Le procédé consiste à a) façonner un mélange en poudre sensiblement homogène de nitrure de silicium, 6 à 18 % d'oxynitrure de silicium yttrium de la phase Y10Si6O24N2 en une quantité permettant de former une solution visqueuse avec au moins une partie du nitrure de silicium, et b) densifier le corps par thermofusion, avec ou sans utilisation de pression mécanique, jusqu'à obtenir la densité et les dimensions requises par le produit final.
摘要:
The method comprises: (a) shaping a substantially homogeneous powder mixture of silicon nitride, 6-18% yttrium silicon oxynitride of the Y10Si6O24N2 phase in an amount to form a viscous solution with at least a portion of the silicon nitride, and (b) densifying the body by heat fusion, with or without the use of mechanical pressure, to a density and a dimension required for the final product.
摘要:
Procédé de production d'un additif en poudre consistant en des oxynitrures de silicium yttrium, de préférence des phases Y10Si6O24N2 ou YSiO2N. Des quantités stoechiométriques de Y2O3, SiO2 et Si3N4 sont mélangées et disposées en contact étroit de réaction, ces quantités permettant de former un oxynitrure selon la formule YaSibOcNd, où a, b, c et d représentent les parties requises des éléments du composé en équilibre avec les éléments du mélange. Le mélange est chauffé dans une atmosphère inerte à une température et pendant une durée de temps suffisantes pour convertir les quantités stoechiométriques du mélange en l'oxynitrure de silicium yttrium désiré. Le mélange aggloméré sous l'effet de la chaleur est ensuite broyé de manière à obtenir une poudre.
摘要:
A method for making a more densified silicon nitride comprising object under less stringent heating conditions without sacrificing physical properties. A mixture of silicon powder, 6-18% yttrium silicon oxynitride (a major proportion of which is the Y10Si6O24N2 phase), .4-3% Al2O3, and possibly up to 2% of an oxynitride forming oxide (Y2O3) is compacted, nitrided, and sintered to produce a silicon nitride/YSiO2N comprising object of relatively high density.
摘要:
A method of making a powder additive consisting of yttrium silicon oxynitrides, preferably of the Y10Si6O24N2 or YSiO2N phases. Stoichiometric amounts of Y2O3, SiO2, and Si3N4 are mixed and arranged in intimate reactive contact, the amounts being to form a desired oxynitride according to the formula YaSibOcNd, where a, b, c and d represent the required element parts of the compound in equilibrium with the mixture elements. The mixture is heated in an inert atmosphere to a temperature and for a time sufficient to convert the stoichiometric amounts of the mixture to the desired yttrium silicon oxynitride. The heat agglomerated mixture is then ground to a powder.
摘要:
Procédé permettant de produire un objet comportant du nitrure de silicium plus densifié dans des conditions de chauffe moins strictes sans détérioration des propriétés physiques. Un mélange de poudre de silicium, 6 à 18 % d'oxynitrure de silicium d'yttrium (dont la partie principale est constituée par la phase Y10Si6O24N2), 0,4 à 3 % d'Al2O3, et éventuellement jusqu'à 2 % d'un oxyde formant un oxynitrure (Y2O3), est compacté, nitruré et fritté pour produire un objet comportant du nitrure de silicium/YSiO2N de densité relativement élevée.