one anodic corrosion inhibitor compound, at least one cathodic corrosion inhibitor compound, or a combination thereof. A concentration of each of the corrosion inhibitor formulation, the water soluble polymer, the organic complexing agent, and the oxidant is each in a range of 1-50 mM.