친환경 습윤 경화형 유·무기 복합 산업용 바닥재 조성물
    1.
    发明授权
    친환경 습윤 경화형 유·무기 복합 산업용 바닥재 조성물 有权
    有机无机混合和环境友好的地板材料使用湿润混凝土条件

    公开(公告)号:KR100874657B1

    公开(公告)日:2008-12-17

    申请号:KR1020080049326

    申请日:2008-05-27

    发明人: 김대동 채우병

    IPC分类号: C04B28/00 C04B26/16

    摘要: A floor material for an environment wet-hardening typed organic/inorganic complex industrial composition is provided to prevent a safety accident of users when is applied at an underground parking lot using an excellent skid resistance. A floor material for an environment wet-hardening typed organic/inorganic complex industrial composition comprises an urethane prepolymer of 18~22 weight%, a polyol of 7~11 weight%, water of 6~8 weight% and a pulverized body of 65~69 weight%. The pulverized body comprises white cement of 45~46 weight%, silica of 11~12 weight%, calcium hydroxide of 3~4 weight%, calcium carbonate of 3~3.5 weight% and chromium dioxide of 3~3.5 weight%.

    摘要翻译: 提供了一种用于环境湿硬化型有机/无机复合工业组合物的地板材料,以防止在地下停车场使用优异的抗滑性的用户安全事故。 用于环境湿硬化型有机/无机复合工业组合物的地板材料包括18〜22重量%的氨基甲酸酯预聚物,7〜11重量%的多元醇,6〜8重量%的水和65〜 69重量%。 粉体为45〜46重量%的白水泥,11〜12重量%的二氧化硅,3〜4重量%的氢氧化钙,3〜3.5重量%的碳酸钙,3〜3.5重量%的二氧化铬。

    실란커플링제로 표면이 개질된 초마이크로 실리카와 나노입자 뵘석이 포함된 2성분형 바닥 마감재 조성물 및 그 제조방법
    2.
    发明授权
    실란커플링제로 표면이 개질된 초마이크로 실리카와 나노입자 뵘석이 포함된 2성분형 바닥 마감재 조성물 및 그 제조방법 有权
    包含表面改性的超高分子二氧化硅和纳米硼酸盐的混合物料的两种组分型表面处理材料组合物及其制备方法

    公开(公告)号:KR101340585B1

    公开(公告)日:2013-12-11

    申请号:KR1020130105268

    申请日:2013-09-03

    摘要: Disclosed is a two component-type finishing material composition which includes: a main material including 50-70 wt% of an epoxy resin, 1-5 wt% of mineral split, 1-10 wt% of a diluent, 0.01-3 wt% of a defoaming agent, 1-6 wt% of a leveling agent, 0.1-4 wt% of a wetting agent, and 3-22 wt% of microsilica with surface modified by a silane coupling agent; and a curing agent including 40-60 wt% of modified aliphatic amine, 20-30 wt% of modified aromatic amine, 1-8 wt% of promoters, 0.01-3 wt% of a defoaming agent, and 3-20 wt% of bohemite nanoparticles with surface modified by a silane coupling agent. [Reference numerals] (AA) Example: matrix damaged state after wet surface adhesion strength test;(BB) Comparative example: interface dropout state after wet surface adhesion strength test

    摘要翻译: 公开了一种双组分型整理材料组合物,其包括:主要材料,其包含50-70重量%的环氧树脂,1-5重量%的矿物分散体,1-10重量%的稀释剂,0.01-3重量% 的消泡剂,1-6重量%的流平剂,0.1-4重量%的润湿剂和3-22重量%的由硅烷偶联剂表面改性的微硅粉; 和包含40-60重量%改性脂族胺,20-30重量%改性芳族胺,1-8重量%助催化剂,0.01-3重量%消泡剂和3-20重量% 具有表面改性硅烷偶联剂的波希米纳粒子。 (附图标记)(AA)实施例:湿表面粘合强度试验后的基体损伤状态;(BB)比较例:湿表面粘合强度试验后界面脱落状态

    판상의 마이크로 실리카와 실란 커플링제가 첨가된 콘크리트 바닥 표면 마감재
    4.
    发明授权
    판상의 마이크로 실리카와 실란 커플링제가 첨가된 콘크리트 바닥 표면 마감재 有权
    混凝土地板的表面处理材料包括层状微量二氧化硅和硅烷偶联剂

    公开(公告)号:KR101358969B1

    公开(公告)日:2014-02-07

    申请号:KR1020120015674

    申请日:2012-02-16

    摘要: 본 발명은 콘크리트 바닥 표면 마감재에 관한 것으로, 보다 상세하게는, 에폭시수지계 주제와 경화제로 구성된 2액형 조성물로서, 주제에 판상형 마이크로 실리카와 실란 커플링제를 충전제로서 첨가하여 습윤면에서도 부착력이 우수하고, 자기 평활성이 우수하여 작업성이 용이하며, 유.무기 조성물의 가교 결합 밀도 상승으로 표면경도가 높고, 시공 후 소정의 규사를 뿌려줄 경우 규사를 강하게 응집하는 효과에 의한 논슬립 기능을 부여할 수 있는 다목적 표면 마감재에 관한 것이다.
    본 발명에 따른 바닥 표면 마감재는, 에폭시 수지와 실란 커플링제, 판상의 마이크로 실리카를 포함하는 제1제와; 아민계 경화제와 실란 커플링제를 포함하는 제2제를 혼합하여 제조되는 2액형 콘크리트 바닥 표면 마감재이다.

    판상의 마이크로 실리카와 실란 커플링제가 첨가된 콘크리트 바닥 표면 마감재
    5.
    发明公开
    판상의 마이크로 실리카와 실란 커플링제가 첨가된 콘크리트 바닥 표면 마감재 有权
    混凝土地板的表面处理材料,包括LAMELLAR MICRO SILICA和SILANE偶联剂

    公开(公告)号:KR1020130094433A

    公开(公告)日:2013-08-26

    申请号:KR1020120015674

    申请日:2012-02-16

    摘要: PURPOSE: 2 liquid type concrete floor surface finishing material is provided to have an excellent adhesive force in a wetted surface, a self smoothness and a surface hardness by adding a plate shaped micro silica and a silane coupling agent to an epoxy resin-based main material. CONSTITUTION: 2 liquid type concrete floor surface finishing material comprises a first material and a second material. The first material comprises an epoxy resin, a silane coupling agent, and a plate shaped micro silica. The second material comprises an amine-based curing agent and a silane coupling agent. The first material comprises 50-70 weight% of epoxy resin, 5-22 weight% of silane coupling agent, 1-5 weight% of mineral spirit, 1-15 weight% of plate shaped micro silica, 1-10 weight% of diluent, 0.01-3 weight% of mineral antifoaming agent, 1-5 weight% of leveling agent, and 0.1-3 weight% of wetting agent. The second material comprises 40-60 weight% of denaturation aliphatic amine, 20-30 weight% of denaturation aromatic amine, 10-20 weight% of silane coupling agent, 1-8 weight% of accelerant, 0.1-5 weight% of silicon-based antifoaming agent. The first material and the second material are mixed as the weight ratio of 3:1.

    摘要翻译: 目的:提供2种液态混凝土地板表面处理材料,通过向环氧树脂为主体材料添加板状微细二氧化硅和硅烷偶联剂,使其在润湿表面具有优异的粘合力,自平滑度和表面硬度 。 构成:2液态混凝土地板表面处理材料包括第一材料和第二材料。 第一种材料包括环氧树脂,硅烷偶联剂和板状微量二氧化硅。 第二种材料包括胺基固化剂和硅烷偶联剂。 第一种材料包括50-70重量%的环氧树脂,5-22重量%的硅烷偶联剂,1-5重量%的矿物油,1-15重量%的板状微量二氧化硅,1-10重量%的稀释剂 ,0.01-3重量%的矿物消泡剂,1-5重量%的流平剂和0.1-3重量%的润湿剂。 第二种材料包含40-60重量%的变性脂族胺,20-30重量%的变性芳香胺,10-20重量%的硅烷偶联剂,1-8重量%的促进剂,0.1-5重量%的硅 - 基于消泡剂。 第一种材料和第二种材料以3:1的重量比混合。

    무기질계 수지의 제조방법 및 이를 이용한 코팅재 조성물
    6.
    发明授权
    무기질계 수지의 제조방법 및 이를 이용한 코팅재 조성물 有权
    无机基树脂及其组合物的制造方法

    公开(公告)号:KR101405368B1

    公开(公告)日:2014-06-11

    申请号:KR1020130143132

    申请日:2013-11-22

    摘要: The present invention relates to an environmentally friendly inorganic based resin composition having excellent chemical resistance, water resistance, wear resistance, impact resistance, excellent expression of adhesive strength and cleaning ability when a pollution source is coated on a fragment, and which does not include toxic components; and to a manufacturing method of a coating material for concrete inner/outer walls and floors.

    摘要翻译: 本发明涉及一种环境友好的无机基树脂组合物,其具有优异的耐化学性,耐水性,耐磨性,耐冲击性,当将污染源涂覆在片上时具有优异的粘合强度表达和清洁能力,并且不含有毒 组件; 以及用于混凝土内/外墙和地板的涂料的制造方法。

    황토와 백토석 함유 붙임용 모르타르 조성물
    7.
    发明公开
    황토와 백토석 함유 붙임용 모르타르 조성물 无效
    含有黄土的麦芽糖组合物和用于粘结物品的TERRA ALBA

    公开(公告)号:KR1020110048756A

    公开(公告)日:2011-05-12

    申请号:KR1020090105464

    申请日:2009-11-03

    发明人: 이정녕 채우병

    CPC分类号: Y02W30/92

    摘要: PURPOSE: A mortar composition containing yellow soil and terra alba is provided to obtain the adhesive intensity, the crack resistance property, and the water resistance property required for mortar for bonding tiles, walls, or floor materials. CONSTITUTION: A mortar composition containing yellow soil and terra alba includes white cement powder, silica powder, yellow soil powder, terra alba powder, calcium carbonate powder, fly ash powder, ethylene vinyl acetate powder, an expanding agent, a thickening agent, and a plasticizer. The particle size of the calcium carbonate is between 42 and 45um. The thickening agent is the mixture of one or two kinds or more of materials selected from hydroxyethyl cellulose, hydroxypropyl methyl cellulose, and starchether. The expanding agent is the mixture of one or two kinds or more of materials selected from ettringite-based, lime-based, and ettringite-lime composite-based materials. The plasticizer is the mixture of one or two kinds or more of materials selected from polycarboxylate ether-based and ligninsulfonate-based materials.

    摘要翻译: 目的:提供含有黄土和白土的砂浆组合物,以获得粘合砖,墙壁或地板材料的砂浆所需的粘合强度,抗裂性和耐水性。 构成:含有黄土和白土的砂浆组合物包括白色水泥粉末,二氧化硅粉末,黄土粉末,白土粉末,碳酸钙粉末,飞灰粉末,乙烯乙酸乙烯酯粉末,发泡剂,增稠剂和 增塑剂。 碳酸钙的粒径在42和45um之间。 增稠剂是选自羟乙基纤维素,羟丙基甲基纤维素和星形树脂中的一种或两种以上的材料的混合物。 发泡剂是选自钙矾石,石灰和钙矾石 - 石灰复合材料的一种或两种以上的材料的混合物。 增塑剂是选自聚羧酸酯醚基和木质素磺酸盐基材料中的一种或两种以上的材料的混合物。