摘要:
A primary object of the present invention is to provide a film exhibiting high electrical insulation properties and excellent withstand voltage properties and a method for producing the film. As a means for achieving the object, the present invention provides a vinylidene fluoride-based polymer film in which the 99% voltage failure resistance value in a Weibull plot is 300 V/µm or more.
摘要:
The present invention provides a film having excellent heat resistance and a small difference between the permittivity at low temperatures and the permittivity at high temperatures. The present invention provides a film having a relative permittivity of 8 or more at a frequency of 1 kHz at 30°C, wherein the rate of change is - 8 to +8% as calculated from a relative permittivity A at a frequency of 1 kHz at 30°C and a relative permittivity B at a frequency of 1 kHz at 150°C according to the following formula: Rate of change % = B − A / A × 100.
摘要:
There is provided a protection cover of solar cell having processability at room temperature, solvent resistance, weather resistance and durability without impairing its transparency, and also a curable fluorine-containing coating composition being capable of forming the protection cover. The curable fluorine-containing coating composition for a protection cover of solar cell comprises (A) a curable fluorine-containing resin, (B) a curing agent and (C) a solvent and is used for forming a top coat layer (III) of a cured article comprising the fluorine-containing resin, in which the top coat layer is provided, directly or via a primer layer (IV), on a transparent resin layer (II) provided on the sunlight irradiation side of a solar cell module (I).
摘要:
Provided is a method for producing an injection molded article for obtaining an injection molded article by injection molding a copolymer using an injection molding machine and a mold having a hot runner, wherein the copolymer is a copolymer containing tetrafluoroethylene unit and a fluoroalkyl vinyl ether unit, and the number of functional groups of the copolymer is 100 or less per 10 6 main-chain carbon atoms.
摘要:
Provided is a molded article comprising a copolymer comprising a tetrafluoroethylene unit and a perfluoro(alkyl vinyl ether) unit, wherein a surface roughness Ra of the molded article is 0.20 µm or less, and a water contact angle of the molded article is 80 degrees or less.
摘要:
An object of the present invention is to provide a touch panel that is hardly affected by pyroelectric noise due to temperature changes. As a means for achieving the above object, the present invention provides a touch panel 2. The touch panel 2 comprises a first pyroelectric material 26 and a second pyroelectric material 27, and is capable of detecting press pressure applied to the first pyroelectric material 26 and/or the second pyroelectric material 27. The upper surface of the first pyroelectric material 26 and the lower surface of the second pyroelectric material 27 are surfaces on which a positive charge is generated when the temperature increases, and a negative charge is generated when the temperature decreases. The lower surface of the first pyroelectric material 26 and the upper surface of the second pyroelectric material 27 are surfaces on which a negative charge is generated when the temperature increases, and a positive charge is generated when the temperature decreases. An electrode disposed on the first surface of the first pyroelectric material 26 and an electrode disposed on the first surface of the second pyroelectric material 27 are electrically connected to each other, and an electrode disposed on the second surface of the first pyroelectric material 26 and an electrode disposed on the second surface of the second pyroelectric material 27 are electrically connected to each other.
摘要:
An object of the present invention is to provide a polarized vinylidene fluoride/tetrafluoroethylene copolymer resin film that can significantly reduce, when used as an optical film, the deterioration of the quality of video or still images formed by display elements. The present invention provides a polarized vinylidene fluoride/tetrafluoroethylene copolymer resin film having 2,000 or fewer spot defects per m 2 , the number of spot defects being measured by a defect measurement method; the method using an surface inspection system in which a CCD camera is placed so as to detect defects at an angle of 45 degrees relative to an LED source, defects of the film are read within a rectangular range of 300 mm in a width direction (the direction perpendicular to the scanning direction), and 150 mm in a machine direction (the scanning direction), while the film is scanned under the camera at a rate of 20 m/min; wherein first, defects having a bright area of 1.5 mm 2 or less and a dark area of 1.4 mm 2 or less are selected; and next, in order to remove defects resulting from causes other than a corona treatment contained in these defects, a circumscribed rectangle of defect is set so as to have two sides along the scanning direction, and the number of only defects that have a circumscribed width of 2.88 mm or less, a circumscribed length of 2.3 mm or less, an aspect ratio of -39 to +27, an occupancy area ratio in the circumscribing rectangle of 4,000 to 6,950, and an area ratio of -3,100 to +5,200, is automatically counted as spot defects by the surface inspection system.
摘要:
Provided is a method for producing a tube, comprising: extruding a melt-fabricable fluororesin from a mold of an extruder into a form of a tube, leading the extruded melt-fabricable fluororesin to a cooling device to cool the extruded melt-fabricable fluororesin, and winding a resulting cooled tube onto a winding reel using a winding device, wherein a gas is fed from a head end of the tube wound onto the winding reel into a hollow of the tube, the gas in the hollow is allowed to pass through a gas-introducing entrance of the mold and then through a gas-discharging hole of the mold to discharge the gas outside, thereby allowing the gas to flow along the hollow, and an internal pressure of the hollow is kept higher than atmospheric pressure and lower than 0.5 kgf/cm 2 .
摘要:
The present invention provides a welded body having a connecting structure formed by welding a first molded body and a second molded body, wherein the first and second molded bodies contain at least one copolymer selected from the group consisting of a tetrafluoroethylene/fluoro(alkyl vinyl ether) copolymer and a tetrafluoroethylene/hexafluoropropylene copolymer, and wherein the connecting structure has a liquid contact surface to be in contact with a liquid having a solubility parameter of 14 to 35 (MPa) 1/2 , a welded part formed in the connecting structure is not exposed to the liquid contact surface, and the number of particles of 30 nm or larger to be eluted from the liquid contact surface in the connecting structure is 1,000 particles/ml or less.