摘要:
A flame-retardant composition having (a) a copolymer comprising at least about 50 wt. % of propylene-derived units, and about 5-35 wt. % of units derived from at least one of ethylene or a C4-10 alpha-olefin, wherein the copolymer has a heat of fusion of about 75 J/g or less; and (b) a flame retardant, wherein the composition satisfies the requirements of UL94 with a V2 rating.
摘要:
A flame-retardant composition having (a) a copolymer comprising at least about 50 wt. % of propylene-derived units, and about 5-35 wt. % of units derived from at least one of ethylene or a C4-10 alpha-olefin, wherein the copolymer has a heat of fusion of about 75 J/g or less; and (b) a flame retardant, wherein the composition satisfies the requirements of UL94 with a V2 rating.
摘要:
A tire tread composition is disclosed. The tire tread composition includes components, by weight of the composition, within the range from: 5 to 75 wt % of a diene elastomer; 0 to 40 wt % of processing oil; 20 to 80 wt % of filler; a curative agent; and 5 to 30 wt % of a propylene-ethylene-diene terpolymer containing from 2 wt % to 40 wt % of ethylene and/or C4-C20 α-olefins derived units, from 0.5 to 10 wt % of diene derived units, and having a heat of fusion, as determined by DSC, of from 0 J/g to 80 J/g.
摘要:
A tire tread composition is disclosed. The tire tread composition includes components, by weight of the composition, within the range from: 5 to 75 wt % of a diene elastomer; 0 to 40 wt % of processing oil; 20 to 80 wt % of filler; a curative agent; and 5 to 30 wt % of a propylene-ethylene-diene terpolymer containing from 2 wt % to 40 wt % of ethylene and/or C4-C20 α-olefins derived units, from 0.5 to 10 wt % of diene derived units, and having a heat of fusion, as determined by DSC, of from 0 J/g to 80 J/g.
摘要:
A polyolefin-polybutadiene block-copolymer and a tire tread composition comprising the polyolefin-polybutadiene block-copolymer, the composition comprising, by weight of the composition, within the range from 15 to 60 wt % of a styrenic copolymer, processing oil, filler, a curative agent, and from 4 to 20 wt % of a polyolefin-polybutadiene block-copolymer, wherein the polyolefin-polybutadiene block-copolymer is a block copolymer having the general formula PO-XL-fPB; where “PO” is a polyolefin block having a weight average molecular weight within the range from 1000 to 150,000 g/mole, the “fPB” is a functionalized polar polybutadiene block having a weight average molecular weight within the range from 500 to 30,000 g/mole, and “XL” is a cross-linking moiety that covalently links the PO and fPB blocks; and wherein the maximum Energy Loss (Tangent Delta) of the immiscible polyolefin domain is a temperature within the range from −30° C. to 10° C.
摘要:
A composition including at least one elastomer, and a hydrocarbon polymer additive having a dicyclopentadiene, cyclopentadiene, and methylcyclopentadiene derived content of about 40 wt % to about 80 wt % of the total weight of the hydrocarbon polymer additive, a weight average molecular weight of about 100 g/mole to about 800 g/mole, and a softening point of about 110° C. to about 150° C. as determined in accordance with ASTM D6090.