摘要:
Provided is an optical glass having high refractive index and low dispersibility, and also having high transmittance in the near-infrared region. An optical glass of the present disclosure contains B 2 O 3 and LaF 3 as essential components without containing a Zn component and a component having absorption in the near-infrared region, in which the total content of La 2 O 3 , Gd 2 O 3 , and Y 2 O 3 and the total content of LaF 3 , GdF 3 , and YF 3 are optimized.
摘要翻译:本发明提供折射率高,分散性低,并且近红外区域的透过率高的光学玻璃。 本发明的光学玻璃含有B 2 O 3和LaF 3作为必需成分,其中不含Zn成分和在近红外区具有吸收的成分,其中La 2 O 3,Gd 2 O 3和Y 2 O 3的总含量以及LaF 3, GdF3和YF3进行了优化。
摘要:
To provide an optical system that lengthens the lifetime of a fiber, an optical system 13 guides light beams emitted from a plurality of light emitting parts ep into a single optical fiber 12, the plurality of light emitting parts ep are arranged to be aligned along a first direction d1, and the optical system 13 allows the light beams emitted from the plurality of light emitting parts ep to have different light collection centers which are offset from each other at least in a second direction d2.
摘要:
An oxide glass showing long afterglow and accelerated phosphorescence wherein energy is stored by excitation by a radiant ray such as gamma -ray, X-ray, ultraviolet light or the like and light emission continues for a long time after stopping the excitation. The oxide glass is characterized in that it comprises terbium oxide (Tb2O3) or manganese oxide (MnO), gallium oxide (Ga2O3) or aluminum oxide (Al2O3), an alkali metal oxide or an alkaline earth metal oxide, and, boron oxide (B2O3) or silicon oxide (SiO2) or zinc oxide (ZnO).
摘要:
A method for manufacturing a solid element device, which comprises providing a glass-containing Al 2 O 3 substrate ( 3 ) having a GaN based LED element ( 2 ) placed thereon, setting a P 2 O 5 -ZnO based low melting point glass in parallel with the substrate, and carrying out a press working at a temperature of 415 °C or higher under a pressure of 60 kgf in a nitrogen atmosphere. Under these conditions, the low melting point glass has a viscosity of 10 9 poise, and is adhered via an oxide formed on the surface of the glass-containing Al 2 O 3 substrate ( 3 ) . A solid element device manufactured by the above method can be manufactured through a glass sealing working at a low temperature and also has a highly reliable sealing structure.
摘要:
The invention relates to a light source unit control method and a light source control unit, and a light source unit comprising a filament lamp with a characteristic of having a light quantity changing almost in proportion to a control voltage, which comprise: a current detection sensor connected in series to the lamp; a multiplication circuit for generating a voltage V w proportionate to the product of a terminal voltage V of the lamp and an output voltage V 1 of said current detection sensor; a square root circuit for generating a voltage V 2 proportionate to the square root of the control voltage V 1 ; an error amplifier circuit for controlling an error to the minimum by comparing the output voltage V w of said multiplication circuit and the output voltage V 2 of said square root circuit; and a constant voltage power source unit for supplying an electric power to the filament lamp, the unit being connected to an output terminal of the error amplifier circuit, wherein the light quantity of the lamp is controlled by controlling the control voltage.