公开(公告)号:EP2658828A1
公开(公告)日:2013-11-06
申请号:EP11817521.5
申请日:2011-12-31
申请人: University of Tartu
发明人: PART, Marko , TÄTTE, Tanel , MÄEORG, Uno , KIISK, Valter , NURK, Gunnar , VOROBJOV, Aleksei , HANSCHMIDT, Kelli
IPC分类号: C04B35/622 , D01D5/24 , D01F9/10
CPC分类号: C04B35/624 , B82Y30/00 , C04B35/62231 , C04B35/6225 , C04B35/6264 , C04B35/6269 , C04B2235/3217 , C04B2235/3224 , C04B2235/3225 , C04B2235/3229 , C04B2235/3239 , C04B2235/3244 , C04B2235/441 , C04B2235/5284 , C04B2235/6021 , C04B2235/606 , C04B2235/762 , C04B2235/765 , C04B2235/96 , D01D5/24 , D01F9/10 , Y10T428/2975
摘要: The present invention prescribes a new sol-gel method of preparing and formation of the metal oxide microtubes. According to the method firstly is prepared the precursor sol from metal oxides or mixtures of metal oxides and alkoxides, thereafter from the precursor sol are extruded the fibres, which are gelatinised afterwards until the inner sol which is less viscous of fibres is converted to thinner wall until alcohol from the precursor is left trough walls. The metal oxide microtubes are applicable as to conduct liquids or gasses, as ionic conductors, as catalyst carriers and as light emitters.
摘要翻译: 本发明规定了制备和形成金属氧化物微管的新型溶胶 - 凝胶方法。 根据该方法,首先由金属氧化物或金属氧化物和醇盐的混合物制备前体溶胶,然后从前体溶胶中挤出纤维,然后将其糊化,直到纤维粘性较低的内溶胶转变成较薄的壁 直到来自前体的酒离开槽壁。 金属氧化物微管适用于传导液体或气体,作为离子导体,作为催化剂载体和作为光发射体。