摘要:
Provided is a method comprises: continuously forming an elongated, glass film having marginal portions from molten glass into a given shape having two marginal portions, in width-directional opposite edge regions thereof, wherein the glass film having marginal portions has the marginal portions, and an effective portion formed in a width-directional central region of the glass film having marginal portions; annealing the glass film having marginal portions; continuously forming resin tapes on the glass film having marginal portions at positions adjacent to and away by a given distance from the respective marginal portions, to extend in a length direction of the glass film having marginal portions; and continuously removing each of the marginal portions from the glass film having marginal portions, along a position between the marginal portion and a corresponding one of the resin tapes, or at a given width-directional position within the corresponding resin tape.
摘要:
Provided is a laminate (1) obtained by integrally laminating glass sheets (4) on both surfaces of a resin sheet (2). The glass sheets (4) have a thickness of 300 µm or less and end surfaces (4a) of the glass sheets (4) are chamfered.
摘要:
A surface light-emitting device includes a light guide plate (1) comprising glass plates (12) respectively in close contact with and fixed to both surfaces of a resin plate (11) via adhesive layers (14), and a light source (2) for causing light to enter the light guide plate from one end surface of the light guide plate (1). As the light source (2), a light source having a blue central wavelength in a wavelength range of 460 nm or more and 490 nm or less, or a light source having a blue central wavelength in a wavelength range of 440 nm or more and less than 460 nm and having a color temperature of 4,000 K or lower is used.
摘要:
Provided is a glass-resin laminate (1) having a laminating structure of at least three layers, the glass-resin laminate (1) including: a layer including a glass sheet (2); a layer including a resin layer (3); and an adhesive layer (4) for bonding the glass sheet (2) and the resin layer (3), in which a spectral transmittance of the adhesive layer (4) in at least a wavelength range of from 430 nm to 680 nm is 90% or more.
摘要:
A sheet roll (1) is manufactured by placing a sheet-like coupling member (3) on end portions of a plurality of glass films (g) so as to span therebetween, coupling the end portions of the glass films (g) together, and rolling the coupled plurality of glass films (g). The sheet-like coupling member (3) used in the sheet roll (1) includes wide width portions (4) for forming wide joint portions joined to the glass films (g) at each of both end portions thereof in a rolling direction, and a necked portion (5), which is narrower than the wide width portions (4) and is formed at a middle portion thereof in the rolling direction.
摘要:
A roll-to-roll apparatus reliably reduces breakage of a glass film even in a case of sequentially performing predetermined processing on the glass film. Provided is a glass roll (1) formed by winding a glass film (2) into a roll, in which a resin film (4) is attached onto the glass film (2), and at least a part of the resin film (4) is arranged on a front side of an unwinding direction relative to a leading end portion in the unwinding direction of the glass film (2).