HIGH-PERFORMANCE MICRO-NEEDLE ARRAY
    3.
    发明公开

    公开(公告)号:EP4159266A1

    公开(公告)日:2023-04-05

    申请号:EP21812732.2

    申请日:2021-05-24

    IPC分类号: A61M37/00

    摘要: Provided is a micro-needle array in which all fine needles can be more easily inserted into the skin regardless of positions where the fine needles of the micro-needle array are located on a substrate. The micro-needle array includes: a substrate; and a plurality of micro-needles arranged on one surface of the substrate. Tip parts of the plurality of micro-needles have a height difference, and the micro-needles have a needle length of 80 um or more and 2000 um or less. The height difference of the plurality of micro-needles is preferably based on unevenness of the substrate.

    MICRONEEDLE ARRAY COATED WITH DRUG
    5.
    发明公开

    公开(公告)号:EP3563900A1

    公开(公告)日:2019-11-06

    申请号:EP17888505.9

    申请日:2017-12-28

    IPC分类号: A61M37/00

    摘要: To provide a practical microneedle preparation which solves a problem that, even if a tip portion of the microneedle could be quantitatively coated with the drug, the drug remained in the stratum corneum when actually applying the microneedle array as a transdermal absorption preparation.
    A microneedle array having needles with a length of 350 µm to 900 µm, and a tip apex diameter of 20 µm to 100 µm, including drug-coated portions, and comprising a non-biosoluble polymer as a base, wherein a lower end of each drug-coated portion is 200 µm or more away from a root of the needle.

    MICRONEEDLE AND METHOD FOR PRODUCING SAME
    6.
    发明公开
    MICRONEEDLE AND METHOD FOR PRODUCING SAME 审中-公开
    MICRONEEDLE及其生产方法

    公开(公告)号:EP3275500A1

    公开(公告)日:2018-01-31

    申请号:EP15886513.9

    申请日:2015-12-10

    IPC分类号: A61M37/00

    摘要: Provided are a microneedle with excellent performance and a method for manufacturing the microneedle.
    A microneedle array in which a polyglycolic acid is used as a material, crystallinity of the polyglycolic acid is 21% or more and axial contraction rate of tips is 99 % or more, and a manufacturing method in which a polyglycolic acid are injection-molded at a cylinder temperature of 230 - 280 °C, a metal mold temperature of 60 - 130 °C, and an injection pressure of 1000 - 1500 KPa so as to manufacture a microneedle array in which crystallinity of the polyglycolic acid is 21 % or more and an axial contraction rate of tips is 99 % or more.

    摘要翻译: 本发明提供一种性能优异的微针和微针的制造方法。 其中使用聚乙醇酸作为材料,聚乙醇酸的结晶度为21%以上且尖端的轴向收缩率为99%以上的微针阵列以及聚乙醇酸注射成型于其中的制造方法 筒体温度230〜280℃,金属模具温度60〜130℃,注射压力1000〜1500KPa的条件下进行制造,制造聚乙醇酸的结晶度为21%以上的微针阵列, 尖端的轴向收缩率为99%以上。

    HIGH-PERFORMANCE MICRONEEDLE ARRAY
    8.
    发明公开

    公开(公告)号:EP4389189A1

    公开(公告)日:2024-06-26

    申请号:EP22858534.5

    申请日:2022-08-19

    IPC分类号: A61M37/00

    CPC分类号: A61M37/00

    摘要: Provided is a microneedle array having high bioavailability and pharmacological availability. A microneedle array including a needle portion and a substrate portion, in which the needle portion contains a valuable material in a base containing a water-soluble polymer as a main component, the substrate portion does not contain the valuable material, and the base of the substrate portion contains a water-insoluble polymer as a main component.