摘要:
Compositionally uniform but nonrandom copolymers of ethylene and a,p-ethylenically unsaturated carboxylic acids having from 3 to 8 carbon atoms are provided having an acid content of from about 6 to about 35 weight percent, a melt index of from about 0.1 to about 800, and a ratio of weight percent adjacent acid to weight percent total acid in the copolymer of from about 0.44 to about 1.0. These copolymers have improved physical properties such as hardness, stiffness, heat resistance and creep resistance. Further provided, is a process for preparing these copolymers in a constant environment stirred autoclave in a continuous manner wherein the reaction zone is maintained in a steady state at a pressure of from 0 to about 500 psi above, and at a temperature of from 0 to about 15°C above that needed to maintain a single phase reaction mixture at a given concentration of copolymer and at the given acid comonomer content of the copolymer.
摘要:
The invention relates to a method of processing plastic waste in which the plastic waste in a container is autoclaved as a coherent, porous bundle with a high water absorption capacity in an atmosphere of water vapour at about 150 to 220 °C, preferably 165 to 190 °C, and thus melted, the molten plastic bodies formed at the end of the autoclaving process are at least partly dried by re-evaporating the water contained in them and cooled.
摘要:
L'invention concerne un procédé pour le retraitement de déchets en matière plastique, dans lequel les déchets en matière plastique placés dans des récipients sont autoclavés et, de ce fait, fondus à environ 150 à 220 °C, et de préférence entre 165 et 190 °C, dans une atmosphère de vapeur d'eau, sous forme d'ensembles homogènes et poreux très hygroscopiques, et dans lequel, à la fin de l'autoclavage, les produits obtenus à partir de la matière plastique fondue sont séchés au moins partiellement par revaporisation de l'eau qu'ils contiennent et refroidis.