摘要:
A resin-coated high-tension flat steel wire includes a high-tension flat steel wire and a fiber-reinforced polyamide resin coated layer. A shape of the high-tension flat steel wire when viewed from a section perpendicular to a longitudinal direction thereof is a rectangular shape including curved portions at four comers thereof. When, among four straight lines that form the rectangular section, the ranges from both end points of the straight lines that form long sides to one fourth of the length of the straight lines are respectively defined as one-fourth segments, a shape of the fiber-reinforced polyamide resin coated layer in the rectangular section includes a mountain shape having an apex within each of the one-fourth segments, and includes a minimum point, where the thickness of the fiber-reinforced polyamide resin coated layer is the minimum, between the apex and both the ends within each of the one-fourth segments.
摘要:
A flat steel wire has a rectangular shape with rounded corners when a cross section perpendicular to a longitudinal direction is viewed. In the flat steel wire: a short side of the cross section is 2 mm to 7 mm; a long side of the cross section is longer than 8 mm to 56 mm; a ratio of the long side to the short side is more than 4 to 8; a tensile strength is 1900 MPa or more; and a twisting value is 12 times or more.
摘要:
The present invention provides a steel wire rod with stable workability. The steel wire rod has steel components containing, by mass%, C: 0.20 to 0.60%, Si: 0.15 to 0.30%, Mn: 0.25 to 0.60%, P: ‰¤0.020%, S: ‰¤0.010%, and a balance of Fe and unavoidable impurities, and an internal microstructure including cementite, in which by number ratio, 80% or more of the cementite in a cross-section vertical to a longitudinal direction of the wire rod has a short axis of 0.1 µm or less and a ratio of a long axis to the short axis, defined as an aspect ratio, of 2.0 or less.
摘要:
A wire rod according to the present invention includes a predetermined chemical composition and the remainder thereof includes Fe and impurity, wherein the average value of a grain size of a pearlite block in a cross section perpendicular to a wire rod axial direction is 23µm or less, and wherein a number density of the pearlite blocks having a grain size of 40µm or more in the cross section perpendicular to the wire rod axial direction is 0 to 20 pieces/mm 2 .