摘要:
A method of constructing an earth-boring, diamond-impregnated drill bit has a first step of coating diamond grit with tungsten to create tungsten-coated diamond particles. These coated particles are then encapsulated in a layer of carbide powder held by an organic green binder material. The encapsulated granules are then mixed along with a matrix material and placed in a mold. The matrix material includes a matrix binder and abrasive particles. The mixture is heated in the mold at atmospheric pressure to cause the matrix binder to melt and infiltrate the encapsulated granules and abrasive particles.
摘要:
Earth-boring tools and components thereof include a particle-matrix composite material having encapsulated diamond particles embedded within a matrix material. Diamonds in the particles comprise less than about 25% by volume of the composite material, the matrix material comprises less than about 50% by volume of the composite material, and encapsulant material surrounding the diamonds at least substantially comprises a remainder of the volume of the composite material. Methods of forming at least a portion of an earth-boring tool include embedding encapsulated diamond particles in a volume of matrix material to form a particle-matrix composite material. The composite material is formed in such a manner as to cause diamonds to comprise less than about 25% of the composite material, the matrix material to comprise less than about 50% of the composite material, and encapsulant material surrounding the diamonds to at least substantially comprise a remainder of the composite material,
摘要:
A method of constructing an earth-boring, diamond-impregnated drill bit has a first step of coating diamond grit with tungsten to create tungsten-coated diamond particles. These coated particles are then encapsulated in a layer of carbide powder held by an organic green binder material. The encapsulated granules are then mixed along with a matrix material and placed in a mold. The matrix material includes a matrix binder and abrasive particles. The mixture is heated in the mold at atmospheric pressure to cause the matrix binder to melt and infiltrate the encapsulated granules and abrasive particles.