- 专利标题: Easy-to-tear stretched aliphatic-polyester film
- 专利标题(中): 易撕撕裂的脂肪族 - 聚酯薄膜
-
申请号: US10500799申请日: 2003-01-06
-
公开(公告)号: US20050106345A1公开(公告)日: 2005-05-19
- 发明人: Keizou Kawahara , Shigeto Yoshida , Masayuki Tsutsumi , Daisuke Sakura , Akinobu Nagara , Yoshiko Akitomo , Noriko Takahashi , Naonobu Oda , Kazumoto Imai , Kunio Takeuchi , Hiroshi Nagano , Hisato Kobayashi , Keiji Mori , Yasuhisa Fujita
- 申请人: Keizou Kawahara , Shigeto Yoshida , Masayuki Tsutsumi , Daisuke Sakura , Akinobu Nagara , Yoshiko Akitomo , Noriko Takahashi , Naonobu Oda , Kazumoto Imai , Kunio Takeuchi , Hiroshi Nagano , Hisato Kobayashi , Keiji Mori , Yasuhisa Fujita
- 专利权人: TOYO BOSEKI KABUSH IKI KAISHA
- 当前专利权人: TOYO BOSEKI KABUSH IKI KAISHA
- 优先权: JP2002-821 20020107; JP2002-108199 20020410; JP2002-339238 20021122; JP2002-339239 20021122; JP2002-377516 20021226
- 国际申请: PCT/JP03/00014 WO 20030106
- 主分类号: C08J5/18
- IPC分类号: C08J5/18 ; B65D1/00
摘要:
The easy-to-tear stretched aliphatic polyester film of the present invention is characterized in that the edge tear strength in the longitudinal direction and the transverse direction is not more than 22 N. The easy-to-tear stretched aliphatic polyester film of the present invention is produced by a method of irradiation of actinic rays on an aliphatic polyester film or a method of film-forming a film obtained by laminating aliphatic polyesters having different melting points in three layers of A/B/A under particular film-forming conditions.