비소성 시멘트를 이용한 보강옹벽용 식생블록 및 이의 제조방법
    1.
    发明授权
    비소성 시멘트를 이용한 보강옹벽용 식생블록 및 이의 제조방법 有权
    用于使用未固化水泥保留墙的可植物块及其制造方法

    公开(公告)号:KR101241818B1

    公开(公告)日:2013-03-15

    申请号:KR1020120088505

    申请日:2012-08-13

    Abstract: PURPOSE: A vegetation block for a reinforcement wall utilizing non-sintered cement and a manufacturing method are provided to improve permeability, durability and intensity and to grow plants well by excellent water absorption and moistness. CONSTITUTION: A vegetation block(100) for a reinforcement wall utilizing non-sintered cement comprises a front portion(110), a rear portion(120), and a vegetation groove(130). The front portion is formed in order to protrude from the rear portion and includes non-sintered cement, an intensity development material, sand, pigment, and red clay. The rear portion comprises a center portion(121) and a latching projection(126) and includes the non-sintered cement, aggregate, the intensity development material, and vermiculite. The vegetation groove is formed in between the front and rear portions.

    Abstract translation: 目的:提供一种利用非烧结水泥的加固墙的植被块和制造方法,以提高渗透性,耐久性和强度,并通过优异的吸水性和湿度良好地种植植物。 构造:用于使用非烧结粘结剂的加固壁的植被块(100)包括前部(110),后部(120)和植被沟槽(130)。 前部形成为从后部突出并且包括非烧结水泥,强度显影材料,砂,颜料和红粘土。 后部包括中心部分(121)和闭锁突起(126),并且包括非烧结水泥,骨料,强度显影材料和蛭石。 植被沟槽形成在前部和后部之间。

    비소성 시멘트를 이용한 옹벽 블록 및 이의 제조방법
    2.
    发明授权
    비소성 시멘트를 이용한 옹벽 블록 및 이의 제조방법 有权
    使用未固化水泥保留墙壁块及其制造方法

    公开(公告)号:KR101241820B1

    公开(公告)日:2013-03-18

    申请号:KR1020120088503

    申请日:2012-08-13

    Abstract: PURPOSE: A retaining wall block by using non-sintered cement and a method thereof is provided to have improved strength and durability and to prevent collapse due to rain water and river water. CONSTITUTION: A retaining wall(100) block by using non-sintered cement comprises a lower layer(110) and an upper layer(120) which is formed on an upper part of the lower layer. The lower layer is formed by mixing non-sintered cement, aggregate, and a strength enhancer. The upper layer is formed by mixing non-sintered cement, sand, pigment, red clay, petro-form extract, aggregate, and a strength enhancer.

    Abstract translation: 目的:提供使用非烧结水泥的挡土墙块及其方法,以提高强度和耐久性,并防止由于雨水和河水而引起的塌陷。 构成:通过使用非烧结胶泥的挡土墙块(100)包括下层(110)和形成在下层的上部上的上层(120)。 下层通过混合非烧结水泥,骨料和强度增强剂而形成。 上层通过混合非烧结水泥,砂,颜料,红粘土,石油化合物提取物,骨料和强度增强剂而形成。

    지반보강용 고화재
    4.
    发明授权
    지반보강용 고화재 有权
    固化剂加强条件

    公开(公告)号:KR101168151B1

    公开(公告)日:2012-08-10

    申请号:KR1020110082853

    申请日:2011-08-19

    Abstract: PURPOSE: A solidifying material for reinforcing ground is provided to remove pore water in soil by using exothermic reaction and a volume expansion reaction of calcium oxide in a blowing agent, thereby stabilizing ground in quick time. CONSTITUTION: A solidifying material for reinforcing ground comprises 40-50 parts by weight of a desulfurized gypsum in petroleum coke and 40-100 parts by weight of a blowing agent on the basis of a blast furnace slag. The blowing agent is a flyash of which content of calcium oxide(CaO) is 20-70%. The blowing agent additionally comprises a mixture of one or more selected from a group consisting of electric slag dust, quicklime, and dolomite.

    Abstract translation: 目的:通过放热反应和氧化钙在发泡剂中的体积膨胀反应,提供了一种用于增强地面的固化材料,以去除土壤中的孔隙水,从而在快速时间内稳定地面。 构成:用于增强地面的固化材料包括40-50重量份的石油焦炭中的脱硫石膏和40-100重量份的基于高炉矿渣的发泡剂。 发泡剂是氧化钙(CaO)的含量为20〜70%的粉煤灰。 发泡剂还包含选自电渣渣,生石灰和白云石中的一种或多种的混合物。

    순환자원을 활용한 친환경 공유수면 매립토 조성물
    5.
    发明授权
    순환자원을 활용한 친환경 공유수면 매립토 조성물 有权
    环磷酸钙水解反应使用高容量工业废水的环境安全管理材料

    公开(公告)号:KR101525034B1

    公开(公告)日:2015-06-09

    申请号:KR1020130070332

    申请日:2013-06-19

    CPC classification number: Y02W30/91 Y02W30/92 Y02W30/94

    Abstract: 본발명은공유수면매립토조성물에관한것으로서, 보다상세하게는토사류에인산석고를혼합하여공유수면매립토를제조함에있어혼합토의고결강도증진, 중화처리및 유해물질용출방지를위해고로슬래그미분말및 페트로코크스탈황석고를포함하여일반성토및 복토재료기준이상의우수한성능을발휘하면서환경적으로안정한매립토조성물에관한것이다. 본발명에의한토사류에인산석고를혼합한혼합토 100중량부에대하여, 고로슬래그미분말 1~10중량부와, 페트로코크스탈황석고 1~20중량부를포함한다.

    비소성 무기결합재를 활용한 바닥용 모르타르 조성물
    6.
    发明公开
    비소성 무기결합재를 활용한 바닥용 모르타르 조성물 有权
    使用非烧结无机粘合剂的地板的MORTAR化合物

    公开(公告)号:KR1020140053620A

    公开(公告)日:2014-05-08

    申请号:KR1020120119770

    申请日:2012-10-26

    CPC classification number: Y02W30/91 Y02W30/94 C04B14/04 C04B18/141 C04B22/148

    Abstract: The present invention relates to a mortar compound for the floor of a building, wherein the compound is coated on the floor of an apartment house, an office building, or a parking lot, and more specifically, to a mortar compound for the floor of a building which uses a non-sintered inorganic binder comprising recycled materials substituted for cement. The mortar compound for a floor according to present invention includes 15-100 wt% of a non-sintered inorganic binder relative to 100 wt% of sand or silica.

    Abstract translation: 本发明涉及一种用于建筑物地板的砂浆化合物,其中所述化合物涂覆在公寓,办公楼或停车场的地板上,更具体地,涉及一种用于地板的砂浆化合物 该建筑物使用非烧结的无机粘合剂,其包括替代水泥的再循环材料。 根据本发明的用于地板的砂浆化合物包括相对于100重量%的砂或二氧化硅的15-100重量%的非烧结无机粘合剂。

    비소성 시멘트를 이용한 식생 블록 및 이의 제조방법
    7.
    发明授权
    비소성 시멘트를 이용한 식생 블록 및 이의 제조방법 有权
    使用未烧结水泥的可浇筑块及其制造方法

    公开(公告)号:KR101205497B1

    公开(公告)日:2012-11-27

    申请号:KR1020120088504

    申请日:2012-08-13

    CPC classification number: Y02W30/91

    Abstract: PURPOSE: A vegetation block using non-sintered cement, and a producing method thereof are provided to offer a heat island phenomenon control effect by having high porosity and water-permeability. CONSTITUTION: A vegetation block(100) using non-sintered cement includes a lower layer(110) and an upper layer(120). The lower layer includes more than one through-hole(130), the non-sintered cement, aggregate, a strength improving agent, and vermiculite. The upper layer is molded into the same shape with the lower layer, and contains the non-sintered cement, the strength improving agent, sand, a pigment, yellow soil, and a PET furnace foam extract. 0.5-10 parts of strength improving agent by weight is mixed with 100 parts of non-sintered cement by weight.

    Abstract translation: 目的:提供一种使用非烧结水泥的植被块及其制造方法,通过具有高孔隙率和透水性提供热岛现象控制效果。 构成:使用非烧结水泥的植被块(100)包括下层(110)和上层(120)。 下层包括多个通孔(130),非烧结水泥,骨料,强度改进剂和蛭石。 上层与下层成型为相同的形状,并含有非烧结水泥,强度改进剂,砂,颜料,黄土和PET炉泡沫提取物。 将0.5-10重量份的强度提高剂与100重量份的非烧结水泥混合。

    흙 고화재
    8.
    发明授权
    흙 고화재 有权
    土壤固化剂

    公开(公告)号:KR101200282B1

    公开(公告)日:2012-11-12

    申请号:KR1020100108844

    申请日:2010-11-03

    Abstract: 본 발명은 흙 고화재에 관한 것으로서, 보다 상세하게는 소각잔재에 다량 함유된 CaO의 발열반응과 체적팽창작용을 이용하여 토양의 간극수를 제거하고 함수율을 저감하여 토양을 조속히 안정시키는 흙 고화재에 관한 것이다.
    본 발명에 의한 흙 고화재는 산화칼슘(CaO) 함량이 35%~70%인 소각잔재 100중량부에 대하여, 폴리실리콘제조공정 부산물인 SAS(Sodium Aluminium Sulfate) 또는 SAF(Sodium Aluminium Fluoride) 10~500중량부를 포함한다.

    6가 크롬이 용출되지 않는 심층혼합처리 공법
    9.
    发明授权
    6가 크롬이 용출되지 않는 심층혼합처리 공법 有权
    没有六价铬溶液的深层水泥混合方法

    公开(公告)号:KR101592199B1

    公开(公告)日:2016-02-11

    申请号:KR1020140127724

    申请日:2014-09-24

    Inventor: 문경주 윤성진

    CPC classification number: E02D3/12 C09K17/06

    Abstract: 본발명은심층혼합처리공법에관한것으로서, 보다상세하게는슬래그와탈황공정부산물이포함된슬러리를이용하여 1종보통시멘트와동등이상성능을발현할수 있을뿐만아니라, 체적팽창작용을이용하여벤토나이트사용을배제할수 있고 6가크롬등 유해성분용출을최소화할수 있는심층혼합처리공법에관한것이다. 본발명에의한심층혼합처리공법은 1) 굴착장비를설계심도까지지중에관입하는단계; 2) 상기굴착장비를다시인발하는단계; 3) 상기 1)단계또는 2)단계중 적어도어느하나의단계에서슬래그와탈황공정부산물을포함하는슬러리를주입하여굴착된지반의토양과혼합하는믹싱단계; 및 4) 상기슬러리를경화시켜양생하는단계;를포함한다.

    Abstract translation: 本发明涉及深混合施工方法,更具体地说,涉及一种能够最小化六价铬等有害成分的洗脱的深混合混凝土方法,通过使用体积膨胀作用抑制膨润土的使用,并进行相同的性能 或超过一级普通水泥,通过使用含有渣的浆料和脱硫工艺的副产物。 根据本发明,深混合施工方法包括:1)将挖掘装置嵌入到设计深度的步骤; 2)再次拔出挖掘装置的步骤; 3)通过注入浆料将含有炉渣的浆料和脱硫工艺的副产物与开采的地面上的土壤混合; 4)硬化和固化浆料的步骤。

    비소성 무기결합제를 활용한 친환경블록 및 그 제조방법
    10.
    发明授权
    비소성 무기결합제를 활용한 친환경블록 및 그 제조방법 有权
    使用非烧结无机粘合剂的自然方块及其制造方法

    公开(公告)号:KR101416005B1

    公开(公告)日:2014-07-08

    申请号:KR1020120057898

    申请日:2012-05-31

    CPC classification number: Y02W30/91

    Abstract: 본 발명은 친환경고화재를 활용한 황토벽돌 및 그 제조방법에 관한 것으로서, 보다 상세하게는 보행자를 위한 보도, 산책로, 경관포장용 등으로 사용될 수 있고, 포틀랜트 시맨트를 전혀 사용하지 않는 친환경 고화재를 활용한 황토벽돌 및 그 제조방법에 관한 것이다.
    본 발명에 의한 친환경 황토벽돌은 황토분말 100중량부에 대하여, 입자크기가 5mm 이하인 마사 60~100중량부 및 고화재 50~80중량부를 포함하며, 상기 고화재는, 산화칼슘(CaO) 함량이 20%~60%인 로내탈황방식 석탄연소 소각로에서 발생하는 고칼슘 소각잔재 100중량부에 대하여, 고로슬래그미분말 150~250중량부 및 페트롤코우크스 탈황석고 20~40중량부를 포함한다.