公开(公告)号:US11196114B2
公开(公告)日:2021-12-07
申请号:US15780935
申请日:2016-12-05
申请人: TOYO KOHAN CO., LTD.
发明人: Kengo Asada , Masao Suda , Kota Sadaki , Hideyuki Minagi
IPC分类号: H01M2/10 , H01M2/02 , C25D5/50 , C23C28/00 , B32B15/00 , H01M50/10 , H01M50/124 , C25D7/00 , C23C28/02 , C23C10/20 , C23C10/30 , C23C10/02 , C23C10/18 , C23C10/28 , C25D5/48 , B32B15/04 , C23C10/08 , C23C30/00 , B32B15/18 , B32B15/01 , C23C10/60 , H01M50/107 , H01M50/116 , H01M50/213 , C25D3/12 , H01M50/131 , H01M50/155
摘要: A surface-treated steel sheet for a battery container, including a steel sheet, an iron-nickel diffusion layer formed on the steel sheet, and a nickel layer formed on the iron-nickel diffusion layer and constituting the outermost layer, wherein when the Fe intensity and the Ni intensity are continuously measured from the surface of the surface-treated steel sheet for a battery container along the depth direction with a high frequency glow discharge optical emission spectrometric analyzer, the thickness of the iron-nickel diffusion layer being the difference between the depth at which the Fe intensity exhibits a first predetermined value and the depth at which the Ni intensity exhibits a second predetermined value is 0.04 to 0.31 μm; and the total amount of the nickel contained in the iron-nickel diffusion layer and the nickel contained in the nickel layer is 4.4 g/m2 or more and less than 10.8 g/m2.
-
公开(公告)号:US11824212B2
公开(公告)日:2023-11-21
申请号:US17512022
申请日:2021-10-27
申请人: TOYO KOHAN CO., LTD.
发明人: Kengo Asada , Masao Suda , Kota Sadaki , Hideyuki Minagi
IPC分类号: B32B15/04 , B32B15/18 , B32B15/01 , C23C28/02 , C23C10/20 , C23C10/30 , C23C10/02 , C23C10/18 , C23C10/28 , C23C10/08 , C23C10/60 , C23C30/00 , C25D3/12 , C25D7/00 , C25D7/06 , C25D5/48 , C25D5/50 , H01M50/124 , H01M50/10 , H01M50/107 , H01M50/116 , H01M50/213 , H01M50/119 , H01M50/133 , H01M50/134 , H01M50/145 , H01M50/131
CPC分类号: H01M50/124 , B32B15/013 , B32B15/015 , B32B15/04 , B32B15/043 , B32B15/18 , C23C10/02 , C23C10/08 , C23C10/18 , C23C10/20 , C23C10/28 , C23C10/30 , C23C10/60 , C23C28/02 , C23C28/021 , C23C28/023 , C23C30/00 , C23C30/005 , C25D3/12 , C25D5/48 , C25D5/50 , C25D7/00 , C25D7/0614 , H01M50/107 , H01M50/119 , H01M50/1245 , H01M50/133 , H01M50/134 , H01M50/145 , H01M50/213 , B32B2250/03 , B32B2311/22 , B32B2311/30 , B32B2439/00 , H01M50/1243 , H01M50/131 , Y02E60/10 , Y10T428/12937 , Y10T428/12944 , Y10T428/12951 , Y10T428/12958 , Y10T428/12965 , Y10T428/12972 , Y10T428/12979 , Y10T428/12993 , Y10T428/2495 , Y10T428/24942 , Y10T428/24967 , Y10T428/24975 , Y10T428/263 , Y10T428/264 , Y10T428/265 , Y10T428/27
摘要: A surface-treated steel sheet for a battery container, including a steel sheet, an iron-nickel diffusion layer formed on the steel sheet, and a nickel layer formed on the iron-nickel diffusion layer (and constituting the outermost layer, wherein when the Fe intensity and the Ni intensity are continuously measured from the surface of the surface-treated steel sheet for a battery container along the depth direction with a high frequency glow discharge optical emission spectrometric analyzer, the thickness of the iron-nickel diffusion layer being the difference between the depth at which the Fe intensity exhibits a first predetermined value and the depth at which the Ni intensity exhibits a second predetermined value is 0.04 to 0.31 μm; and the total amount of the nickel contained in the iron-nickel diffusion layer and the nickel contained in the nickel layer is 4.4 g/m2 or more and less than 10.8 g/m2.
-
公开(公告)号:US20220166092A1
公开(公告)日:2022-05-26
申请号:US17512022
申请日:2021-10-27
申请人: TOYO KOHAN CO., LTD
发明人: Kengo Asada , Masao Suda , Kota Sadaki , Hideyuki Minagi
IPC分类号: H01M50/124 , C25D7/00 , C23C28/02 , C23C10/20 , C23C10/30 , C23C10/02 , C23C10/18 , C23C10/28 , C25D5/48 , B32B15/04 , C23C10/08 , C23C30/00 , B32B15/18 , B32B15/01 , C23C10/60 , H01M50/10 , H01M50/107 , H01M50/116 , H01M50/213 , C25D7/06 , C25D5/50 , C25D3/12
摘要: A surface-treated steel sheet for a battery container, including a steel sheet, an iron-nickel diffusion layer formed on the steel sheet, and a nickel layer formed on the iron-nickel diffusion layer (and constituting the outermost layer, wherein when the Fe intensity and the Ni intensity are continuously measured from the surface of the surface-treated steel sheet for a battery container along the depth direction with a high frequency glow discharge optical emission spectrometric analyzer, the thickness of the iron-nickel diffusion layer being the difference between the depth at which the Fe intensity exhibits a first predetermined value and the depth at which the Ni intensity exhibits a second predetermined value is 0.04 to 0.31 μm; and the total amount of the nickel contained in the iron-nickel diffusion layer and the nickel contained in the nickel layer is 4.4 g/m2 or more and less than 10.8 g/m2.
-
-