PROPYLENE ETHYLENE RANDOM COPOLYMER
    1.
    发明申请

    公开(公告)号:US20200216587A1

    公开(公告)日:2020-07-09

    申请号:US16647672

    申请日:2018-08-30

    Abstract: A propylene ethylene copolymer having: i) xylene soluble fraction at 25° C. ranging from 14 wt % to 27 wt %; ii) intrinsic viscosity of the fraction soluble in xylene at 25° C. ranging from 1.0 to 2.4 dl/g; iii) melt flow rate, MFR, ranging from 1.0 g/10 min to 50.0 g/10 min; iv) an ethylene derived units content ranging from 5.0 wt % to 12.0 wt %; v) the ethylene derived units content on the fraction insoluble in xylene at 25° C. ranging from 2.5 wt % to 6.0 wt %; vi) the ethylene derived units content on the fraction soluble in xylene at 25° C. ranging from 15.2. wt % to 30.2 wt %; and vii) C13 NMR sequences PEP measured on the fraction insoluble in xylene at 25° C. ranging from 3.5 mol % to 5.5 mol % and C13 NMR sequences PEP measured on the fraction soluble in xylene at 25° C. ranging from 11.0 mol % to 14.2 mol %.

    PROPYLENE POLYMER COMPOSITIONS
    2.
    发明申请

    公开(公告)号:US20190338065A1

    公开(公告)日:2019-11-07

    申请号:US16093491

    申请日:2017-03-17

    Abstract: The present disclosure provides a propylene composition made from or containing A) from 60 wt % to 75 wt %, of a propylene homopolymer having a Polydispersity Index (P.I.) value from 4.3 to 4.9, a fraction insoluble in xylene at 25° C., higher than 95%, based upon the weight of the propylene homopolymer, and MFR (Melt Flow Rate according to ISO 1133, condition L, at 230° C. and 2.16 kg load) ranging from 20 to 75 g/10 min; B) from 25 wt % to 40 wt %, of a copolymer of propylene with from 46.0 wt % to 49.0 wt %; of ethylene derived units, based upon the weight of the propylene copolymer; wherein the propylene polymer composition having an intrinsic viscosity of the fraction soluble in xylene at 25° C. between 2.2 to 2.9 dl/g; and the relation: 10.7+1.3×MFRa−17.7×P.I.−29.3×IV+4.9×Xs  (I) between about 40 to about 66; wherein MFRa is the melt flow rate of the component A); P.I. is the polydispersity index of component A); IV is the intrinsic viscosity of the fraction soluble in xylene at 25° C.; and Xs is the fraction soluble in xylene at 25° C.; and wherein the amount of A+B is equal to 100 wt %.

    PROCESS FOR GAS-PHASE POLYMERIZATION OF OLEFINS

    公开(公告)号:US20200216588A1

    公开(公告)日:2020-07-09

    申请号:US16649044

    申请日:2018-09-13

    Abstract: A process for the polymerization of olefins in gas phase carried out in a reactor having two interconnected polymerization zones, a first zone (riser) and a second zone (downcomer), wherein growing polymer particles: a) flow through the riser under fast fluidization conditions established by feeding a mixture of gas and liquid; b) leave the riser and enter the downcomer, through which the growing polymer particles flow downward in a densified form; and c) leave the downcomer and are reintroduced into the riser, thereby establishing a circulation of polymer between the riser and the downcomer; the reactor is operated at a temperature between 0° C. and 5° C. above the dew point of the riser gas at the operating pressure, and in the riser, besides the growing polymer particles and gas flow, an amount of liquid is present.

    PROPYLENE POLYMER COMPOSITION
    4.
    发明公开

    公开(公告)号:US20230151196A1

    公开(公告)日:2023-05-18

    申请号:US17911938

    申请日:2021-03-08

    Inventor: DAVIDE TARTARI

    CPC classification number: C08L23/12 C08L2205/025 C08L2203/30

    Abstract: A polypropylene composition made from or containing:

    A) From 96 wt % to 80 wt %; of a propylene homopolymer having a fraction insoluble in xylene at 25° C. greater than 90 wt %, based upon the total weight of the propylene homopolymer; and a melt flow rate, MFR, measured according to ISO 1133 at 230° C. with a load of 2.16 kg between 80.0 g/10 min and 300.0 g/10 min; and
    B) From 4 wt % to 20 wt %; of a propylene ethylene copolymer having an ethylene derived units content ranging from 18 wt % to 38 wt %, based upon the total weight of the propylene ethylene copolymer;
    wherein the polypropylene composition having:
    a melt flow rate, MFR, measured according to ISO 1133 at 230° C. with a load of 2.16 kg, between 80.0 g/10 min and 150.0 g/10 min;
    the sum of the amounts of A) and B) being 100 wt %.

    PROCESS FOR GAS-PHASE POLYMERIZATION OF OLEFINS

    公开(公告)号:US20200031957A1

    公开(公告)日:2020-01-30

    申请号:US16498303

    申请日:2018-03-07

    Abstract: Process for the preparation of heterophasic propylene copolymer compositions (RAHECO) made from or containing a random propylene copolymer (RACO) and an elastomeric propylene copolymer (BIPO), the process being carried out in a reactor having two interconnected polymerization zones, a riser and a downcomer, wherein growing polymer particles: (a) flow through the first polymerization zone, the riser, under fast fluidization conditions in the presence of propylene and of ethylene or an alpha-olefin having from 4 to 10 carbon atoms, thereby obtaining the random propylene copolymer (RACO); (b) leave the riser and enter the second polymerization zone, the downcomer, through which the growing polymer particles flow downward in a densified form in the presence of propylene and of ethylene or an alpha-olefin having from 4 to 10 carbon atoms, wherein the concentration of ethylene or of the alpha-olefin in the downcomer is higher than in the riser, thereby obtaining the elastomeric propylene copolymer (BIPO); and (c) leave the downcomer and are reintroduced into the riser, thereby establishing a circulation of polymer between the riser and the downcomer.

    FIBER COMPRISING PROPYLENE ETHYLENE RANDOM COPOLYMER

    公开(公告)号:US20220228298A1

    公开(公告)日:2022-07-21

    申请号:US17617325

    申请日:2020-05-26

    Abstract: A fiber of a propylene ethylene copolymer having: i) xylene soluble fraction at 25° C. ranging from 14 wt % to 27 wt %; ii) intrinsic viscosity of the fraction soluble in xylene at 25° C. ranging from 1.0 to 2.4 dl/g; iii) melt flow rate, MFR, ranging from 12 g/10 min to 60 g/10 min; iv) an ethylene derived units content ranging from 5.0 wt % to 12.0 wt %; v) the ethylene derived units content of the fraction insoluble in xylene at 25° C. ranging from 2.5 wt % to 6.0 wt %; vi) the ethylene derived units content of the fraction soluble in xylene at 25° C. ranging from 15.2. wt % to 30.2 wt % vii) C13 NMR sequences PEP measured on the fraction insoluble in xylene at 25° C. ranging from 3.5 mol % to 5.5 mol %; and viii) the C13 NMR sequences PEP measured on the fraction soluble in xylene at 25° C. ranging from 11.0 mol % to 14.2 mol %.

    PROPYLENE TERPOLYMER
    7.
    发明申请

    公开(公告)号:US20220033596A1

    公开(公告)日:2022-02-03

    申请号:US17275939

    申请日:2019-09-04

    Abstract: A terpolymer compositions made from or containing: A) From 80 wt % to 97 wt %; of a first propylene, ethylene, 1-butene terpolymer having: i) the content of ethylene derived units ranging from 0.5 wt % to 3.2 wt %; ii) the content of 1-butene derived units ranging from 7.2 wt % to 14.8 wt %; and B) From 20 wt % to 3 wt %; of a second propylene, ethylene, 1-butene terpolymer having: i) the content of ethylene derived units ranging from 0.5 wt % to 3.2 wt %; ii) the content of 1-butene derived units ranging from 14.4 wt % to 26.5 wt %; and the terpolymer composition having the melt flow rate, MFR, measured according to ISO 1133 at 230° C. with a load of 2.16 kg, ranging from 3.0 g/10 min to 20.0 g/10 min; the sum of the amounts of A) and B) being 100 wt %.

    PROPYLENE ETHYLENE RANDOM COPOLYMER
    8.
    发明申请

    公开(公告)号:US20200032041A1

    公开(公告)日:2020-01-30

    申请号:US16495289

    申请日:2018-03-23

    Abstract: A propylene ethylene copolymer having: (i) an ethylene derived units content (C2) ranging from 2.0 wt % to 11.0 wt %, based upon the total weight of the copolymer; (ii)) a fraction soluble in xylene (Xs) at 25° C. (Xs) ranging from 7.1 wt % to 28.5 wt %, based upon the total weight of the copolymer; (iii) an intrinsic viscosity of the fraction soluble in xylene at 25° C. ranging from 3.2 dl/g to 5.6 dl/g; (iv) a melting point (Tm) higher than 140.0° C. and fulfilling the relation (I): Tm>155−1.4×C2   (I); and (v) a flexural modulus (TM) higher than 500 MPa and fulfilling the relation (II) TM>1900−285×C2+50×Xs   (II).