Heat-sensitive recording material
    2.
    发明授权
    Heat-sensitive recording material 失效
    热敏记录材料

    公开(公告)号:US5447899A

    公开(公告)日:1995-09-05

    申请号:US249807

    申请日:1994-05-26

    IPC分类号: B41M5/41 B41M5/40

    CPC分类号: B41M5/41

    摘要: A heat-sensitive recording material is prepared by forming a heat-sensitive recording layer on a synthetic paper having a laminated structure. The synthetic paper has a front surface having a smoothness (in accordance with JIS P-8119) of not less than 2000 seconds on which the heat-sensitive recording layer is provided, and a back surface having a smoothness of not more than 1000 seconds, and has an opacity (in accordance with JIS P-8138) of not higher than 40%. The heat-sensitive recording material is superior in recording runnability and recording quality, and gives recorded materials useful as a second original for diazo print.

    摘要翻译: 通过在具有层叠结构的合成纸上形成热敏记录层来制备热敏记录材料。 合成纸具有平滑度(按照JIS P-8119)设置有热敏记录层的不少于2000秒的平滑度的前表面和平滑度不超过1000秒的背面, 并且具有不高于40%的不透明度(按照JIS P-8138)。 热敏记录材料的记录运行性和记录质量优异,并且记录材料可用作重氮印刷的第二原件。

    Method for preparing a heat-sensitive recording material
    3.
    发明授权
    Method for preparing a heat-sensitive recording material 失效
    制备热敏记录材料的方法

    公开(公告)号:US5393560A

    公开(公告)日:1995-02-28

    申请号:US98238

    申请日:1993-07-29

    摘要: A heat-sensitive recording material having a uniform protective layer on a heat-sensitive recording layer formed on a base sheet which is a plastic film or synthetic paper can be obtained without generating a bar-line, streak or scratch. The protective layer is formed on the heat-sensitive recording layer after adjusting Bekk smoothness (measured by TAPPI standard T479 om-81) of the heat-sensitive recording layer to 500.about.6,000 seconds, preferably 1,500.about.4,500 seconds.

    摘要翻译: 可以获得在形成在作为塑料膜或合成纸的基片上的热敏记录层上具有均匀保护层的热敏记录材料,而不产生条纹,条纹或划痕。 在将热敏记录层的Bekk平滑度(通过TAPPI标准T479 om-81测量)调节到6000秒之间,优选1500差别4,500秒后,在热敏记录层上形成保护层。

    Process for producing powder of microcapsules
    4.
    发明授权
    Process for producing powder of microcapsules 失效
    微胶囊粉末生产工艺

    公开(公告)号:US4601863A

    公开(公告)日:1986-07-22

    申请号:US695646

    申请日:1985-01-28

    IPC分类号: B01J13/20 B41M5/165 B01J13/02

    CPC分类号: B01J13/20 B41M5/165

    摘要: A process for producing a powder of microcapsules characterized by adding an aldehyde resin precondensate to a microcapsule dispersion prepared in water or a hydrophilic medium with use of a water-soluble high molecular compound as an emulsifier, maintaining the resulting mixture in a condition for promoting polycondensation of the precondensate, and removing the dispersing medium from the reaction mixture, and a process for producing a powder of microcapsules characterized by emulsifying a hydrophobic core material containing a specific oil-soluble melamine-formaldehyde resin precondensate in water or a hydrophilic medium, subjecting the emulsion to a condition for promoting polycondensation to form capsule wall films and obtain a microcapsule dispersion, and thereafter removing the dispersing medium from the dispersion are disclosed.Further, processes for producing a non-aqueous microcapsule composition are also disclosed.

    摘要翻译: 一种微胶囊粉末的制造方法,其特征在于,使用水溶性高分子化合物作为乳化剂,在水或亲水性介质中制备的微胶囊分散液中加入醛树脂预缩合物,将所得混合物保持在促进缩聚的条件下 的预缩合物,并且从反应混合物中除去分散介质,以及一种制备微胶囊粉末的方法,其特征在于在水或亲水介质中乳化含有特定油溶性三聚氰胺 - 甲醛树脂预缩合物的疏水性芯材料, 乳液到促进缩聚以形成胶囊壁膜并获得微胶囊分散体的条件,然后从分散体中除去分散介质。 此外,还公开了制备非水性微胶囊组合物的方法。

    Method of preparing microcapsules
    5.
    发明授权
    Method of preparing microcapsules 失效
    微胶囊制备方法

    公开(公告)号:US4525520A

    公开(公告)日:1985-06-25

    申请号:US592553

    申请日:1984-03-23

    IPC分类号: B01J13/18 C08L61/28

    摘要: In a microencapsulation process which causes hydrophobic core material containing an oil-soluble melamine-formaldehyde precondensate to emulsified in water or in a hydrophilic medium, and to form capsule wall film under conditions for promoting polycondensation, the process which is characterized in that said oil-soluble melamine-formaldehyde precondensate is 40 to 100% in a degree of formaldehyde substitution, 80 to 100% in alkylation degree, and 4 to 11 in hydrophobic degree.

    摘要翻译: 在将包含油溶性三聚氰胺 - 甲醛预缩合物的疏水性芯材料在水或亲水性介质中乳化的微胶囊化方法中,在促进缩聚的条件下形成胶囊壁膜的方法,其特征在于, 可溶性三聚氰胺 - 甲醛预缩合物的甲醛取代度为40〜100%,烷基化度为80〜100%,疏水性为4〜11。

    Recording materials
    6.
    发明授权
    Recording materials 失效
    录音材料

    公开(公告)号:US4602264A

    公开(公告)日:1986-07-22

    申请号:US522315

    申请日:1983-08-11

    摘要: In a recording material producing images due to a complex formed from an organic phosphorus-iron compound having a bond of PO.sup.- and/or PS.sup.- with Fe.sup.3+ in the molecule and a ligand compound which reacts with the organic phosphorus-iron compound, the present recording material is characterized in that (a) a colorless or light-colored oil-soluble and/or heat-fusible organic compound adheres to the surface of the organic phosphorus-iron compound and/or (b) an organic base is present out of contact with the organic phosphorus-iron compound. The present invention also provides a desensitizer comprising at least one compound selected from the group consisting of (a) organic phosphorus compounds having a bond of P--OH and/or P--SH, (b) organic compounds having an aminocarboxyl group and (c) salts of these compounds (a) and (b).

    摘要翻译: 在由分子中具有PO - 和/或PS-键与Fe 3+的有机磷 - 铁化合物形成的复合物和与有机磷 - 铁化合物反应的配体化合物产生图像的记录材料中,本发明 记录材料的特征在于(a)无色或浅色的油溶性和/或热熔性有机化合物粘附到有机磷 - 铁化合物的表面和/或(b)有机碱存在于 与有机磷铁化合物接触。 本发明还提供一种脱敏剂,其包含至少一种选自(a)具有P-OH和/或P-SH键的有机磷化合物的化合物,(b)具有氨基羧基的有机化合物和(c )这些化合物(a)和(b)的盐。