摘要:
A process for reducing or removing at least 90% of sulfur in a tall oil composition, e.g., to a level of 15 ppm or less is disclosed. The process employs at least a first desulfurization and a second desulfurization treatment in parallel or in series. The first treatment comprises adsorptive desulfurization, wherein the adsorbent material comprises silica adsorbent having an average pore size between 50-200 Å, BET surface area of at least 300 mm 2 /, pore volume of 1.20 to 3.00 cc/g, and a silanol [Si-OH] level of 0.5 to 5 unit/nm 2 . The second desulfurization treatment is selected from adsorptive treatment, heat treatment, distillation, extraction, oxidation, reduction, hydrogenation, and sulfur scavenging for a reduced sulfur content.
摘要:
A polymer composition comprising a star-branched copolymer having a plurality of arms is disclosed. Each polymer arm has a molecular weight of from 1 kg/mol to 50 kg/mol and comprises polymerized units (i) derived from a first vinyl aromatic monomer comprising a radical-reactive group, wherein from greater than 10 mol % to 100 mol % of the units (i) are unhydrogenated; and optionally, polymerized units (ii) comprising hydrogenated and unhydrogenated forms of polymerized units derived from a high Tg monomer, and hydrogenated form of polymerized units (i) or hydrogenated form of polymerized styrene units; and optionally, polymerized units (iii) comprising (a) hydrogenated form of polymerized units derived from one or more acyclic conjugated dienes, and (b) polymerized units derived from one or more of a second vinyl aromatic monomer; wherein less than 10 wt. % of units (a) are unhydrogenated.
摘要:
The present invention is directed to a process for preparing a polymer modified bituminous binder composition in the substantial absence of crosslinking agents by heating a bitumen component in a stirred tank to a temperature from 185 °C to 221 °C; adding a block copolymer composition to the bitumen component while the bitumen component is being stirred to form a homogeneous mixture of the bitumen component and the block copolymer composition; and continuing to stir the homogeneous mixture while maintaining the temperature from 185 °C to 221 °C for a period of time from 4 hours to 30 hours thereby forming a cured polymer modified bituminous binder composition. The block copolymer composition utilized in the process comprises a diblock copolymer comprising one block of a monovinylaromatic hydrocarbon and one block of a conjugated diene having a peak molecular weight from 30,000 to 78,000 and a vinyl content from 35 to 80 mol percent based on the number of repeat monomer units in the conjugated diene block, and optionally one or more block copolymers comprising at least two blocks of monovinylaromatic hydrocarbon and at least one block of conjugated diene, the block copolymer selected from linear triblock copolymers having a peak molecular weight that is 1.5 to 3.0 times the peak molecular weight of the diblock copolymer, multiarm coupled block copolymers having a peak molecular weight that is 1.5 to 9.0 times the peak molecular weight of the diblock copolymer, and mixtures thereof, wherein each block copolymer has a vinyl content from 35 to 80 mol percent based on the number of repeat monomer units in the conjugated diene block, wherein when both (i) and (ii) are present in the block copolymer composition, the ratio of (i) to (ii) is greater than 1:1. The present invention is further related to an alternative to this process, a specific class of bituminous binder compositions and concentrates and a specific class of block copolymer compositions.
摘要:
A bituminous composition which comprises a bituminous component and a block copolymer which comprises at least two blocks of a conjugated diene and at least two blocks of a monovinylaromatic hydrocarbon, being of the general formula: S1-B1-S2-B2 wherein B1 is a block of polymerized conjugated diene comprising at least 50 mole% isoprene having an apparent molecular weight of from 180,000 to 400,000, S1 and S2 are blocks of polymerized monovinylaromatic hydrocarbon having a weight average molecular weight of 12,000 to 40,000, and B2 is a block of polymerized conjugated diene comprising at least 50 mole% isoprene having an apparent molecular weight of from 15,000 to 60,000; wherein the weight ratio W of B1 over B2 is in the range of 3.0 to 12.0; and wherein the content of polymerized monovinylaromatic hydrocarbon is in the range from 10 to 35 wt.%.
摘要:
A hydrogenated styrenic block copolymer composition for overmolding onto a polar substrate is provided, comprising: a) 100 pbw of a hydrogenated styrenic block copolymer having at least two resinous endblocks of polymerized monovinyl arene and an elastomeric midblock of polymerized and subsequently hydrogenated conjugated diene or dienes, b) from 25 to 60 pbw of a functionalized polyolefin, and optionally c) from 0 to 100 pbw of a plasticizer, d) from 0 to 200 pbw of one or more fillers and filler deactivators, e) from 0 to 2 pbw of antioxidants, f) from 0 to 100 pbw of a polar engineering thermoplast, wherein component (a) is a linear hydrogenated styrenic block copolymer having an apparent molecular weight in the range of from 200,000 to 500,000 or a radial hydrogenated styrenic block copolymer having an apparent molecular weight in the range of from n times 100,000 to 250,000, n equals the number of polymer arms, and component (a) has a content of hydrogenated 1,2-polymerized conjugated dienes (vinyl content) of greater than 40% and a content of poly(monovinyl arene) in the range of from 20 to 50%,and component (b) is an acid, anhydride or ester functionalized polyolefin having a grafting level of 0.5 to 5%w and a melt flow rate (MFR, ASTM D 1238-95 at Condition L) equal to or greater than 20 g/10 minutes.
摘要:
Disclosed is a thermoplastic gel composition that can be fabricated into an article, such as an air freshener or a gasket, and then be converted into a thermoset gel composition by exposure to radiation. The thermoset composition has better slump resistance at high temperatures compared to the thermoplastic composition. Prior to irradiation, the composition is a thermoplastic and so it can be easily mixed and formed into an article.
摘要:
An asphalt binder is provided, comprising 85 to 97.5 parts by weight of a bitumen and 16 to 2.5 parts by weigh of a polymer composition, wherein the polymer composition comprises:(i) from 2 to 8, preferably from 3 to 6 parts by weight of a styrenic block copolymer having at least two blocks of monovinylaromatic hydrocarbon (A) and at least one block of a conjugated diene (B), wherein the block copolymer composition has a vinyl content of at least 25% by weight, preferably from 25 to 40% by weight, based on the total diene content; (ii) from 0 to 5, preferably from 1 to 3 parts by weight of a styrenic diblock copolymer having one block of monovinylaromatic hydrocarbon (A) and one block of a conjugated diene (B); and (iii) from 0.5 to 3, preferably from 1 to 2.5 parts by weight of an ethylene-vinyl acetate copolymer, wherein the weight ratio of (i) + (ii):(iii) is from 2:1 to 6:1, preferably from 3:1 to 4:1. In addition, an asphalt mix is provided comprising 2 to 8 parts by weight of the asphalt binder of the present invention and 98 to 92 parts by weight of gap-graded aggregate or open-graded aggregate material. Furthermore, a porous pavement is claimed, produced from the open or gap-graded mixes, by compacting the asphalt mix mentioned above.