Abstract:
A solid catalyst component for the polymerization of olefins CH2═CHR in which R is hydrogen or a hydrocarbon radical with 1-12 carbon atoms, made from or containing Mg, Ti, Bi, halogen and an electron donor obtained from a process including the steps: (a) dissolving a Mg(OR)2 compound wherein R groups, equal to or different from each other, are C1-C15 hydrocarbon groups optionally containing a heteroatom selected from O, N and halogen, in an organic liquid medium, thereby forming a first liquid mixture; (b) contacting the first liquid mixture (a) with TiCl4, thereby forming a second liquid mixture absent a solid phase, and (c) subjecting the second liquid mixture (b) to conditions, whereby solid catalyst particles are formed, wherein (i) a Bi compound and (ii) a bidentate electron donor compound are present in one or more of steps (a) to (c) and/or contacted with the solid catalyst particles obtained from (c).
Abstract:
A propylene polymer composition made from or containing: a) from 15 wt % to 35 wt % of a propylene 1-hexene copolymer containing from 6.2 to 8.5% by weight, of 1-hexene derived units and having a Melt Flow Rate from 3.5 to 8.5 g/10 min; b) from 15 wt % to 35 wt % of a propylene 1-hexene copolymer containing from 10.4 wt % to 14.5 wt %, of 1-hexene derived units and having a Melt Flow Rate from 3.5 to 8.5 g/10 min; and c) from 38 wt % to 68 wt % of a propylene ethylene copolymer containing from 3.4 wt % to 5.7 wt % of ethylene derived units and having a Melt Flow Rate from 3.5 to 12.0 g/10 min, wherein the sum of the amount of a), b) and c) being 100.
Abstract:
A polypropylene composition made from or containing: A) from 50 wt % to 90 wt %, based upon the total weight of the polypropylene composition, of a propylene homopolymer; and B) from 10 wt % to 50 wt %, based upon the total weight of the polypropylene composition, of a copolymer of propylene and ethylene having from 30.0 wt % to 70.0 wt %, based upon the total weight of the copolymer, of ethylene derived units; the polypropylene composition having: i) an intrinsic viscosity of the fraction soluble in xylene at 25° C. between 2.2 and 4.0 dl/g; ii) a MFR L from 0.5 to 100 g/10 min; and iii) a xylene soluble fraction ranging from 10 wt % to 50 wt %, based upon the total weight of the polypropylene composition.
Abstract:
The present disclosure relates to a multilayer film characterized by one or more skin layers comprising propylene/ethylene copolymers characterized by the following features: an ethylene derived units content of between 1.0 wt % and 15.0% wt %; and a molecular weight distribution (MWD), expressed in terms of Mw/Mn, of greater than 4.0;a content of xylene soluble fraction (XS) and an ethylene derived units content (C2) that fulfills the following relationship: XS
Abstract:
A polypropylene composition made from or containing: A) from 50 wt % to 90 wt %; of a propylene homopolymer; B) from 10 wt % to 50 wt %; of a copolymer of propylene having from 30.0 wt % to 70.0 wt %, of ethylene derived units, based upon the total weight of the copolymer; the sum of the amount of component A) and B) being 100; the polypropylene composition having: i) an intrinsic viscosity of the fraction soluble in xylene at 25° C. between 2.2 to 4.0 dl/g; ii) a MFR L (Melt Flow Rate according to ISO 1133, condition L, at 230° C. and 2.16 kg load) from 0.5 to 100 g/10 min; iii) a xylene soluble fraction ranging from 20 wt % to 50 wt %, based upon the total weight of the polypropylene composition; wherein the polypropylene composition being obtained by a polymerization process wherein the catalyst system contains bismuth.
Abstract:
A polyolefin composition made from or containing:A) from about 19 wt % to about 50 wt % of a propylene ethylene copolymer having an ethylene derived units content ranging from about 1.5 wt % to about 6.0 wt %B) from about 50 wt % to about 81 wt % of a propylene ethylene 1-butene terpolymer having an ethylene derived units content ranging from about 1.5 wt % to about 6.0 wt % and 1-butene derived units content between about 4.8 wt % and about 12.4 wt %;the sum of the amount of component A) and B) being 100;the polyolefin composition being characterized by the following features: molecular weight distribution (MWD), expressed in terms of Mw/Mn, greater than about 4.0; the creep and recovery curve measured on the polymer fuse at 200° C. shows a maximum value between 600 and 1200 seconds, lower than about 53×10−4 l/Pa.
Abstract:
The present disclosure relates to propylene-ethylene copolymers comprising an ethylene content of 0.1-10% by weight, a molecular weight distribution (MWD), expressed in terms of Mw/Mn, of greater than 3.0 and a xylene soluble (XS) fraction content defined by values that fall below the line given by the equation XS=1.0296·e0.435C2. The propylene-ethylene copolymers advantageously exhibit high transparency and low melting temperatures.
Abstract:
A solid catalyst component for the polymerization of olefins made from or containing Mg, Ti, Cl and at least an electron donor compound which is the reaction product obtained by bringing into contact a Mg compound and a Ti compound having at least a Ti-halogen bond with an electron donor selected from diphenol derivatives.
Abstract:
A propylene ethylene copolymer having the following features: an ethylene content of between 1.0 and 4.0% by weight; a molecular weight distribution (MWD), expressed in terms of Mw/Mn, of greater than 4.0; a content of xylene soluble fraction (XS) and ethylene content (C2) that fulfills the following relationship: (C2×1.1)+1.25
Abstract:
A catalyst for the homopolymerization or copolymerization of CH2═CHR olefins, made from or containing the product obtained by contacting: (i) a solid catalyst component made from or containing Ti, Mg, Cl, and an internal electron donor compound, wherein the solid catalyst component contains from about 0.1 to about 50 wt % of Bi, based upon the total weight of the solid catalyst component; (ii) an alkyl aluminum compound and, (iii) an external electron donor compound having the formula: (R1)aSi(OR2)b wherein R1 and R2 are independently selected from the group consisting of alkyl radicals with 1-8 carbon atoms and a is 0 or 1 and a+b=4.