公开(公告)号:JP2014005474A
公开(公告)日:2014-01-16
申请号:JP2013212733
申请日:2013-10-10
IPC分类号: C01G39/06 , C10M159/18 , C07C333/20 , C07F11/00 , C10M125/06 , C10M129/24 , C10M129/26 , C10M133/04 , C10M135/14 , C10M135/18 , C10M135/20 , C10M137/06 , C10M137/10 , C10M139/00 , C10M163/00 , C10M169/04 , C10N10/12 , C10N30/00 , C10N30/06 , C10N30/10 , C10N40/25
CPC分类号: C07C333/20 , C07F11/005 , C10M159/18 , C10M163/00 , C10M169/045 , C10M2227/066 , C10M2227/09 , C10N2210/06 , C10N2230/10 , C10N2230/20 , C10N2230/54 , C10N2240/08 , C10N2240/104 , C10N2240/105 , C10N2240/12 , C10N2250/10
摘要: PROBLEM TO BE SOLVED: To provide an additive which has a satisfactory color appearance, a low chlorine content, and a sulfur-to-molybdenum ratio acceptable to be significantly benign to copper corrosion and seal degradation.SOLUTION: A process for making an additive comprising one or more oil-soluble or oil-dispersible molybdenum-sulfur compounds comprises the steps of: (I) reacting in a polar medium a reactant molybdenum compound (A) and a source of a ligand (B), which is capable of rendering molybdenum-sulfur compounds oil-soluble or oil-dispersible; and (II) reacting a compound (C), which is capable of reacting with labile sulfur, with either (a) the reaction mixture of the step (I) after the reaction of (A) and (B) has begun, or (b) the product of the step (I).
摘要翻译: 要解决的问题:提供一种添加剂,其具有令人满意的颜色外观,低氯含量和硫与钼的比率,其对于铜腐蚀和密封降解是显着良好的。解决方案:一种制备添加剂的方法,包括 一种或多种油溶性或油分散性钼 - 硫化合物包括以下步骤:(I)在极性介质中使反应物钼化合物(A)和配体(B)的源反应,其能够使钼 磺化合物油溶性或油分散性; 和(II)使能够与不稳定硫反应的化合物(C)与(a)在(A)和(B)反应开始后的步骤(I)的反应混合物开始或( b)步骤(I)的产物。
-
公开(公告)号:JP2004051985A
公开(公告)日:2004-02-19
申请号:JP2003192694
申请日:2003-07-07
IPC分类号: C01G39/06 , C07C333/20 , C07F11/00 , C10M125/06 , C10M129/24 , C10M129/26 , C10M133/04 , C10M135/14 , C10M135/18 , C10M135/20 , C10M137/06 , C10M137/10 , C10M139/00 , C10M159/18 , C10M163/00 , C10M169/04 , C10N10/12 , C10N30/00 , C10N30/06 , C10N30/10 , C10N40/25
CPC分类号: C07C333/20 , C07F11/005 , C10M159/18 , C10M163/00 , C10M169/045 , C10M2227/066 , C10M2227/09 , C10N2210/06 , C10N2230/10 , C10N2230/20 , C10N2230/54 , C10N2240/08 , C10N2240/104 , C10N2240/105 , C10N2240/12 , C10N2250/10
摘要: PROBLEM TO BE SOLVED: To provide an additive having a satisfactory color appearance, a little chlorine content, and an acceptable ratio of sulfur to molybdenum so that copper corrosive properties and sealing decomposability are significantly good. SOLUTION: In a producing method of the additive comprising at least one of oil-soluble or oil-dispersible molybdenum-sulfur compounds, the method comprises the steps of: (I) reacting in a polar medium a reactive molybdenum compound (A) with a source of a ligand (B) which can make the molybdenum-sulfur compound oil-soluble or oil-dispersible, and (II) reacting a compound (C) which is capable of reacting a labile sulfur with either (a) a reaction mixture of the step (I) after reaction initiation of (A) and (B), or (b) a resulting product of the step (I). COPYRIGHT: (C)2004,JPO
摘要翻译: 要解决的问题:为了提供具有令人满意的颜色外观,少量氯含量和硫与钼的可接受的比例的添加剂,使得铜的腐蚀性和密封分解性显着良好。 解决方案:在包含油溶性或油分散性钼 - 硫化合物中的至少一种的添加剂的制造方法中,该方法包括以下步骤:(I)在极性介质中使反应性钼化合物(A )与可以使钼 - 硫化合物油溶性或油分散性的配体(B)的来源,和(II)使能够使不稳定硫与(a) (A)和(B)的反应开始后的步骤(I)的反应混合物,或(b)步骤(I)的所得产物。 版权所有(C)2004,JPO
-