SELF-HEALING ELASTOMER AND PROCESS FOR ITS PREPARATION
    1.
    发明公开
    SELF-HEALING ELASTOMER AND PROCESS FOR ITS PREPARATION 审中-公开
    SELBSTHEILENDES ELASTOMER UND VERFAHREN ZUR HERSTELLUNG DAVON

    公开(公告)号:EP3110877A1

    公开(公告)日:2017-01-04

    申请号:EP14707734.1

    申请日:2014-02-28

    IPC分类号: C08G79/00 C08G18/00

    摘要: The self-healing cross-linked polymer comprises units of formula (I), wherein: P is a polymeric chain, R1 and R1' are independently selected from the group consisting of: -H, (C1-C20)alkyl, (C5-C14)aryl, -OR4, -(CO)R5, -O(CO)R6, -(SO)R7, -NH-CO-R8, -COOR9, -NR10R11, -NO2, and halogen; R2, R2', R3 and R3' are independently selected from the group consisting of: -H, (C1-C20)alkyl and (C5-C14)aryl; R4 to R11 are the same or different, and are selected from the group consisting of: -H, (C1-C20)alkyl, and (C5-C14)aryl; m is from 3 to 4;n is from 1 to 2; provided that n + m is 5; the polymer having H-bonding interactions and being able to undergo catalyst free aromatic disulfide metathesis at room-temperature, and having a tensile strength value from 0.5 to 1.5 MPa and an elongation at break value higher than 200% at room- temperature. (I)

    摘要翻译: 自愈交联聚合物包含式(I)单元,其中:P是聚合链,R1和R1'独立地选自:-H,(C1-C20)烷基,(C5- C14)芳基,-OR4, - (CO)R5,-O(CO)R6, - (SO)R7,-NH-CO-R8,-COOR9,-NR10R11,-NO2和卤素; R2,R2',R3和R3'独立地选自:-H,(C1-C20)烷基和(C5-C14)芳基; R 4至R 11相同或不同,并且选自:-H,(C 1 -C 20)烷基和(C 5 -C 14)芳基; m为3〜4; n为1〜2; n + m为5; 所述聚合物具有H-键相互作用并且能够在室温下进行无催化剂的芳族二硫化物复分解,并且在室温下的拉伸强度值为0.5-1.5MPa,断裂伸长率高于200%。 (一世)