- Patent Title: Multilayer film comprising propylene-ethylene-1-butene terpolymers
-
Application No.: US15750799Application Date: 2016-07-19
-
Publication No.: US11028259B2Publication Date: 2021-06-08
- Inventor: Paola Massari , Caroline Cathelin , Claudio Cavalieri , Marco Ciarafoni , Andrea Felisati , Angelo Ferraro , Giampiero Morini , Fabrizio Piemontesi , Gianni Vitale
- Applicant: BASELL POLIOLEFINE ITALIA S.R.L.
- Applicant Address: IT Milan
- Assignee: BASELL POLIOLEFINE ITALIA S.R.L.
- Current Assignee: BASELL POLIOLEFINE ITALIA S.R.L.
- Current Assignee Address: IT Milan
- Priority: EP15180036 20150806
- International Application: PCT/EP2016/067143 WO 20160719
- International Announcement: WO2017/021137 WO 20170209
- Main IPC: C08L23/14
- IPC: C08L23/14 ; B32B27/32 ; B32B27/08

Abstract:
A multilayer film made from or containing a skin layer made from or containing a polyolefin composition made from or containing:
A) from 19 wt % to 50 wt % of a propylene ethylene copolymer having an ethylene derived units content ranging from 1.5 wt % to 6.0 wt % and
B) from 50 wt % to 81 wt % of a propylene ethylene 1-butene terpolymer having an ethylene derived units content ranging from 1.5 wt % to 6.0 wt % and 1-butene derived units content of between 4.8 wt % to 12.4 wt %;
the sum of the amount of component A) and B) being 100;
the composition being characterized by the following features: molecular weight distribution (MWD), expressed in terms of Mw/Mn, greater than 4.0; the creep and recovery curve measured on the polymer fuse at 200° C. shows a maximum value between 600 and 1200 seconds, lower than 53×10−5 1/Pa.
A) from 19 wt % to 50 wt % of a propylene ethylene copolymer having an ethylene derived units content ranging from 1.5 wt % to 6.0 wt % and
B) from 50 wt % to 81 wt % of a propylene ethylene 1-butene terpolymer having an ethylene derived units content ranging from 1.5 wt % to 6.0 wt % and 1-butene derived units content of between 4.8 wt % to 12.4 wt %;
the sum of the amount of component A) and B) being 100;
the composition being characterized by the following features: molecular weight distribution (MWD), expressed in terms of Mw/Mn, greater than 4.0; the creep and recovery curve measured on the polymer fuse at 200° C. shows a maximum value between 600 and 1200 seconds, lower than 53×10−5 1/Pa.
Public/Granted literature
- US20180223084A1 MULTILAYER FILM COMPRISING PROPYLENE-ETHYLENE-1-BUTENE TERPOLYMERS Public/Granted day:2018-08-09