公开(公告)号:EP3507344B1
公开(公告)日:2024-11-06
申请号:EP17844699.3
申请日:2017-09-01
-
2.
公开(公告)号:EP3728516B1
公开(公告)日:2024-07-03
申请号:EP18892070.6
申请日:2018-12-21
IPC分类号: C10C3/00 , C04B35/83 , C10C3/02 , C10C3/06 , C10C3/08 , D01F9/145 , C01B32/158 , C01B32/182 , C01B32/20 , C01B32/30 , C10B53/04 , C10B57/08 , C10G1/00 , C10G1/02 , C10G1/04 , C10G7/02 , C10G27/12 , D01F9/15 , G01N33/22 , C10G17/02
CPC分类号: C10B53/04 , G01N33/222 , C10B57/08 , C10C3/002 , C10G1/002 , C10G1/02 , C10G1/04 , C10G17/02 , C10G27/12 , C01B32/20 , C01B32/30 , C01B32/182 , C01B32/158 , D01F9/15 , C01P2002/8220130101
-
-
公开(公告)号:EP4370299A1
公开(公告)日:2024-05-22
申请号:EP22747324.6
申请日:2022-07-08
申请人: Soprema
IPC分类号: B29B17/04 , B29B7/48 , B29B7/58 , B29B7/82 , C10C3/00 , E01C19/10 , B29K95/00 , B29L31/10 , B29B7/72
CPC分类号: B29B17/04 , B29B2017/04620130101 , B29K2095/0020130101 , C10C3/007 , B29B7/826 , B29B7/481 , B29B7/72 , B29B7/582 , B29B7/488 , B29L2031/10820130101 , B09B3/00
-
公开(公告)号:EP4314197A1
公开(公告)日:2024-02-07
申请号:EP22719935.3
申请日:2022-04-01
-
-
7.
-
公开(公告)号:EP4284877A1
公开(公告)日:2023-12-06
申请号:EP22705342.8
申请日:2022-01-27
-
公开(公告)号:EP4215597A1
公开(公告)日:2023-07-26
申请号:EP22152942.3
申请日:2022-01-24
发明人: Spahr, Michael , Kuhnt, Christopher , Claes, Joris , Denoo, Bram
摘要: The present invention is directed to a carbon precursor material characterized by a flashpoint above 290°C and a softening point between 110 and 300°C Mettler and comprising petroleum-derived pitch product derived from a petroleum-based raw material having a concentration of less than 40% by weight of asphaltenes as measured by SARA analysis. Further, the present invention is directed to the use of such carbon precursor material in binding/coating/impregnation processes in the production of graphite electrodes for electric arc furnaces used in steel/ferro-alloy/silicon production or in carbon electrodes for aluminum production and/or manufacture of graphite particles for the manufacturing of battery electrodes. The present invention is further directed to a carbon or graphite electrode comprising said pitch binder in converted state, and in particular a battery electrode. The present invention provides also a process for producing a coating and/or binding and/or impregnation carbon precursor material comprising a petroleum-derived pitch product, the process comprising the steps of providing petroleum-based raw material having a concentration of less than 40% by weight of asphaltenes measured by SARA analysis, thermally treating said petroleum-based raw material above 300°C at atmospheric pressure, and subsequently distill the thermally treated material, thereby obtaining a distillation residue being said petroleum-derived pitch product.
-
公开(公告)号:EP4194396A1
公开(公告)日:2023-06-14
申请号:EP21214111.3
申请日:2021-12-13
摘要: The present invention is directed to use of a petroleum-derived pitch product as coating material for graphite particles for the manufacturing of battery electrodes, characterized in that said pitch product has a melt viscosity index log 10 (visc)*100/SPM between 1.2 and 3.0 at 220°C and between 1.0 and 2.5 at 240°C, wherein visc = melt viscosity (mPa.s) and SPM= softening point °C Mettler.
Further, the present invention is directed to a battery electrode comprising a coating made of said pitch product, as well as directed to a battery comprising an electrode having a coating made of said pitch product.
In addition, the present invention is directed to a process for obtaining a petroleum-derived pitch product as mentioned above, said process comprising a petroleum vacuum distillation process step for obtaining petroleum-derived distillation residue. Further, the invention is directed to a process for manufacturing a battery electrode comprising said process for producing a pitch product.
-
-
-
-
-
-
-
-
-