摘要:
A ductile boron bearing nickel based welding material which includes boron within the range of 0.4 - 0.6 wt. % B, carbon from a trace amount to 0.04 wt. % C, 17 - 23 wt. % Cr, 0.35 - 10 wt. % Mo, 0.1 - 4.15 wt. % Nb with nickel or iron and impurities to balance for manufacturing of welding and brazing wires, powders and foils used in the repair of various articles made of nickel, cobalt and iron based alloys.
摘要:
The present concept is a method of cladding and fusion welding of superalloys and includes the steps of firstly application of a composite filler powder that consists of 5-50% by weight brazing powder which includes melting point depressants, and 50-95% by weight high temperature welding powder, to a superalloy base material. Secondly there is simultaneous heating of the base material and the composite filler powder by a welding heat source that is movable relative to the base material. There is heating to a temperature that will fully melt the brazing powder and at least partially melt the high temperature welding powder and also melt a surface layer of the base material, thereby forming a weld pool. Thirdly upon solidification and cooling of the weld pool, there is coalescence between the weld bead and the base material.
摘要:
A precipitation strengthened nickel based welding material that comprises 5-15 wt. % Co, 5-25 wt. % Cr, 1-6 wt. % Al, 0.05-0.2 wt. % C, 0.015-0.4 wt. % B, 1-3 wt. % Si, chemical elements selected from among tungsten and molybdenum from about 1 to 20 wt. %, chemical elements selected from among titanium, zirconium, hafnium, tantalum and rhenium from about 1 to 18 wt. % and nickel with impurities to balance, wherein the boron content is inversely proportional to silicon content and decreases from about 0.3 wt. % to about 0.015 wt. % when silicon content increases from about 1 wt. % to about 3 wt. % produces sound high strength and high oxidation resistance crack free welds on precipitation strengthened superalloys and single crystal materials.
摘要:
The present invention is a composite welding wire for fusion welding of components manufactured of superalloys. The composite weld wire includes an inner core wire and a surface layer applied and bonded to the inner core wire. The surface layer includes alloying elements selected from among B and Si with a total bulk content of B and Si in the composite welding wire of 0.1 to 10 wt. %. Preferably the total bulk content of B is less than 4 wt. % and the surface layer comprises from 5 to 95 wt.% of the alloying elements selected from among B and Si.
摘要:
This invention relates to a composition for repairing metallic articles which in its initial state is in the form of an adhesive, self-supporting putty, capable of being molded including 5-15 % by weight of a sacrificial binder containing at least one acrylic resin and volatile solvent. The invention also relates to a kit for the composition and methods for repair.
摘要:
This invention relates to a composition for repairing metallic articles which in its initial state is in the form of an adhesive, self-supporting putty, capable of being molded including 5-15 % by weight of a sacrificial binder containing at least one acrylic resin and volatile solvent. The invention also relates to a kit for the composition and methods for repair.
摘要:
A ductile boron bearing nickel based welding material which includes boron within the range of 0.4 - 0.6 wt. % B, carbon from a trace amount to 0.04 wt. % C, 17 - 23 wt. % Cr, 0.35 - 10 wt. % Mo, 0.1 - 4.15 wt. % Nb with nickel or iron and impurities to balance for manufacturing of welding and brazing wires, powders and foils used in the repair of various articles made of nickel, cobalt and iron based alloys.