Invention Application
- Patent Title: SURFACE-TREATED STEEL PLATE FOR CELL CONTAINER
-
Application No.: US17512022Application Date: 2021-10-27
-
Publication No.: US20220166092A1Publication Date: 2022-05-26
- Inventor: Kengo Asada , Masao Suda , Kota Sadaki , Hideyuki Minagi
- Applicant: TOYO KOHAN CO., LTD
- Applicant Address: JP Tokyo
- Assignee: TOYO KOHAN CO., LTD
- Current Assignee: TOYO KOHAN CO., LTD
- Current Assignee Address: JP Tokyo
- Priority: JP2015-236710 20151203
- Main IPC: H01M50/124
- IPC: H01M50/124 ; C25D7/00 ; C23C28/02 ; C23C10/20 ; C23C10/30 ; C23C10/02 ; C23C10/18 ; C23C10/28 ; C25D5/48 ; B32B15/04 ; C23C10/08 ; C23C30/00 ; B32B15/18 ; B32B15/01 ; C23C10/60 ; H01M50/10 ; H01M50/107 ; H01M50/116 ; H01M50/213 ; C25D7/06 ; C25D5/50 ; C25D3/12

Abstract:
A surface-treated steel sheet for a battery container, including a steel sheet, an iron-nickel diffusion layer formed on the steel sheet, and a nickel layer formed on the iron-nickel diffusion layer (and constituting the outermost layer, wherein when the Fe intensity and the Ni intensity are continuously measured from the surface of the surface-treated steel sheet for a battery container along the depth direction with a high frequency glow discharge optical emission spectrometric analyzer, the thickness of the iron-nickel diffusion layer being the difference between the depth at which the Fe intensity exhibits a first predetermined value and the depth at which the Ni intensity exhibits a second predetermined value is 0.04 to 0.31 μm; and the total amount of the nickel contained in the iron-nickel diffusion layer and the nickel contained in the nickel layer is 4.4 g/m2 or more and less than 10.8 g/m2.
Public/Granted literature
- US11824212B2 Surface-treated steel plate for cell container Public/Granted day:2023-11-21