摘要:
The invention is a rolled and/or forged product, made of an aluminium-based alloy comprising, in % by weight, Cu: 3.2 - 4.0; Li: 0.80 - 0.95; Zn: 0.45 - 0.70; Mg: 0.15 - 0.7; Zr: 0.07 - 0.15; Mn: 0.1 - 0.6; Ag :
摘要:
[Object] To provide a bonded body of an aluminum alloy and a copper alloy and a bonding method for the bonded body, the bonded body being bonded by a novel bonding method which ensures excellent bonding properties, small material deformation during bonding, and high reliability. [Solving Means] A bonded body made of an aluminum alloy and a copper alloy and obtained by employing the aluminum alloy as one member to be bonded and the copper alloy as the other member to be bonded, the one bonded member and the other bonded member being bonded to each other through metallic connection, wherein the one bonded member is made of comprising an aluminum alloy containing Cu: 3.0 mass % to 8.0 mass % and Si: 0.1 mass % to 10 mass % with balance being Al and unavoidable inevitable impurities, and satisfying the chemical formula: C + 2.4 · S · 7.8 where C (mass %) is a Cu concentration and S (mass %) is a Si composition concentration is satisfied, and the other bonded member is made of comprising a copper alloy having a higher solidus temperature than the one bonded member. A bonding method for the bonded body is also provided.
摘要:
The invention relates to a method for manufacturing an aluminium alloy product including the steps of: creating a bath of liquid metal in an aluminium - copper - lithium alloy, casting said alloy by vertical semi-continuous casting so as to obtain a plate with thickness T and width W such that, during solidification, the hydrogen content of said liquid metal bath (1) is lower than 0.4 ml/100 g, the oxygen content above the liquid surface (14, 15) is less than 0.5 % by volume, the tundish used (7) for casting is made of a fabric including essentially carbon, including a lower surface (76), an upper surface defining the opening through which the liquid metal is inserted (71) and a wall with a substantially rectangular section, the wall containing two longitudinal portions parallel to the width W (720, 721) and two transverse portions parallel to the thickness T (730, 731) said transverse and longitudinal portions being formed by at least two fabrics, a first substantially sealing and semi-rigid fabric (77) ensuring that the tundish keeps its shape during casting, and a second non-sealing fabric (78) allowing the passage and filtration of the liquid, said first and second fabrics being connected to one another with no overlap and no gaps separating same, said first fabric continuously covering at least 30 % of the surface of said wall portions (720, 721, 730, 731) and being positioned such that the liquid surface is in contact with same over the entire section.
摘要:
The invention relates to a method for production of thick sheets made from Al-Zn-Cu-Mg type alloys, comprising 4 to 12 % zinc, less than 4 % magnesium, less than 4 % copper, trace elements = 0.5 % each, the remainder being aluminium, said method comprising hot lamination, placing in solution, quenching, controlled drawing with a permanent extension of more than 0.5 % and aging, characterised in that the time D between the end of the quench and the beginning of the controlled drawing is less than 2 hours.