摘要:
A metal porous body is a metal porous body mainly composed of nickel and having a framework of a three-dimensional network structure, Ni(OH) 2 being present in a surface of the framework, when the metal porous body is subjected to at least 30 potential scans between a lower limit potential of -0.10 V and an upper limit potential of +0.65 V with respect to a hydrogen standard potential in not less than 10% by mass and not more than 35% by mass of a potassium hydroxide aqueous solution, at least oxygen being detected within a depth of 5 nm from the surface, and hydrogen being detected at least in the surface.
摘要:
A method for producing a nickel alloy porous body includes a step of applying a coating material that contains a nickel alloy powder of nickel and an added metal, the nickel alloy powder having a volume-average particle size of 10 µm or less, onto a surface of a skeleton of a resin formed body having a three-dimensional mesh-like structure; a step of plating with nickel the surface of the skeleton of the resin formed body onto which the coating material has been applied; a step of removing the resin formed body; and a step of diffusing the added metal into the nickel by a heat treatment.
摘要:
Provided is a porous metal body having higher corrosion resistance than existing porous metal bodies composed of nickel-tin binary alloys and existing porous metal bodies composed of nickel-chromium binary alloys. The porous metal body contains at least nickel, tin, and chromium. An example of a method of producing such a porous metal body is a method including a conductive-coating-layer formation step of forming a conductive coating layer containing chromium on a surface of a porous base formed of a resin material; a metal-layer formation step of forming a nickel layer and a tin layer in any order on a surface of the conductive coating layer; a removal step of removing the porous base; and a diffusion step of, by a heat treatment, causing interdiffusion of metal atoms between the nickel layer and the tin layer and diffusing chromium contained in the conductive coating layer into the nickel layer and the tin layer.
摘要:
An object of the present invention is to provide, at a low cost, a porous metal body that can be used in an electrode of a fuel cell and that has better corrosion resistance. The porous metal body has a three-dimensional mesh-like structure and contains nickel (Ni), tin (Sn), and chromium (Cr). A content ratio of the tin is 10% by mass or more and 25% by mass or less, and a content ratio of the chromium is 1% by mass or more and 10% by mass or less. On a cross section of a skeleton of the porous metal body, the porous metal body contains a solid solution phase of chromium, nickel, and tin. The solid solution phase contains a solid solution phase of chromium and trinickel tin (Ni 3 Sn), the solid solution phase having a chromium content ratio of 2% by mass or less, and does not contain a solid solution phase that is other than a solid solution phase of chromium and trinickel tin (Ni 3 Sn) and that has a chromium content ratio of less than 1.5% by mass.
摘要:
Provided is a porous metal body having higher corrosion resistance than existing porous metal bodies composed of nickel-tin binary alloys and existing porous metal bodies composed of nickel-chromium binary alloys. The porous metal body contains at least nickel, tin, and chromium. An example of a method of producing such a porous metal body is a method including a conductive-coating-layer formation step of forming a conductive coating layer containing chromium on a surface of a porous base formed of a resin material; a metal-layer formation step of forming a nickel layer and a tin layer in any order on a surface of the conductive coating layer; a removal step of removing the porous base; and a diffusion step of, by a heat treatment, causing interdiffusion of metal atoms between the nickel layer and the tin layer and diffusing chromium contained in the conductive coating layer into the nickel layer and the tin layer.
摘要:
Provided is a surface-coated metal porous body having a three-dimensional network structure, the surface-coated metal porous body including: a framework forming the three-dimensional network structure; and a coating film provided on a surface of the framework, wherein the framework has a body including a metal element as a constituent element, the coating film includes a scale-like carbon material and a fine-grained conductive material, a distance D between two points that are farthest from each other on an outer perimeter of a main surface of the scale-like carbon material is 5% or more and 120% or less relative to a thickness of the framework, and the scale-like carbon material is deposited on the surface of the framework.
摘要:
A method for producing a nickel alloy porous body includes a step of applying a coating material that contains a nickel alloy powder of nickel and an added metal, the nickel alloy powder having a volume-average particle size of 10 µm or less, onto a surface of a skeleton of a resin formed body having a three-dimensional mesh-like structure; a step of plating with nickel the surface of the skeleton of the resin formed body onto which the coating material has been applied; a step of removing the resin formed body; and a step of diffusing the added metal into the nickel by a heat treatment.
摘要:
An object of the present invention is to provide, at a low cost, a porous metal body that can be used in an electrode of a fuel cell and that has better corrosion resistance. The porous metal body has a three-dimensional mesh-like structure and contains nickel (Ni), tin (Sn), and chromium (Cr). A content ratio of the tin is 10% by mass or more and 25% by mass or less, and a content ratio of the chromium is 1% by mass or more and 10% by mass or less. On a cross section of a skeleton of the porous metal body, the porous metal body contains a solid solution phase of chromium, nickel, and tin. The solid solution phase contains a solid solution phase of chromium and trinickel tin (Ni 3 Sn), the solid solution phase having a chromium content ratio of 2% by mass or less, and does not contain a solid solution phase that is other than a solid solution phase of chromium and trinickel tin (Ni 3 Sn) and that has a chromium content ratio of less than 1.5% by mass.
摘要:
Provided is a porous metal body having superior corrosion resistance to conventional metal porous bodies composed of nickel-tin binary alloys and conventional metal porous bodies composed of nickel-chromium binary alloys. The porous metal body has a three-dimensional network skeleton and contains at least nickel, tin, and chromium. The concentration of chromium contained in the porous metal body is highest at the surface of the skeleton of the porous metal body and decreases toward the inner side of the skeleton. In one embodiment, the chromium concentration at the surface of the skeleton of the porous metal body is more preferably 3% by mass or more and 70% by mass or less.
摘要:
Provided is a porous metal body having superior corrosion resistance to conventional metal porous bodies composed of nickel-tin binary alloys and conventional metal porous bodies composed of nickel-chromium binary alloys. The porous metal body has a three-dimensional network skeleton and contains at least nickel, tin, and chromium. The concentration of chromium contained in the porous metal body is highest at the surface of the skeleton of the porous metal body and decreases toward the inner side of the skeleton. In one embodiment, the chromium concentration at the surface of the skeleton of the porous metal body is more preferably 3% by mass or more and 70% by mass or less.