摘要: A compressible and highly flexible plugging agent comprises the following components in parts by weight: 70-80 parts of natural rubber, 0.5-1 part of polyacrylamide (PAM), 1.5-3 parts of polyanionic cellulose (PAC), 0.5-1 part of biopolymer XC and 10-15 parts of ultrafine calcium carbonate; and the preparation method thereof comprises the following steps: adding the components in the weight parts into the natural rubber in order according to the common preparing method at normal temperature and pressure, mixing and stirring evenly, drying and then grinding into particles of 0.05-50 mm. The plugging agent is characterized by wide raw material sources, simple process, safe application, high plugging ratio and high compressibility, which is suitable for oil recovering and geological drilling applications.
摘要翻译: 可压缩和高度柔性的堵塞剂包括以下重量份的组分:70-80份天然橡胶,0.5-1份聚丙烯酰胺(PAM),1.5-3份聚阴离子纤维素(PAC),0.5-1份 生物聚合物XC和10-15份超细碳酸钙; 其制备方法包括以下步骤:按常规制备方法在常温常压下将重量份中的组分加入天然橡胶中,均匀混合搅拌,干燥后再研磨成0.05〜 mm。 封堵剂的特点是原料来源广泛,工艺简单,应用安全,堵塞比高,压缩率高,适用于采油和地质钻井应用。
-
公开(公告)号:US08598252B2
公开(公告)日:2013-12-03
申请号:US13129576
申请日:2010-04-26
申请人: Yuehua Sui , Fang Guan , Aizhao Zhou , Xiaoping Zhao , Shuai Zhang , Genyu Cui , Yuanqiang Cui , Yongquan Sui , Shuwei Wang , Lei Ge , Zhanfu Chi , Chunyu Wang , Zhijie Liu
发明人: Yuehua Sui , Fang Guan , Aizhao Zhou , Xiaoping Zhao , Shuai Zhang , Genyu Cui , Yuanqiang Cui , Yongquan Sui , Shuwei Wang , Lei Ge , Zhanfu Chi , Chunyu Wang , Zhijie Liu
IPC分类号: C09K8/00 , B22F1/00 , C08K3/10 , C08K3/22 , C08L89/00 , C08L39/00 , C08L67/00 , C08L73/00 , C08L77/00 , C04B26/04 , C08F8/30
CPC分类号: C09K8/426 , C04B26/045 , C09K8/44 , C04B14/28 , C04B24/2652 , C04B24/38 , C04B24/383
摘要: A compressible and highly flexible plugging agent comprises the following components in parts by weight: 70-80 parts of natural rubber, 0.5-1 part of polyacrylamide (PAM), 1.5-3 parts of polyanionic cellulose (PAC), 0.5-1 part of biopolymer XC and 10-15 parts of ultrafine calcium carbonate; and the preparation method thereof comprises the following steps: adding the components in the weight parts into the natural rubber in order according to the common preparing method at normal temperature and pressure, mixing and stirring evenly, drying and then grinding into particles of 0.05-50 mm. The plugging agent is characterized by wide raw material sources, simple process, safe application, high plugging ratio and high compressibility, which is suitable for oil recovering and geological drilling applications.
摘要翻译: 可压缩和高度柔性的堵塞剂包括以下重量份的组分:70-80份天然橡胶,0.5-1份聚丙烯酰胺(PAM),1.5-3份聚阴离子纤维素(PAC),0.5-1份 生物聚合物XC和10-15份超细碳酸钙; 其制备方法包括以下步骤:按常规制备方法在常温常压下将重量份中的组分加入天然橡胶中,均匀混合搅拌,干燥后再研磨成0.05〜 mm。 封堵剂的特点是原料来源广泛,工艺简单,应用安全,堵塞比高,压缩率高,适用于采油和地质钻井应用。
-