摘要:
An aluminum alloy having improved strength and ductility, comprising: Cu 3.5-5.8 wt. %, Mg 0.2-1.5 wt. % Mn 0.2-0.5 wt. % Ag 0.2-0.8 wt. % Ti 0.02-0.12 wt. % and optionally one or more selected from the group consisting of Cr 0.1-0.8 wt. %, Hf 0.1-1.0 wt. %, Sc 0.03-0.6 wt. %, and V 0.05-0.15 wt. %, balance aluminum and incidental elements and impurities, and wherein the alloy is substantially zirconium-free.
摘要:
A rolled or forged Al—Zn—Cu—Mg aluminum-based alloy wrought product having a thickness from 2 to 10 inches. The product has been treated by solution heat-treatment, quenching and aging, and the product comprises (in weight-%): Zn 6.2-7.2, Mg 1.5-2.4, Cu 1.7-2.1. Fe 0-0.13, Si 0-0.10, Ti 0-0.06, Zr 0.06-0.13, Cr 0-0.04, Mn 0-0.04, Mn 0-0.04, impurities and other incidental elements ≦̸0.05 each. Alloys per se and aircraft and aerospace uses, as well as methods of making products are also disclosed.
摘要:
The present invention relates to wrought 7xxx aluminum alloy product comprising in weight % Zn 6.7 - 7.4, Mg 1.35 - 1.75, Cu 1.85 - 2.35, Zr 0.04 - 0.14, Mn 0 - 0.5, Ti 0 - 0.15, V 0 - 0.15, Cr 0 - 0.25, Fe ≤0.05, Si≤0.05 with a Fe+Si ≤ 0.08 % and artificially aged wherein the total equivalent aging time t(eq) at 155°C is comprised from 24 hours to 45 hours which permits to optimize the compromise between tensile yield strength and toughness with improved cryogenic fracture toughness and fatigue resistance in corrosive environment.