Invention Application
- Patent Title: METHOD OF MANUFACTURING NON-AQUEOUS ELECTROLYTE SOLUTION SECONDARY BATTERY AND NON-AQUEOUS ELECTROLYTE SOLUTION SECONDARY BATTERY
-
Application No.: US15676416Application Date: 2017-08-14
-
Publication No.: US20180076450A1Publication Date: 2018-03-15
- Inventor: Koji TORITA , Tatsuya HASHIMOTO , Keiichi TAKAHASHI , Akihiro TANIGUCHI , Shuji TSUTSUMI , Yusuke FUKUMOTO , Yuji YOKOYAMA
- Applicant: TOYOTA JIDOSHA KABUSHIKI KAISHA
- Applicant Address: JP Toyota-shi
- Assignee: TOYOTA JIDOSHA KABUSHIKI KAISHA
- Current Assignee: TOYOTA JIDOSHA KABUSHIKI KAISHA
- Current Assignee Address: JP Toyota-shi
- Priority: JP2016-178432 20160913
- Main IPC: H01M4/36
- IPC: H01M4/36 ; H01M4/505 ; H01M10/0525 ; H01M4/525 ; H01M4/131

Abstract:
A method of manufacturing a non-aqueous electrolyte solution secondary battery includes: (A) preparing a first composite material by mixing a first positive electrode active material, a first conductive material and a first binder; (B) preparing a second composite material by mixing a second positive electrode active material, a second conductive material and a second binder; and (C) manufacturing a positive electrode by forming a positive electrode composite layer including the first composite material and the second composite material. The first positive electrode active material has an average discharge potential lower than that of the second positive electrode active material. The first conductive material has a first OAN. The second conductive material has a second OAN. A ratio of the second OAN to the first OAN is 1.3 or more and 2.1 or less. A sum of the first OAN and the second OAN is 31.64 ml/100 g or less.
Public/Granted literature
Information query