公开(公告)号:US3968786A
公开(公告)日:1976-07-13
申请号:US470254
申请日:1974-05-15
申请人: David H. Spielberg
发明人: David H. Spielberg
CPC分类号: F24J2/48 , F24J2/1047 , F24J2/14 , F24J2/487 , F24J2002/1042 , Y02E10/45 , Y10S126/908 , Y10S165/905
摘要: An improved form of solar heat absorbing tubing comprises a plastic material which contains small subdivided black body absorber particles being fully distributed throughout the thickness of the tubing. A preferred form of tubing will utilize electrical conductive carbon, or carbonized particles, in an amount to provide conductivity to the resulting tubing such that there may be electroplating or electrostatic spray coating for the tubing to still further enhance its absorptive and reradiation properties.
摘要翻译: 一种改进形式的太阳能吸热管包括塑料材料,其包含完全分布在管道整个厚度上的小细分黑体吸收体颗粒。 管道的优选形式将利用导电碳或碳化颗粒,其量为所得管材提供导电性,使得可以使用用于管道的电镀或静电喷涂来进一步增强其吸收和再辐射性能。
-
公开(公告)号:US4018943A
公开(公告)日:1977-04-19
申请号:US226035
申请日:1972-02-14
CPC分类号: H05B3/141 , C04B41/5001 , H01B1/00 , H01C17/20 , H01M4/86
摘要: A method of making conductive material for a conducting device. The material is formed by reacting an organic pyrolyzable substance in the presence of a refractory oxide having a surface area of from about 1 to about 500 square meters per gram in a non-oxidizing atmosphere at a temperature of at least 400.degree. C.
摘要翻译: 制造用于导电装置的导电材料的方法。 该材料是通过在至少400℃的温度下在非氧化性气氛中,在表面积为约1至约500平方米/克的难熔氧化物存在下使有机热解物质反应而形成的。
-
公开(公告)号:US3973234A
公开(公告)日:1976-08-03
申请号:US513026
申请日:1974-10-08
IPC分类号: H01C1/012
CPC分类号: H01C1/012
摘要: Improved forms of electric resistance elements or resistors may be made from semiconducting organic-refractory oxide fibers, as for example drawn alumina fibers which have been subjected to contact with a pyrolyzable organic substance at a temperature above about 400.degree. C. A few, or a large number of the semiconductive fibers, can be used in a group or bundle form to provide a desired resistance for a particular resistor. A preferred form of resistance element will cover the fibers in a quartz tube or other suitable encapsulating material to preclude moisture problems.
摘要翻译: 电阻元件或电阻器的改进形式可以由半导体有机难熔氧化物纤维制成,例如在高于约400℃的温度下与可热解的有机物质接触的拉伸氧化铝纤维。几个或 大量的半导体纤维可以以组或束形式使用,以为特定电阻器提供期望的电阻。 电阻元件的优选形式将覆盖石英管或其它合适的封装材料中的纤维以排除湿气问题。
-
-