MANUFACTURE OF LINEAR AMORPHOUS SOLAR BATTERY

    公开(公告)号:JPS6084887A

    公开(公告)日:1985-05-14

    申请号:JP19321483

    申请日:1983-10-14

    IPC分类号: H01L31/04 H01L31/20

    摘要: PURPOSE:To enable the linear and even formation of the titled device in continuous length by a method wherein an amorphous layer is formed on a wire by passage of the wire through a discharge-decomposed atmosphere of a raw material gas. CONSTITUTION:A center conductor wire 1 serving as the substrate of a solar battery turns into a wire 2 with a solar battery layer after passage through the centers of reaction baths 8, 9, and 10. This wire is supported by guide rollers 12. For silane decomposition, the raw material gas 13 introduced through a gas introduction port 4 is decomposed by means of a coil 3. A coil peripheral member 11 on the wall of the reaction baths should be an insulator so that an electromagnetic field generating in the coil may be transmitted into the baths. For example, quartz glass of the like can be used. The baths are exhausted from vacuum exhaust ports 6 in order to keep the gas pressure therein at a desired pressure, and then the pressure is kept constant by control of the exhaust capacity. In the case of using for example a P-I-N structure as the solar battery structure, a P-layer reaction bath 8, an I-layer one 9, and an N-layer one 10 are provided, and the coil length is varied in proportion to the film-forming time per unit length.

    LINEAR AMORPHOUS SOLAR BATTERY
    6.
    发明专利

    公开(公告)号:JPS6084886A

    公开(公告)日:1985-05-14

    申请号:JP19321383

    申请日:1983-10-14

    摘要: PURPOSE:To enable the titled device to be used in a flexible and knitting structure and to become sensitive to lights from all directions by a method wherein a linear or pipe form is used as a substrate. CONSTITUTION:Either structure of a linear pipe or a hollow pipe is used as the center conductor 1. Its material should have a strength necessary to support the whole and a good electric conductivity; e.g., an Al wire or an SUS wire is used. The amorphous solar battery part 2 has a P-I-N structure or a structure of the repetition thereof or a Schottky structure, and light is converted into electricity in this part. A transparent conductive film 3 is an electrode that leads out the electricity generating in the layer 2 along with the center conductor, and ITO or SnO2 is used for the electrode. Since the transparent conductive film 3 does not have so large an electric conductivity, an electricity lead 5 which leads electricity to the end of the wire is mounted on this conductive film. The material of the lead 5 is needed to be a good conductor, and an Al wire, Au wire, or the like is used.

    COATED OPTICAL FIBER
    8.
    发明专利

    公开(公告)号:JPS5862601A

    公开(公告)日:1983-04-14

    申请号:JP16179981

    申请日:1981-10-09

    摘要: PURPOSE:To obtain an optical fiber having high weathering resistance and reliability, by coating a surface of SiO2 optical fiber with >= one kind selected from TiC, TiN, SiC, Si3N4, Al2O3 and TiO2. CONSTITUTION:A surface of an optical fiber tansmitting UV, visible and IR rays contg. >= one kind selected from GeO2, Be2O3, P2O5, Na2O, CaO, Al2O3 and F, consisting essentially of SiO2, is coated with >= one kind selected from TiC, TiN, SiC, Si3N4, Al2O3 and TiO2. The thickness of a coated layer is 500Angstrom - 30mum (most preferably 0.1-10mum) and as coating methods, a vacuum depositing, ionic plating, sputtering and plasma CVD methods are used preferably.

    COATED PLASTIC OPTICAL FIBER
    9.
    发明专利

    公开(公告)号:JPS5858502A

    公开(公告)日:1983-04-07

    申请号:JP15713181

    申请日:1981-10-01

    IPC分类号: G02B6/44

    摘要: PURPOSE:To provide long-term durability and to prevent degradation in attenuation rate by covering >=1 kind among Al2O3, SiO2, ZrO2, MgO as water repellent oxides on the surface of plastic optical fibers used for optical communication. CONSTITUTION:Al2O3 is coated at 0.5mum by an ion plating method on the surface of, for example, acrylic plastic fibers with 0.2mm.phi as plastic fibers for transmission of UV, visible and IR rays, and further a silicone resin is coated thereon at 0.2mm. to form products. oxides which have no hydrating nature and prevent sticking of moisture are used for the compds. to be coated on the plastic surface. More particularly, oxides consisting of >=1 kind among Al2O3, SiO2, ZrO2, MgO provide indexpensive and stable covering. When the thickness of the covering is set at >=500Angstrom and