摘要:
Disclosed are a reinforcing fiber bundle composed of a carbon fiber bundle treated with an emulsion; a carbon fiber reinforced thermoplastic resin molded body using the same; and a method for producing a reinforcing fiber bundle; wherein the emulsion contains a modified polyolefin (A1) comprising at least a metal carboxylate bonded to the polymer chain, and 0.1 to 5,000 moles of an amine compound (B) represented by the following general formula (1), per one mole of the carboxylate group in the modified polyolefin (A1);
R-NH 2 (1)
wherein the formula (1), R is a hydrogen atom or a hydrocarbon group having 1 to 10 carbon atoms.
摘要:
The invention provides a polymeric piezoelectric material including a helical chiral polymer having a weight-average molecular weight of from 50,000 to 1,000,000 and having optical activity, wherein a crystallinity of the material measured by a DSC method is from 20% to 80%, and a product of a standardized molecular orientation MORc measured by a microwave transmission type molecular orientation meter based on a reference thickness of 50 µm and the crystallinity is from 25 to 250.
摘要:
The invention provides a polymeric piezoelectric material including a helical chiral polymer having a weight-average molecular weight of from 50,000 to 1,000,000 and having optical activity, wherein a crystallinity of the material measured by a DSC method is from 20% to 80%, and a product of a standardized molecular orientation MORc measured by a microwave transmission type molecular orientation meter based on a reference thickness of 50 µm and the crystallinity is from 25 to 250.
摘要:
The present invention provides a polymeric piezoelectric material comprising an aliphatic polyester (A) with a weight-average molecular weight of from 50,000 to 1,000,000 and having optical activity, and a stabilizing agent (B) with a weight-average molecular weight of from 200 to 60,000 having at least one kind of functional group selected from the group consisting of a carbodiimide group, an epoxy group and an isocyanate group, wherein the crystallinity of the material obtained by a DSC method is from 20% to 80%, and a content of the stabilizing agent (B) is from 0.01 part by mass to l 0 parts by mass with respect to 100 parts by mass of the aliphatic polyester (A), as well as a process for producing the same.