摘要:
A process for the preparation of an alkenyl-substituted succinic anhydride wherein the alkenyl substituent has a number average molecular weight of from about 500 to 5000 and the average number of succinic groups per alkenyl group is greater than 1.2 which comprises: (a) reacting a polyolefin having an alkylvinylidene isomer content of less than about 10 percent and a number average molecular weight of about 500 to 5000 with maleic anhydride at a temperature in the range of about 200 °C to 250 °C to provide a mixture of alkenyl succinic anhydride having an average of about 1.0 succinic group per alkenyl group and unreacted polyolefin, and (b) reacting the mixture of alkenyl succinic anhydride and unreacted polyolefin from step (a) with maleic anhydride in the presence of a free radical initiator at a temperature in the range of about 100 °C to 220 °C to thereby provide an alkenyl succinic anhydride having an average of greater than 1.2 succinic groups per alkenyl group.
摘要:
L'invention se rapporte à un procédé de préparation d'un anhydride succinique à substitution alcényle. Le substituant alcényle possède un poids moléculaire moyen au nombre d'environ 500 à 5000 et le nombre moyen de groupes succiniques par groupe alcényle est supérieur à 1,2. Ce procédé consiste: (a) à faire réagir une polyoléfine ayant une teneur en isomère d'alkylvinylidène inférieure à environ 10 pour cent et un poids moléculaire moyen au nombre d'environ 500 à 5000 avec de l'anhydride maléique, à une température comprise entre environ 200 °C et 250 °C afin d'obtenir un mélange d'anhydride succinique alcényle ayant une moyenne d'environ 1,0 groupe succinique par groupe alcényle et une polyoléfine qui n'est pas entrée en réaction, et (b) à faire réagir le mélange d'anhydride succinique alcényle et la polyoléfine de l'étape (a) qui n'est pas entrée en réaction avec l'anhydride maléique en présence d'un initiateur de radical libre, à une température comprise entre environ 100 °C et 220 °C afin d'obtenir un anhydride succinique alcényle ayant une moyenne supérieure à 1,2 groupes succiniques par groupe alcényle.
摘要:
L'invention porte sur un procédé de préparation d'un anhydride succinique substitué en alcényle dans lequel le substituant d'alcényle présente un poids moléculaire moyen au nombre d'environ 500 à 5000, le nombre moyen de groupes succiniques par groupe alcényle étant supérieur à 1,2. Ce procédé consiste: (a) à faire réagir une polyoléfine présentant une teneur en isomère d'alkylvinylidène de moins de 10 % et un poids moléculaire moyen au nombre d'environ 500 à 5000 avec un anhydride maléique en présence d'un initiateur à radicaux libres, à une température comprise entre 100 °C et 220 °C afin de produire un mélange d'anhydride succinique d'alcényle présentant une moyenne de plus de 1,2 groupes succiniques par groupe alcényle et polyoléfine n'ayant pas réagi, la conversion à environ 30 à 65 %, et, (b) à faire réagir le mélange d'anhydride succinique d'alcényle et la polyoléfine n'ayant pas réagi avec de l'anhydride maléique, à une température de l'ordre de 200 à 250 °C afin de produire un anhydride succinique d'alcényle présentant une moyenne de plus de 1,2 groupes succiniques par groupe alcényle, la conversion totale de la polyoléfine etant de 5 à 40 % supérieure à la conversion dans l'étape (a).
摘要:
An oil-soluble lubricating oil additive composition prepared by the process which comprises reacting a copolymer, with at least one ether compound and with at least one aromatic amine.
摘要:
The present invention aims to provide a surface modification method for a rubber vulcanizate or a thermoplastic elastomer, which can impart various functions such as sliding properties and biocompatibility according to its use. The present invention relates to a surface modification method for modifying a rubber vulcanizate or a thermoplastic elastomer as an object to be modified, the method including: Step 1 of forming polymerization initiation points on a surface of the object to be modified; Step 2 of radical polymerizing monomers starting from the polymerization initiation points to grow polymer chains on the surface of the object to be modified; and Step 3 of functionalizing the polymer chains.
摘要:
Provided are an encapsulation film, an organic electronic device including the same, and a method of manufacturing the organic electronic device. Therefore, provided is the encapsulation film, which may form a structure capable of effectively blocking moisture or water entering the organic electronic device from the outside, and have excellent processability in a process of manufacturing a panel and excellent heat retention under a high-temperature and high-humidity condition.
摘要:
Disclosed is a photocurable elastomer composition that exhibits, when cured, excellent flexibility and barrier properties and has low compression set. The photocurable elastomer composition may comprise components (A) to (D) such that the mass ratio of the component (A) to the component (B) ((A):(B)) is from 25:75 to 75:25, and that the content of the component (C) is 50 mass% or less based on the total content of the components (A), (B), and (C).
摘要:
Disclosed is a photocurable elastomer composition that exhibits, when cured, excellent flexibility and barrier properties and has low compression set. The photocurable elastomer composition may comprise components (A) to (D) such that the mass ratio of the component (A) to the component (B) ((A):(B)) is from 25:75 to 75:25, and that the content of the component (C) is 50 mass% or less based on the total content of the components (A), (B), and (C).