公开(公告)号:EP3307679A4
公开(公告)日:2018-06-20
申请号:EP16807132
申请日:2016-06-09
申请人: SHARP KK
IPC分类号: B01J21/08 , B01J23/34 , B01J23/40 , B01J23/74 , B01J23/75 , B01J35/00 , B01J35/02 , B01J35/10 , B01J37/03 , C01B33/32 , H01M4/58
CPC分类号: H01M4/5825 , B01J21/08 , B01J23/34 , B01J23/40 , B01J23/74 , B01J23/745 , B01J23/75 , B01J23/755 , B01J23/8892 , B01J35/002 , B01J35/023 , B01J35/1066 , B01J35/1076 , B01J37/031 , C01B33/32 , C01P2004/61 , C01P2004/62 , C01P2006/12 , C01P2006/16 , C01P2006/40 , H01M2004/021 , H01M2004/028
摘要: A macroporous sodium transition metal silicate material includes a composition represented by AaM1bM2cXdOe, wherein A is sodium or a mixture of sodium with lithium and/or potassium; M1 is one or more transition metals; M2 is one or more metals and/or metalloids; X is silicon or a mixture containing silicon and one or more elements selected from phosphorus, boron and aluminium; a is >0; b is >0; c is ≧0; d is ≧1; and e is ≧2. A method of forming the macroporous sodium transition metal silicate material includes mixing one or more transition metal precursor materials in a solvent to form a transition metal mixture; adding one or more silicate precursors to the transition metal mixture to form a precursor mixture; raising the pH of the precursor mixture to form a precipitate; stirring the mixture; aging and drying the mixture; washing the mixture; and drying.