Abstract:
Thermoplastic polyamide particles comprise at least one polyamide and at least one particulate inorganic filler having a density of at least 2.5 g/cm3, the thermoplastic polyamide particles having a density of at least 1.65 g/cm3, preferably at least 1.9 g/cm3, and an ellipsoidal or approximately ellipsoidal shape with a largest diameter of 1 to 100 mm, preferably 2 to 10 mm, more preferably 3 to 8 mm, or they comprise at least one polyamide and at least one inorganic filler, which is a particulate BaSO4 filler, having a D50-value of the particle size distribution of at least 10 μm and/or a D90-value of at least 15 μm, preferably at least 40 μm.
Abstract translation:热塑性聚酰胺颗粒包含至少一种聚酰胺和至少一种密度为至少2.5g / cm 3的颗粒状无机填料,所述热塑性聚酰胺颗粒的密度为至少1.65g / cm 3,优选至少1.9g / cm 3 以及具有最大直径为1至100mm,优选2至10mm,更优选3至8mm的椭圆形或近似椭圆形的形状,或者它们包含至少一种聚酰胺和至少一种无机填料,其为微粒BaSO 4填料,其粒度分布的D 50值为至少10μm和/或D 90值为至少15μm,优选至少40μm。
Abstract:
A composition comprises polyalkylene terephthalate and terpolymer of alkylene diol, isophthalic acid and terephthalic acid, and polyalkylene terephthalate reinforcing fiber. The composition may be used to form an article, alone or with other thermoplastic material, at lower processing temperature, with higher melt flowability. The article formed is characterized with lower warpage and improved mechanical properties. The article may be useful for automotive, electrical, household, construction, and industrial applications. A method of preparing such thermoplastic polyester is also disclosed.
Abstract:
The invention relates to the use of thermoplastic moulding compounds containing, as essential components, (A) 29-99.99% by weight of a polyester; (B) 0.01-3.0% by weight of an alkali metal salt of nitric acid, phosphoric acid or carbonic acid or mixtures thereof, in relation to 100% by weight (A) and (B), and in addition (C) 0-70% by weight of other additives, the sum of (A) to (C) amounting to 100% by weight, for producing cable sheaths or optical waveguide sheaths by blow moulding, profile extrusion and/or pipe extrusion.
Abstract:
The invention relates to a flame retardant composition, wherein the following components: a) At least one flame retardant component selected from the group consisting of phosphinic acid salts and nitrogen containing compounds; and b) At least one polymeric dispersing agent selected from the group consisting of styrenemaleic acid anhydride copolymers, long chain carboxylic acid salts and aliphatic polyether substituted by acidic groups; and c) A polymer substrate; are present.
Abstract:
A composition comprises polyalkylene terephthalate and terpolymer of alkylene diol, isophthalic acid and terephthalic acid, and polyalkylene terephthalate reinforcing fiber. The composition may be used to form an article, alone or with other thermoplastic material, at lower processing temperature, with higher melt flowability. The article formed is characterized with lower warpage and improved mechanical properties. The article may be useful for automotive, electrical, household, construction, and industrial applications. A method of preparing such thermoplastic polyester is also disclosed.