Abstract:
A polyolefin composition made from or containing:
A) 5-35% by weight of a propylene homopolymer; B) 20-50% by weight of an ethylene homopolymer; and C) 30-60% by weight of a terpolymer of ethylene, propylene and 1-butene derived units.
Abstract:
A nucleated propylene polymer composition made from or containing: A) a propylene homopolymer; B) a copolymer of propylene with ethylene derived units; the nucleated composition having a fraction soluble in xylene at 25° C. between 9.0 and 21.0 wt %, an intrinsic viscosity of the fraction soluble in xylene at 25° C. between 1.0 and 1.9 dl/g, a total melt flow rate between 1.5 and 5 g/10 min and the value of the relation (I): 22.5+0.2*MFR−1.2*Xs+0.2*IV (I) is higher than 5.9; wherein MFR is the melt flow rate of the nucleated composition; IV is the intrinsic viscosity of the fraction soluble in xylene at 25° C.; and Xs is the fraction soluble in xylene at 25° C., the amount of A+B is equal to 100 wt %, and the nucleating agent is selected from the group consisting of aromatic or aliphatic carboxylic acids, aromatic metal phosphates, sorbitol derivatives and talc.
Abstract:
The present disclosure provides an article of manufacture made from or containing a propylene-based terpolymer, having (i) ethylene-derived units in the range from about 0.5 wt. % to about 1.8 wt. %; (ii) 1-butene-derived units in the range from about 1.5 wt. % to about 2.5 wt. %; (iii) a ratio of C2 wt %/C4 wt % in the range from about 0.40 to about 0.80, wherein C2 wt % is the weight percent of ethylene-derived units and C4 wt % is the weight percent of 1-butene-derived units; (iv) a melt flow rate in the range from about 30 g/10 min to about 80 g/10 min; (v) a xylene soluble fraction at 25° C. lower than about 5.0 wt. %; and (vi) a melting point higher than about 140° C. The article can be a container, which can be used for food applications.
Abstract:
Propylene polymer compositions comprising: A) from 70 wt % to 95 wt %, of a random copolymer of propylene with ethylene, containing from 3.5 wt % to 8.5 wt %, of ethylene derived units, having a content of fraction soluble in xylene at 25° C. comprised between 7.1 wt % and 15.2 wt % and having a melting point higher than 142.0° C.; B) from 5 wt % to 35 wt %, of a copolymer of propylene with ethylene, containing from 8.5 wt % to 17.0 wt % of ethylene derived units; the sum A+B being 100; the melt flow rate, MFR (ISO 1133 (230° C., 2.16 kg).) from 0.6 g/10 min to 20.2 g/10 min.
Abstract:
The present disclosure relates to a polypropylene composition for the production of molded articles, such as finished parts for the automotive industry, has melt flow rate (230° C., 2.16 kg) of at least 25 g/10 min and comprising: (A) 50-95% of a composition having an intrinsic viscosity of the fraction soluble in xylene at 25° C. of 3.0-5.0 dl/g; and (A1) 70-95% of a propylene homopolymer having a polydispersity index (PI) of 4.3-10, a fraction insoluble in xylene at 25° C. higher than 90% and an MFR (230° C., 2.16 kg) of 100-250 g/10 min; (A2) 5-30% of a copolymer of propylene with 36-44% of ethylene-derived units; (B) optionally up to 45% of a heterophasic propylene polymer, having an MFR (230° C., 2.16 kg) of 10-25 g/10 min, a flexural modulus higher than 1400 MPa, comprising 5-20% of a copolymer rubber component and 80-95% of a matrix propylene polymer component; (C) 2-10% of an ethylene based elastoplastic copolymer; and (D) optionally up to 20% of talc.
Abstract:
A polyolefin composition comprising: A) from 65 wt % to 85 wt %, of a propylene/ethylene/1-butene terpolymer wherein: i) the content of ethylene derived units ranges from 0.6 wt % to 2.5 wt; ii) the content of 1-butene derived units ranges from 6 wt % to 12 wt %; iii) the fraction soluble in xylene at 25° C. ranges from 3.5 wt % to 20 wt %; B) from 15 wt % to 35 wt % of a propylene/ethylene copolymer having a content of ethylene derived units ranging from 10 wt % to 40 wt %; the copolymer optionally can contains 1-butene derived units in an amount less than 1 wt %; the sum A)+B) being 100.
Abstract:
A masterbatch composition comprising: 70-90% wt of a component (A) being a propylene homopolymer or copolymer of propylene with ethylene or C4-C10 alpha olefins, having a MFRA according to ISO 1133 (230° C./2.16 Kg) ranging from 15 to 70 g/10 min; and 10-30% wt of a component B) being a propylene-ethylene copolymer comprising 25-45% wt of ethylene derived units and having a value of the intrinsic viscosity [η] of the fraction soluble in xylene at room temperature ranging from 5 to 9 dl/g, said masterbatch composition having a total MFR higher than 4 g/10 min, and a value of the flexural modulus measured according to ISO method 178 ranging from 950 to 2000 MPa.
Abstract:
A terpolymer compositions made from or containing:
A) From 80 wt % to 97 wt %; of a first propylene, ethylene, 1-butene terpolymer having:
i) the content of ethylene derived units ranging from 0.5 wt % to 3.2 wt %; ii) the content of 1-butene derived units ranging from 7.2 wt % to 14.8 wt %; and
B) From 20 wt % to 3 wt %; of a second propylene, ethylene, 1-butene terpolymer having:
i) the content of ethylene derived units ranging from 0.5 wt % to 3.2 wt %; ii) the content of 1-butene derived units ranging from 14.4 wt % to 26.5 wt %; and
the terpolymer composition having the melt flow rate, MFR, measured according to ISO 1133 at 230° C. with a load of 2.16 kg, ranging from 3.0 g/10 min to 20.0 g/10 min; the sum of the amounts of A) and B) being 100 wt %.
Abstract:
A multilayer film made from or containing a skin layer made from or containing a polyolefin composition made from or containing: A) from 19 wt % to 50 wt % of a propylene ethylene copolymer having an ethylene derived units content ranging from 1.5 wt % to 6.0 wt % and B) from 50 wt % to 81 wt % of a propylene ethylene 1-butene terpolymer having an ethylene derived units content ranging from 1.5 wt % to 6.0 wt % and 1-butene derived units content of between 4.8 wt % to 12.4 wt %; the sum of the amount of component A) and B) being 100; the composition being characterized by the following features: molecular weight distribution (MWD), expressed in terms of Mw/Mn, greater than 4.0; the creep and recovery curve measured on the polymer fuse at 200° C. shows a maximum value between 600 and 1200 seconds, lower than 53×10−5 1/Pa.
Abstract:
A propylene polymer composition comprising: A) from 81 wt % to 91 wt % of a propylene ethylene copolymer containing from 1.0 wt % to 3.5 wt % of ethylene derived units having a fraction soluble in xylene at 25° C. comprised between 10 wt % and 3 wt %; and a melt flow rate ranging from 5 to 50 g/10 min; B) from 9 wt % to 19 wt %, of a copolymer of propylene and ethylene with from 21.0 wt % to 31.0 wt % of ethylene derived units; the sum A)+B) being 100; the composition having an melt flow rate ranging from 20 to 35 g/10 min; the xylene soluble fraction to 25° C. ranging from 13.0 wt % to 25.0 wt % and the intrinsic viscosity of the fraction soluble in xylene at 25° C. ranging from 0.7 dl/g to 1.9 dl/g.